# US 2015/0147267 A1 · METHOD OF PREPARING CATALYST HAVING Pt-Pd DISPERSED POLYMER ELECTROLYTE MULTILAYERS TREATED WITH SULFURIC ACID

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0147267 A1
- Document ID: US20150147267A1
- Status: Published application
- Kind: A1
- Application number: 14/539,496
- Filed: 2014-11-12
- Published: 2015-05-28
- Earliest claimed: 2013-11-26
- Assignees: SK Innovation Co., Ltd.; SK Global Chemical Co., Ltd.
- Applicants: SK Innovation Co., Ltd.; SK Global Chemical Co., Ltd.
- Inventors: Suk Joon HONG; Yong Tak KWON; Hwa Jung LEE; Tae JIn KIM; Dae Hyun CHOO
- Web page: https://patentgrep.com/patent/US20150147267A1

## CPC

- B01J 37/16: Reducing
- B01J 23/44: Palladium
- B01J 31/06: containing polymers {(organometallic polymers B01J31/123; polymer-bound organometallic complexes B01J31/165; coordination polymers B01J31/1691)}
- B01J 31/08: Ion-exchange resins
- B01J 31/10: sulfonated
- B01J 35/393: {Metal or metal oxide crystallite size}
- B01J 35/45: Nanoparticles
- B01J 37/0244: {Coatings comprising several layers}
- C01B 15/029: Preparation from hydrogen and oxygen
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}

## Abstract

Disclosed herein is a method of preparing a catalyst having Pt—Pd dispersed in polymer electrolyte multilayers, suitable for use in production of hydrogen peroxide, wherein the use of the catalyst prepared by forming polymer electrolyte multilayers on an anionic resin support and performing sulfuric acid treatment and loading (insertion or attachment) of Pt—Pd particles can result in high hydrogen conversion, hydrogen selectivity and hydrogen peroxide yield for a long period of time.

## Claims

### Claim 1

A method of preparing a catalyst having polymer electrolyte multilayers, comprising:
a) sequentially forming a cationic polymer electrolyte layer and an anionic polymer electrolyte layer on an anionic support to form polymer electrolyte multilayers;
b) treating the polymer electrolyte multilayers of step a) with sulfuric acid; and
c) loading or inserting a Pt precursor and a Pd precursor into the polymer electrolyte multilayers treated with sulfuric acid in step b), and reducing the Pt precursor and the Pd precursor by a reductant to form Pt—Pd metal particles dispersed in the polymer electrolyte multilayers,
wherein a Pt/Pd atomic ratio in the reduced Pt—Pd metal particles is 0.02 to 0.15.

### Claim 2 (depends on 1)

The method of claim 1, wherein the anionic support has a sulfonic acid functional group.

### Claim 3 (depends on 1)

The method of claim 1, wherein step a) is repeated two or more times.

### Claim 4 (depends on 1)

The method of claim 1, wherein step a) is performed by bringing a cationic polymer electrolyte solution and an anionic polymer electrolyte solution into sequential contact with the anionic support.

### Claim 5 (depends on 1)

The method of claim 1, wherein the cationic polymer electrolyte is poly(allylamine)hydrochloride, polydiallyldimethylammonium, poly(ethyleneimine), poly(acrylamide-co-diallyldimethylammonium) or a combination thereof.

### Claim 6 (depends on 1)

The method of claim 1, wherein the anionic polymer electrolyte is poly(4-styrenesulfonate), poly(acrylic acid), poly(acrylamide), poly(vinylphosphonic acid), poly(2-acrylamido-2-methyl-11-propanesulfonic acid), poly(anetholesulfonic acid), poly(vinylsulfonate) or a combination thereof.

### Claim 7 (depends on 4)

The method of claim 4, wherein a solvent for the cationic polymer electrolyte solution and the anionic polymer electrolyte solution is water, n-hexane, ethanol, triethylamine, tetrahydrofuran (THF), dimethyl sulfoxide (DMSO), ethylacetate, isopropylalcohol, acetone, acetonitrile, benzene, butylalcohol, chloroform, diethylether, or a mixture thereof.

### Claim 8 (depends on 1)

The method of claim 1, wherein the sulfuric acid used in step b) is an aqueous sulfuric acid solution with a concentration of 0.05 to 8 M.

### Claim 9 (depends on 8)

The method of claim 8, wherein step b) is performed by bringing the aqueous sulfuric acid solution into contact with the polymer electrolyte multilayers at 20 to 120° C. for 5 to 600 min.

### Claim 10 (depends on 1)

The method of claim 1, wherein step c) comprises bringing a solution containing the Pt precursor and the Pd precursor into contact with the support having the polymer electrolyte multilayers,
wherein the Pt precursor and the Pd precursor in the solution have a concentration of 0.05 to 10 mM.

### Claim 11 (depends on 10)

The method of claim 10, wherein the solution containing the Pt precursor and the Pd precursor has a pH of 1 to 6.

### Claim 12 (depends on 1)

The method of claim 1, wherein an amount of the reduced Pt—Pd metal particles in the catalyst is 0.01 to 5 wt %.

### Claim 13 (depends on 1)

The method of claim 1, wherein the Pt/Pd atomic ratio in the reduced Pt—Pd metal particles is 0.05 to 0.1.

### Claim 14 (depends on 1)

The method of claim 1, wherein the reduced Pt—Pd metal particles have a size of 1 to 100 nm.

### Claim 15 (depends on 1)

A method of producing hydrogen peroxide, comprising:
reacting hydrogen and oxygen using a catalyst having polymer electrolyte multilayers prepared by the method of claim 1.

### Claim 16 (depends on 15)

The method of claim 15, wherein the reaction is performed in a liquid-phase reaction using a solvent containing 100 ppm or less of a halogen additive and free of an acid promoter.

### Claim 17 (depends on 15)

The method of claim 15, wherein the reaction is performed at a reaction temperature of 20 to 60° C. and at a reaction pressure of 35 to 70 bar.