# US 2015/0147228 A1 · Permanent magnet, and motor and generator using the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0147228 A1
- Document ID: US20150147228A1
- Status: Published application
- Kind: A1
- Application number: 14/611,431
- Filed: 2015-02-02
- Published: 2015-05-28
- Earliest claimed: 2013-03-26
- Assignees: Kabushiki Kaisha Toshiba
- Applicants: Kabushiki Kaisha Toshiba
- Inventors: Masaki Endo; Shinya Sakurada; Yosuke Horiuchi; Tsuyoshi Kobayashi; Keiko Okamoto; Masaya Hagiwara
- Web page: https://patentgrep.com/patent/US20150147228A1

## CPC

- H01F 1/055: and magnetic transition metals, e.g. SmCo5
- H01F 1/0557: {sintered}
- H02K 1/02: characterised by the magnetic material
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- H02K: DYNAMO-ELECTRIC MACHINES (dynamo-electric relays H01H53/00; conversion of DC or AC input power into surge output power {H03K3/53})

## Abstract

In one embodiment, a permanent magnet has a composition represented by a composition formula: RpFeqMrCusCo100-p-q-r-s, where R is a rare earth element, M is at least one element selected from Zr, Ti, and Hf, p is 8.0 atomic % or more and 13.5 atomic % or less, q is 25 atomic % or more and 40 atomic % or less, r is 0.88 atomic % or more and 7.2 atomic % or less, and s is 3.5 atomic % or more and 13.5 atomic % or less, and a metallic structure including a cell phase having a Th2Zn17 crystal phase, a cell wall phase, and a platelet phase existing along a c plane of the Th2Zn17 crystal phase. An average thickness of the platelet phase is in a range of from 2.5 nm to 20 nm.

## Claims

### Claim 1

A permanent magnet, comprising:
a composition represented by the following composition formula:
RpFeqMrCusCo100-p-q-r-s
wherein R is at least one element selected from the group consisting of rare earth elements,
M is at least one element selected from the group consisting of Zr, Ti, and Hf,
p is 8.0 atomic % or more and 13.5 atomic % or less,
q is 25 atomic % or more and 40 atomic % or less,
r is 0.88 atomic % or more and 7.2 atomic % or less, and
s is 3.5 atomic % or more and 13.5 atomic % or less; and
a metallic structure comprising a cell phase having a Th2Zn17 crystal phase, a cell wall phase existing in a form surrounding the cell phase, and a platelet phase existing along a c plane of the Th2Zn17 crystal phase,
wherein an average thickness of the platelet phase is in a range of from 2.5 nm to 20 nm.

### Claim 2 (depends on 1)

The permanent magnet of claim 1,
wherein a concentration of the element M in the platelet phase is 1.2 times or more of a concentration of the element M in the cell phase.

### Claim 3 (depends on 1)

The permanent magnet of claim 1,
wherein a concentration of the element M in the platelet phase is 2 atomic % or more.

### Claim 4 (depends on 1)

The permanent magnet of claim 1,
wherein an average thickness of the platelet phase is in a range of from 3 nm to 15 nm.

### Claim 5 (depends on 1)

The permanent magnet of claim 1,
wherein coercive force of the permanent magnet is 650 kA/m or more, and residual magnetization of the permanent magnet is 1.15 T or more.

### Claim 6 (depends on 1)

The permanent magnet of claim 1,
wherein 50 atomic % or more of the element R is Sm.

### Claim 7 (depends on 1)

The permanent magnet of claim 1,
wherein 50 atomic % or more of the element M is Zr.

### Claim 8 (depends on 1)

The permanent magnet of claim 1,
wherein 20 atomic % or less of the Co element is replaced with at least one element A selected from the group consisting of Ni, V, Cr, Mn, Al, Ga, Nb, Ta, and W.

### Claim 9 (depends on 1)

A motor comprising the permanent magnet of claim 1.

### Claim 10 (depends on 1)

A generator comprising the permanent magnet of claim 1.