# US 2015/0147247 A1 · Method of pre-treating molybdenite containing copper

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0147247 A1
- Document ID: US20150147247A1
- Status: Published application
- Kind: A1
- Application number: 14/105,756
- Filed: 2013-12-13
- Published: 2015-05-28
- Earliest claimed: 2013-11-28
- Assignees: Korea Institute of Geoscience and Mineral Resources
- Applicants: Korea Institute of Geoscience and Mineral Resources
- Inventors: Young-Yoon Choi; Shun-Myung Shin; Chul-Woo Nam; Hyung-Seok Kim
- Web page: https://patentgrep.com/patent/US20150147247A1

## CPC

- C22B 34/34: Obtaining molybdenum {(treatment or purification of solutions by adsorption on solids C22B3/24, by liquid-liquid extraction C22B3/26, by ion-exchange extraction C22B3/42; preparation of molybdenum involving liquid-liquid extraction, adsorption or ion-exchange C01G39/003)}
- C22B 1/00: Preliminary treatment of ores or scrap
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS

## Abstract

Disclosed is a method of pre-treating molybdenite containing copper. The method includes mixing molybdenite containing copper with sulfuric acid, performing a sulfation reaction through a heating process after the mixing process is performed, performing a water leaching process by putting and stirring water after the sulfation reaction is performed, separating a cake from liquid after the water leaching process is performed, and drying the separated cake.

## Claims

### Claim 1

A method of pre-treating molybdenite containing copper, the method comprising:
mixing molybdenite containing copper with sulfuric acid;
performing a sulfation reaction through a heating process after the mixing process is performed;
performing a water leaching process by putting and stirring water after the sulfation reaction is performed;
separating a cake from liquid after the water leaching process is performed; and
drying the separated cake.

### Claim 2 (depends on 1)

The method of claim 1, wherein the sulfation reaction is performed at a temperature of 180° C. to 240° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein the sulfation reaction is performed for time of 20 minutes to 80 minutes.

### Claim 4 (depends on 1)

The method of claim 1, wherein the sulfuric acid is mixed with the molybdenite at an equivalent ratio of 0.9 to 1.8 with respect to the molybdenite.

### Claim 5 (depends on 1)

The method of claim 1, wherein the sulfation reaction is performed at a temperature of 180° C. to 240° C. for time of 20 minutes to 80 minutes after the sulfuric acid is mixed at an equivalent ratio of 0.9 to 1.8.

### Claim 6 (depends on 1)

The method of claim 1, wherein the sulfation reaction is performed at a temperature of 210° C. to 240° C.

### Claim 7 (depends on 6)

The method of claim 6, wherein the sulfation reaction is performed for time of 40 minutes to 80 minutes.

### Claim 8 (depends on 6)

The method of claim 6, wherein the sulfuric acid is mixed with the molybdenite at an equivalent ratio of 0.9 to 1.8 with respect to the molybdenite.

### Claim 9 (depends on 1)

The method of claim 1, wherein the sulfation reaction is performed at a temperature of 210° C. to 240° C. for time of 40 minutes to 80 minutes after the sulfuric acid is mixed at an equivalent ratio of 0.9 to 1.8.

### Claim 10 (depends on 1)

The method of claim 1, wherein the water comprises at least one selected from the group consisting of distilled water, deionized water, hard water, and heavy water.

### Claim 11 (depends on 1)

The method of claim 1, further comprising performing a floatation process with respect to the molybdenite before the molybdenite is mixed with the sulfuric acid.