# US 2015/0147258 A1 · Single crystal silicon ingot and wafer, and apparatus and method for growing said ingot

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0147258 A1
- Document ID: US20150147258A1
- Status: Published application
- Kind: A1
- Application number: 14/402,405
- Filed: 2013-04-02
- Published: 2015-05-28
- Earliest claimed: 2012-05-23
- Assignees: LG SILTRON INCORPORATION a corporation
- Applicants: LG Siltron Incorporated
- Inventors: Young Ho Hong; Jung Ha Hwang; Il Seon Cha
- Web page: https://patentgrep.com/patent/US20150147258A1

## CPC

- C30B 29/06: Silicon
- C30B 15/00: Single-crystal growth by pulling from a melt, e.g. Czochralski method (under a protective fluid C30B27/00)
- C30B 15/14: Heating of the melt or the crystallised materials
- C30B 15/20: Controlling or regulating (controlling or regulating in general G05)
- C30B 30/04: using magnetic fields
- Y10T 117/1068: including heating or cooling details [e.g., shield configuration]
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The single crystal silicon ingot and wafer of one embodiment has a transition region formed therein which predominantly has crystal defects of 10 nm to 30 nm in size from among crystal defects included in at least one region of a vacancy predominant non-defective region and an interstitial predominant non-defective region.

## Claims

### Claim 1

A single-crystal silicon ingot and wafer comprising a transition region having predominant crystal defects having a size of 10 nm to 30 nm among crystal defects included in at least one of a vacancy predominant non-defective region and an interstitial predominant non-defective region.

### Claim 2 (depends on 1)

The single-crystal silicon ingot and wafer according to claim 1, wherein the crystal defects having a size of 10 nm to 30 nm make up above 50% of all crystal defects included in the transition region.

### Claim 3 (depends on 1)

The single-crystal silicon ingot and wafer according to claim 1, wherein the crystal defects having a size of 10 nm to 30 nm make up 70% or more of all crystal defects included in the transition region.

### Claim 4 (depends on 1)

The single-crystal silicon ingot and wafer according to claim 1, wherein the transition region include no ring-shaped oxidation induced stacking faults.

### Claim at position 5

-6. (canceled)

### Claim 7 (depends on 1)

The single-crystal silicon ingot and wafer according to claim 1, wherein the interstitial predominant non-defective region occupies 100x % of the entire transition region (here, 0≦x≦1), and the vacancy predominant non-defective region occupies 100(1−x) % of the entire transition region, in the single-crystal silicon ingot and wafer.

### Claim 8 (depends on 1)

The single-crystal silicon ingot and wafer according to claim 1, wherein the interstitial predominant non-defective region occupies 70% or more of the entire transition region on the basis of a diameter of the single-crystal silicon ingot and wafer.

### Claim 9 (depends on 1)

The single-crystal silicon ingot and wafer according to claim 1, wherein the vacancy predominant non-defective region occupies 30% or less of the entire transition region on the basis of a diameter of the single-crystal silicon ingot and wafer.

### Claim 10

(canceled)

### Claim 11 (depends on 1)

The single-crystal silicon ingot and wafer according to claim 1, wherein the size of the crystal defects included in the transition region is detectable by a Magics method.

### Claim 12 (depends on 11)

The single-crystal silicon ingot and wafer according to claim 11, wherein the size of the crystal defects included in the transition region is detectable by the Magics method, under a state without thermal treatment of the single-crystal silicon ingot and wafer.

### Claim 13

(canceled)

### Claim 14

An apparatus of growing a single-crystal silicon ingot, the apparatus comprising:
a crucible configured to receive a silicon melt therein;
a heater installed around the crucible to apply heat to the crucible; and
a magnetic field generator configured to apply a magnetic field to the crucible such that a maximum magnetic plane (MGP) is created at a position determined according to a position of a maximum heat radiation point of the heater.

### Claim 15

(canceled)

### Claim 16 (depends on 14)

The apparatus according to claim 14, wherein the heater is configured to adjust the radiation amount of heat in the vertical direction.

### Claim 17 (depends on 14)

The apparatus according to claim 14, wherein the MGP is located lower than the position of the maximum heat radiation point.

### Claim 18 (depends on 17)

The apparatus according to claim 17, wherein the MGP is located lower than the position of the maximum heat radiation point by 20% to 40% on the basis of an interface of the silicon melt.

### Claim 19 (depends on 14)

The apparatus according to claim 14, wherein the MGP is located lower than the interface of the silicon melt by 50 mm to 300 mm.

### Claim 20 (depends on 14)

The apparatus according to claim 14, wherein the single-crystal silicon ingot to be grown has a target pulling rate range of 0.010 mm/min to 0.030 mm/min.

### Claim 21

A method of growing a single-crystal silicon ingot performed by an apparatus of growing a single-crystal silicon ingot, the apparatus comprising a crucible configured to receive a silicon melt therein, a heater installed around the crucible to apply heat to the crucible and a magnetic field generator configured to apply a magnetic field to the crucible, the method comprising:
determining a position of a maximum heat radiation point of the heater;
determining a position of a maximum magnetic plane (MGP) according to the determined position of the maximum heat radiation point; and
applying the magnetic field to the crucible so as to create the MGP at the determined position.

### Claim 22

(canceled)

### Claim 23 (depends on 21)

The method according to claim 21, wherein the magnetic field is applied to the crucible so as to create the MGP at a position lower than the position of the maximum heat radiation point.

### Claim 24 (depends on 21)

The method according to claim 21, wherein the magnetic field is applied to the crucible so as to create the MGP at a position lower than the position of the maximum heat radiation point by 20% to 40% on the basis of an interface of the silicon melt.

### Claim 25 (depends on 21)

The method according to claim 21, wherein the magnetic field is applied to the crucible so as to create the MGP at a position lower than an interface of the silicon melt by 50 mm to 300 mm.

### Claim 26 (depends on 25)

The method according to claim 25, wherein the single-crystal silicon ingot to be grown has a target pulling rate range of 0.010 mm/min to 0.030 mm/min.

### Claim at position 26

-33. (canceled)