# US 2015/0146341 A1 · ALD dielectric films with leakage-reducing impurity layers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0146341 A1
- Document ID: US20150146341A1
- Status: Published application
- Kind: A1
- Application number: 14/092,431
- Filed: 2013-11-27
- Published: 2015-05-28
- Earliest claimed: 2013-11-27
- Assignees: Globalfoundries Inc.; Intermolecular, Inc.
- Applicants: GLOBALFOUNDRIES, Inc.; Intermolecular Inc.
- Inventors: Nobumichi Fuchigami; David Paul Brunco; Karthik Ramani; Dina Triyoso
- Web page: https://patentgrep.com/patent/US20150146341A1

## CPC

- H01G 4/10: Metal-oxide dielectrics {(H01G4/085 takes precedence)}
- C23C 16/403: {of aluminium, magnesium or beryllium}
- C23C 16/405: {of refractory metals or yttrium}
- C23C 16/45525: {Atomic layer deposition [ALD]}
- H01G 4/085: {Vapour deposited}
- H01G 4/1281: {with grain boundary layer}
- H01G 4/306: {made by thin film techniques}
- H01G 4/33: Thin- or thick-film capacitors {(thin- or thick-film circuits; capacitors without a potential-jump or surface barrier specially adapted for integrated circuits, details thereof, multistep manufacturing processes therefor)}
- H10D 1/68: Capacitors having no potential barriers
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A thin sub-layer (<15 Å) of an impurity is formed under, over, or inside a thicker layer (˜30-100 Å) of a high-k (k>12) host material. The sub-layer may be formed by atomic layer deposition (ALD). The layer and sub-layer are annealed to form a composite dielectric layer. The host material crystallizes, but the crystalline lattice and grain boundaries are disrupted near the impurity sub-layer, impeding the migration of electrons. The impurity may be a material with a lower dielectric constant than the high-k material, added in such a small relative amount that the composite dielectric is still high-k. Metal-insulator-metal capacitors may be fabricated by forming the composite dielectric layer between two electrodes.

## Claims

### Claim 1

A thin-film capacitor, comprising:
a first conductive layer;
a second conductive layer; and
a composite dielectric layer between the first conductive layer and the second conductive layer;
wherein the first conductive layer and the second conductive layer are operable as electrodes;
wherein the composite dielectric layer comprises a host material and an impurity sub-layer;
wherein the impurity sub-layer is less than about 15 Å thick and comprises an impurity material; and
wherein a lattice structure or a grain boundary of the host material is disrupted at an interface with the impurity sub-layer.

### Claim 2 (depends on 1)

The capacitor of claim 1, wherein a dielectric constant of the host material is greater than a dielectric constant of the impurity material.

### Claim 3 (depends on 1)

The capacitor of claim 1, wherein the host material, similarly processed without the impurity sub-layer, would be crystalline or polycrystalline.

### Claim 4 (depends on 3)

The capacitor of claim 3, wherein an X-ray diffraction spectrum of a film stack comprising the composite dielectric has attenuated peaks associated with the host material, as compared to a similar film stack with a host-material dielectric having no impurity sub-layer.

### Claim 5 (depends on 3)

The capacitor of claim 3, wherein an X-ray diffraction spectrum of a film stack comprising the composite dielectric has no peaks larger than 30 counts associated with the host material.

### Claim 6 (depends on 1)

The capacitor of claim 1, wherein a dielectric constant of the composite dielectric layer is greater than about 80% of a dielectric constant of the host material.

### Claim 7 (depends on 1)

The capacitor of claim 1, wherein a dielectric constant of the host material is greater than about 12.

### Claim 8 (depends on 1)

The capacitor of claim 1, wherein a dielectric constant of the impurity material is less than about 12.

### Claim 9 (depends on 1)

The capacitor of claim 1, wherein the composite dielectric layer is between about 30 Å and about 100 Å thick.

### Claim 10 (depends on 1)

The capacitor of claim 1, wherein the impurity sub-layer is less than about 10 Å thick.

### Claim 11 (depends on 1)

The capacitor of claim 1, wherein the composite dielectric comprises at least one additional impurity sub-layer.

### Claim 12 (depends on 11)

The capacitor of claim 11, wherein at least one of the impurity sub-layers is less than about 1 monolayer thick.

### Claim 13 (depends on 11)

The capacitor of claim 11, wherein at least part of the composite dielectric is an alloy of the host material and the impurity material.

### Claim 14 (depends on 1)

The capacitor of claim 1, wherein the impurity sub-layer is embedded within the host material.

### Claim 15 (depends on 1)

The capacitor of claim 1, wherein the impurity sub-layer is between the host material and one of the conductive layers.

### Claim 16 (depends on 1)

The capacitor of claim 1, wherein at least one of the impurity sub-layer or the host material comprise a metal oxide.

### Claim 17 (depends on 1)

The capacitor of claim 1, wherein the host material comprises hafnium oxide or zirconium oxide and the impurity sub-layer comprises aluminum oxide or lanthanum oxide.

### Claim 18 (depends on 1)

The capacitor of claim 1, wherein at least 90% of the impurity material in the capacitor is in the impurity sub-layer.

### Claim 19

A method of making a composite dielectric layer, comprising:
forming a layer of a host material on a substrate;
forming an impurity sub-layer less than 15 Å thick; and
annealing the substrate at a temperature between about 300 and about 45° C.;
wherein the host material and the impurity sub-layer are in direct contact;
wherein the host material forms a crystalline lattice after the annealing; and
wherein the crystalline lattice is disrupted at an interface with the impurity sub-layer.

### Claim 20 (depends on 19)

The method of claim 19, wherein the impurity sub-layer is formed by atomic layer deposition.