# US 2015/0146840 A1 · Sodium-resistant joining glass and the use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0146840 A1
- Document ID: US20150146840A1
- Status: Published application
- Kind: A1
- Application number: 14/526,672
- Filed: 2014-10-29
- Published: 2015-05-28
- Earliest claimed: 2013-11-26
- Assignees: Schott AG
- Applicants: Schott AG
- Inventors: Jens Suffner
- Web page: https://patentgrep.com/patent/US20150146840A1

## CPC

- C03C 8/24: Fusion seal compositions being frit compositions having non-frit additions, i.e. for use as seals between dissimilar materials, e.g. glass and metal; Glass solders
- C03C 3/091: containing aluminium
- C03C 3/093: containing zinc or zirconium
- C03C 8/02: Frit compositions, i.e. in a powdered or comminuted form
- C03C 8/04: containing zinc
- F16B 11/00: Connecting constructional elements or machine parts by sticking or pressing them together, e.g. cold pressure welding (non-electric welding in general B23K; methods of using adhesives independently of the form of the surfaces joined C09J5/00)
- G21C 13/02: Details
- H02G 3/22: Installations of cables or lines through walls, floors or ceilings, e.g. into buildings
- C03C 2204/00: Glasses, glazes or enamels with special properties
- C03C 2205/00: Compositions applicable for the manufacture of vitreous enamels or glazes
- G21C 1/02: Fast fission reactors, i.e. reactors not using a moderator {; Metal cooled reactors; Fast breeders}
- H01M 10/39: working at high temperature
- H01M 50/186: characterised by the disposition of the sealing members
- Y02E 30/30: Nuclear fission reactors
- Y02E 60/10: Energy storage using batteries
- Y10T 29/4911: including sealing
- Y10T 403/477: Fusion bond, e.g., weld, etc.
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- F16B: DEVICES FOR FASTENING OR SECURING CONSTRUCTIONAL ELEMENTS OR MACHINE PARTS TOGETHER, e.g. NAILS, BOLTS, CIRCLIPS, CLAMPS, CLIPS OR WEDGES; JOINTS OR JOINTING (couplings for transmitting rotation F16D)
- G21C: NUCLEAR REACTORS (fusion reactors, hybrid fission-fusion reactors G21B; nuclear explosives G21J)
- H02G: INSTALLATION OF ELECTRIC CABLES OR LINES, OR OF COMBINED OPTICAL AND ELECTRIC CABLES OR LINES
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The sodium-resistant joining glass (1) is substantially free of ZrO2 and is based on a SiO2—B2O3—Na2O—Al2O3 glass system. It is suitable for producing a joint of a metal and/or ceramic component with a further joining component (2, 3, 4) using the joining glass (1). Feedthrough-devices (20) using the joining glass (1) as fixing material are also disclosed.

## Claims

### Claim 1

A joining glass (1) that is free of ZrO2 except for at most impurities and that comprises, in % by weight based on oxide content:
SiO2
40-50
B2O3
>25-30
Na2O
5-15
Al2O3
17-25
Σ MO
0-<2,
wherein MO represents, individually or in any combination, CaO and/or SrO and/or BaO.

### Claim 2 (depends on 1)

The joining glass (1) according to claim 1, additionally comprising, individually or in any combination, in % by weight based on oxide content:
ZnO
0-5
TiO2
0-5
SnO2
0-5
MgO
0-15.

### Claim 3 (depends on 1)

The joining glass (1) according to claim 1, which has a coefficient of linear thermal expansion α20-300° C. in a temperature range of 20 to 300° C. of from 5.5×10−6 K−1 to 10.5×10−6 K−1.

### Claim 4 (depends on 1)

The joining glass (1) according to claim 1, which has a coefficient of linear thermal expansion α20-300° C. in a temperature range of 20 to 300° C. of from 5.5×10−6 K−1 to 8.5×10−6 K−1.

### Claim 5 (depends on 1)

The joining glass (1) according to claim 1, which has a coefficient of linear thermal expansion α20-300° C. in a temperature range of 20 to 300° C. of from 6.0×10−6 K−1 to 8.0×10−6 K−1.

### Claim 6 (depends on 1)

The joining glass (1) according to claim 1, additionally comprising up to 30% by volume of an oxidic filler for setting or adjusting thermal expansion behaviour, corrosion resistance and/or flow behaviour.

### Claim 7 (depends on 6)

The joining glass (1) according to claim 6, wherein the filler is in the form of particles and/or fibres.

### Claim 8

A joint between a first joining component (2) and a second joining component (3, 4, 41), said joint comprising a joining glass (1),
wherein the joining glass (1) bonds a joining area of the first joining component (2) to a joining area of the second joining component (3, 4, 41);
wherein said joining glass (1) is free of ZrO2 except for at most impurities and comprises, in % by weight based on oxide content:
SiO2
40-50
B2O3
>25-30
Na2O
5-15
Al2O3
17-25
Σ MO
0-<2;
wherein MO represents, individually or in any combination, CaO and/or SrO and/or BaO.

### Claim 9 (depends on 8)

The joint according to claim 8, wherein the first joining component (2) comprises a ceramic at least at the joining area thereof and the second joining component (3, 4, 41) comprises a metal and/or a ceramic at least at the joining area thereof.

### Claim 10 (depends on 9)

The joint according to claim 9, wherein the ceramic at the joining area of the first joining component (2) and/or at the joining area of the second joining component (3, 4, 41) is selected from the group consisting of alumina, α-alumina, β-alumina, β″-alumina and sodium super ionic conductor (NASICON).

### Claim 11 (depends on 9)

The joint according to claim 9, wherein the metal of the second joining component (41) has a coefficient of linear thermal expansion α20-300° C. which in a temperature range is greater than or equal to a coefficient of linear thermal expansion α20-300° C. of the ceramic in said temperature range.

### Claim 12 (depends on 8)

The joint according to claim 8, wherein the first joining component (2) comprises a metal at least at the joining area thereof and the second joining component (3, 4, 41) comprises a metal at least at the joining area thereof.

### Claim 13 (depends on 12)

The joint according to claim 12, wherein the metal (41) of the second joining component has a coefficient of linear thermal expansion α20-300° C.>8×10−6 K−1.

### Claim 14 (depends on 8)

An electrochemical energy storage and/or energy generation unit comprising at least one joint according to claim 8.

### Claim 15 (depends on 8)

A sodium-sulphur battery or sodium-metal chloride battery comprising at least one joint according to claim 8.

### Claim 16

An electrical feedthrough-device (20) comprising at least one joint that bonds a joining area of a first joining component (2) to a joining area of a second joining component (3, 4, 41), said joint comprising a joining glass;
wherein said joining glass (1) is free of ZrO2 except for at most impurities and comprises, in % by weight based on oxide content:
SiO2
40-50
B2O3
>25-30
Na2O
5-15
Al2O3
17-25
Σ MO
0-<2;
and
wherein MO represents, individually or in any combination, CaO and/or SrO and/or BaO.

### Claim 17 (depends on 1)

An electrical feedthrough-device (20) comprising
a metal carrier element (30) with at least one feedthrough opening, and
a metal functional component (31),
wherein the metal functional component (31) is fixed within the feedthrough opening electrically insulated from the metal carrier element (30) by the joining glass (1) according to claim 1 so that the feedthrough opening is sealed.

### Claim 18 (depends on 1)

An installation or a containment of an installation for disposal of waste or within a nuclear reactor, preferably a breeder reactor, comprising an electrical feedthrough-device (20), wherein said electrical feedthrough-device (20) comprises:
a metal carrier element (30) with at least one feedthrough opening, and
a metal functional component (31),
wherein the metal functional component (31) is fixed within the feedthrough opening electrically insulated from the metal carrier element (30) by the joining glass (1) according to claim 1 so that the feedthrough opening is sealed.

### Claim 19 (depends on 1)

A method of making a sodium-sulphur battery or a sodium-metal chloride battery comprising the step of hermetically sealing a housing (4) of the battery and/or closing off membrane components (2) of the battery with the joining glass (1) according to claim 1.