# US 2015/0147186 A1 · Silicon carbide-containing mold and facecoat compositions and methods for casting titanium and titanium aluminide alloys

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0147186 A1
- Document ID: US20150147186A1
- Status: Published application
- Kind: A1
- Application number: 14/090,974
- Filed: 2013-11-26
- Published: 2015-05-28
- Earliest claimed: 2013-11-26
- Assignees: General Electric Company
- Applicants: General Electric Company
- Inventors: Bernard Patrick BEWLAY; Joan MCKIEVER; Brian Michael ELLIS; Nicholas Vincent MCCLASKY
- Web page: https://patentgrep.com/patent/US20150147186A1

## CPC

- B22C 1/02: characterised by additives for special purposes, e.g. indicators, breakdown additives
- B22C 1/00: Compositions of refractory mould or core materials; Grain structures thereof (refractory materials in general C04B35/00); Chemical or physical features in the formation or manufacture of moulds
- B22C 9/22: Moulds for peculiarly-shaped castings
- B22D 21/06: Casting non-ferrous metals with a high melting point, e.g. metallic carbides (B22D21/02 takes precedence)
- C04B 28/06: Aluminous cements (monolithic refractories or refractory mortars C04B35/66)
- C04B 35/057: based on calcium oxide
- C04B 35/117: Composites
- C04B 35/44: based on aluminates
- C04B 35/565: based on silicon carbide
- C04B 35/6263: {characterised by their solids loadings, i.e. the percentage of solids}
- C04B 35/6303: {Inorganic additives}
- C04B 38/08: by adding porous substances
- F01D 5/28: Selecting particular materials; {Particular measures relating thereto;} Measures against erosion or corrosion
- B22C 9/04: Use of lost patterns
- C04B 2111/00939: {for the fabrication of moulds or cores}
- C04B 2235/3208: Calcium oxide or oxide-forming salts thereof, e.g. lime
- C04B 2235/3222: Aluminates other than alumino-silicates, e.g. spinel (MgAl2O4)
- C04B 2235/3826: Silicon carbides
- C04B 2235/5436: micrometer sized, i.e. from 1 to 100 micron
- C04B 2235/6028: Shaping around a core which is removed later
- C04B 2235/9676: against molten metals such as steel or aluminium
- Y02T 50/60: Efficient propulsion technologies, e.g. for aircraft
- B22C: FOUNDRY MOULDING (moulding refractory materials in general B28B)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- F01D: NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAM TURBINES (machines or engines for liquids F03; non-positive displacement pumps F04D)
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION

## Abstract

The disclosure relates generally to mold compositions and methods of molding and the articles so molded. More specifically, the disclosure relates to silicon carbide-containing mold compositions, silicon carbide-containing intrinsic facecoat compositions, and methods for casting titanium-containing articles, and the titanium-containing articles so molded.

## Claims

### Claim 1

A method for forming a mold for casting a titanium-containing article, comprising:
mixing calcium aluminate and silicon carbide with a liquid to produce a slurry, wherein the percentage of solids in the slurry is about 60% to about 80% by weight of the slurry and a viscosity of the slurry is about 30 to about 1500 centipoise;
introducing the slurry into a mold cavity that contains a fugitive pattern; and
allowing the slurry to cure in the mold cavity to form the mold for casting the titanium-containing article.

### Claim 2 (depends on 1)

The method of claim 1, wherein the silicon carbide particles are from about 10 microns to about 50 microns in outside dimension.

### Claim 3 (depends on 1)

The method of claim 1, wherein the calcium aluminate comprises more than 20% by weight of the slurry.

### Claim 4 (depends on 1)

The method of claim 1, wherein a particle size of the calcium aluminate is less than about 50 microns in outside dimension.

### Claim 5 (depends on 1)

The method of claim 1, wherein, the slurry further comprises oxide particles.

### Claim 6 (depends on 5)

The method of claim 5, wherein said oxide particles are hollow.

### Claim 7 (depends on 5)

The method of claim 5, wherein the oxide particles are selected from a group consisting of aluminum oxide particles, magnesium oxide particles, calcium oxide particles, zirconium oxide particles, titanium oxide particles, silicon oxide particles, and compositions thereof.

### Claim 8 (depends on 5)

The method of claim 5, wherein the oxide particles are aluminum oxide particles.

### Claim 9 (depends on 8)

The method of claim 8, wherein said aluminum oxide particles comprise from about 30% by weight to about 68% by weight of the slurry.

### Claim 10 (depends on 8)

The method of claim 8, wherein said aluminum oxide particles are from about 50 microns to about 1500 microns in outside dimension.

### Claim 11 (depends on 1)

The method of claim 1, wherein before introducing the slurry into the mold cavity, large scale hollow oxide particles are added to the slurry to form a final calcium aluminate-liquid cement mixture, such that the solids in the slurry are about 70% to about 95% by weight of the slurry.

### Claim 12 (depends on 1)

The method of claim 1, further comprising calcium oxide added such that more than about 10% by weight and less than about 50% by weight of the slurry is calcium oxide.

### Claim 13 (depends on 1)

The method of claim 1, wherein the percentage of solids in the slurry is about 60% to about 78%.

### Claim 14 (depends on 1)

The method of claim 1, further comprising adding less than 2% silica to the slurry.

### Claim 15

A method for casting titanium and titanium alloys, comprising:
obtaining an investment casting mold composition comprising calcium aluminate and large scale aluminum oxide, wherein the calcium aluminate and alumina are combined with a liquid and silicon carbide to produce a final calcium aluminate/liquid mixture slurry, and wherein the solids in the final mixture is about 70% to about 95% by weight of the slurry;
pouring said investment casting mold composition into a vessel containing a fugitive pattern;
curing said investment casting mold composition;
removing said fugitive pattern from the mold;
firing the mold;
preheating the mold to a mold casting temperature;
pouring molten titanium or titanium alloy into the heated mold;
solidifying the molten titanium or titanium alloy;
forming a solidified titanium or titanium alloy casting; and
removing the solidified titanium or titanium alloy casting from the mold.

### Claim 16 (depends on 15)

The method of claim 15, wherein particles of the aluminum oxide are about 50 microns to about 1500 microns in outside dimension.

### Claim 17 (depends on 15)

The method of claim 15, wherein silicon carbide particles are about 10 microns to about 100 microns in outside dimension.

### Claim 18 (depends on 15)

The method of claim 15, wherein the silicon carbide is present between 15% to 45% by weight and provides increased thermal conductivity during casting by at least 25% as compared to casting performed without silicon carbide.

### Claim 19

A turbine blade produced by the process, comprising:
providing an investment casting mold, said mold comprising calcium aluminate, silicon carbide and aluminum oxide;
pouring molten titanium or titanium alloy into the mold;
solidifying the molten titanium or titanium alloy;
forming a solidified titanium or titanium alloy casting; and
removing the solidified titanium or titanium alloy casting from the mold to produce the turbine blade, wherein the turbine blade has an average roughness, Ra, of less than 20 across at least a portion of its surface area.

### Claim 20 (depends on 19)

The method of claim 19, wherein silicon carbide particles are about 10 microns to about 100 microns in outside dimension.

### Claim 21 (depends on 19)

The method of claim 19, wherein the silicon carbide is present between 15% to 45% by weight and provides increased thermal conductivity during casting by at least 25% as compared to casting performed without silicon carbide.

### Claim 22

A method for manufacturing a turbine component, comprising:
making a mold from a mixture comprising calcium aluminate, calcium dialuminate, silicon carbide, mayenite and water, wherein the silicon carbide is present at about 15% to about 45% by weight;
firing the mold;
pouring molten titanium or titanium alloy into the mold;
solidifying the molten titanium or titanium alloy to form a solidified casting; and
removing the casting from the mold.

### Claim 23 (depends on 22)

The method of claim 22, further comprising hollow aluminum oxide particles that are larger than about 50 microns.

### Claim 24 (depends on 22)

The method of claim 22, wherein silicon carbide particles are about 10 microns to about 100 microns in outside dimension.

### Claim 25 (depends on 22)

The method of claim 22, wherein the silicon carbide is present between 15% to 45% by weight and provides increased thermal conductivity during casting by at least 25% as compared to casting performed without silicon carbide.