# US 2015/0145816 A1 · Substrate with transparent electrode, method for manufacturing same, and touch panel

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0145816 A1
- Document ID: US20150145816A1
- Status: Published application
- Kind: A1
- Application number: 14/401,495
- Filed: 2013-01-29
- Published: 2015-05-28
- Earliest claimed: 2012-05-17
- Assignees: Kaneka Corporation
- Applicants: Kaneka Corporation
- Inventors: Hiroaki Ueda; Kozo Kondo; Kazuhisa Danno
- Web page: https://patentgrep.com/patent/US20150145816A1

## CPC

- G06F 3/0443: {using a single layer of sensing electrodes}
- C23C 14/0036: {Reactive sputtering}
- C23C 14/08: Oxides (C23C14/10 takes precedence)
- C23C 14/083: {of refractory metals or yttrium}
- C23C 14/086: {of zinc, germanium, cadmium, indium, tin, thallium or bismuth}
- C23C 14/10: Glass or silica
- C23C 14/34: Sputtering
- C23C 14/35: by application of a magnetic field, e.g. magnetron sputtering {(C23C14/3457 takes precedence)}
- C23C 14/562: {for coating elongated substrates}
- G06F 1/16: Constructional details or arrangements
- G06F 3/0412: {Digitisers structurally integrated in a display}
- G06F 2203/04103: Manufacturing, i.e. details related to manufacturing processes specially suited for touch sensitive devices
- G06F 2203/04112: Electrode mesh in capacitive digitiser: electrode for touch sensing is formed of a mesh of very fine, normally metallic, interconnected lines that are almost invisible to see. This provides a quite large but transparent electrode surface, without need for ITO or similar transparent conductive material
- G06F: ELECTRIC DIGITAL DATA PROCESSING (computer systems based on specific computational models G06N)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A substrate is provided with a transparent electrode in which the pattern is hardly visible even when the transparent electrode layer has been patterned, and a method for manufacturing thereof is provided. On at least one of the surfaces of a transparent film, a first, second, and third dielectric material layer, and a patterned transparent electrode layer are included, in this order, each preferably having a film thickness and refractive index within a specific range. The first and third dielectric material layers are silicon oxide layers containing SiOx and SiOv as main components, respectively. The second dielectric material layer is a metal oxide layer containing a metal oxide. The transparent electrode layer is a conductive metal oxide layer containing an indium-tin composite oxide as a main component. The refractive indexes of the first (n1), second (n2), and third (n3) dielectric material layers satisfy the relationship n3<n1<n2.

## Claims

### Claim 1

A substrate with a transparent electrode, comprising: a transparent film; and a first dielectric material layer, a second dielectric material layer, a third dielectric material layer, and a transparent electrode layer patterned into an electrode layer-formed part and an electrode layer-non-formed part, in this order on at least one surface of the transparent film, wherein
the first dielectric material layer is a silicon oxide layer containing SiOx (x≧1.5) as a main component and having a thickness of 1 nm to 25 nm,
the second dielectric material layer is a metal oxide layer containing as a main component at least one oxide of a metal selected from the group consisting of Nb, Ta, Ti, Zr, Zn and Hf and having a thickness of 5 nm or more and less than 10 nm,
the third dielectric material layer is a silicon oxide layer containing SiOy (y>x) as a main component and having a thickness of 35 nm to 80 nm,
the transparent electrode layer is a conductive metal oxide layer containing an indium-tin composite oxide as a main component and having a thickness of 20 nm to 35 nm,
a refractive index n1 of the first dielectric material layer, a refractive index n2 of the second dielectric material layer and a refractive index n3 of the third dielectric material layer satisfy a relationship of n3<n1<n2,
the transparent electrode layer has a resistivity of 5.0×10−4 Ω·cm or less, and
the electrode layer-formed part of the substrate with transparent electrode has a transmittance of 87% or more.

### Claim 2 (depends on 1)

The substrate with a transparent electrode according to claim 1, wherein the transparent electrode layer has a refractive index n4 of 1.88 or less.

### Claim 3 (depends on 1)

The substrate with a transparent electrode according to claim 1, wherein a refractive index n4 of the transparent electrode layer is larger than the refractive index n1 of the first dielectric material layer, and smaller than the refractive index n2 of the second dielectric material layer.

### Claim 4 (depends on 1)

The substrate with a transparent electrode according to claim 1, wherein the transparent electrode layer has a resistivity of 3.7×10−4 Ω·cm or less.

### Claim 5 (depends on 1)

The substrate with a transparent electrode according to claim 1, wherein an average crystal grain size of the indium-tin composite oxide in the transparent electrode layer is 110 nm to 700 nm.

### Claim 6 (depends on 5)

The substrate with a transparent electrode according to claim 5, wherein a variation coefficient of the crystal grain size of the indium-tin composite oxide in the transparent electrode layer is 0.35 or more.

### Claim 7 (depends on 1)

The substrate with a transparent electrode according to claim 1, wherein an arithmetic mean roughness of the third dielectric material layer is 1 nm or less.

### Claim 8 (depends on 1)

The substrate with a transparent electrode according to claim 1, wherein the second dielectric material layer is a metal oxide layer containing Nb2O5 as a main component.

### Claim 9 (depends on 1)

The substrate with a transparent electrode according to claim 1, wherein the transparent electrode layer has a carrier density of 6.1×1020/cm3 or more.

### Claim 10 (depends on 1)

The substrate with a transparent electrode according to claim 1, wherein the transparent electrode layer contains tin oxide in an amount of 4 parts by weight to 14 parts by weight based on 100 parts by weight of a sum of indium oxide and tin oxide.

### Claim 11 (depends on 1)

The substrate with a transparent electrode according to claim 1, wherein the thickness of the third dielectric material layer is more than 55 nm and not more than 80 nm.

### Claim 12

A method for manufacturing the substrate with a transparent electrode, wherein
a first dielectric material layer of a silicon oxide layer containing SiOx (x≧1.5) as a main component and having a thickness of 1 nm to 25 nm, a second dielectric material layer of a metal oxide layer containing as a main component at least one oxide of a metal selected from the group consisting of Nb, Ta, Ti, Zr, Zn and Hf and having a thickness of 5 nm or more and less than 10 nm, a third dielectric material layer of a silicon oxide layer containing SiOv (v>x) as a main component and having a thickness of 35 nm to 80 nm, and a transparent electrode layer of a conductive metal oxide layer containing an indium-tin composite oxide as a main component having a thickness of 20 nm to 35 nm and a resistivity of 5.0×10−4 Ω·cm or less, are formed in this order on a transparent film, wherein
the transparent electrode layer is formed by: an amorphous layer forming step of forming an amorphous transparent electrode layer containing an amorphous indium-tin composite oxide as a main component using a sputtering method; and a crystallization step of crystallizing the amorphous transparent electrode layer to obtain a crystalline transparent electrode layer, and
a magnetic flux density of a surface of a target during sputtering in the amorphous layer forming step is 30 mT or more.

### Claim 13 (depends on 12)

The method for manufacturing a substrate with a transparent electrode according to claim 12, wherein the third dielectric material layer is formed under a pressure of less than 0.4 Pa by a sputtering method.

### Claim 14 (depends on 13)

The method for manufacturing a substrate with a transparent electrode according to claim 13, wherein the first dielectric material layer is formed under a pressure of less than 0.4 Pa by a sputtering method.

### Claim 15

A substrate with a transparent electrode, comprising: a transparent film; and a dielectric material layer containing an oxide as a main component and a transparent electrode layer patterned into an electrode layer-formed part and an electrode layer-non-formed part, in this order, on at least one surface of the transparent film, wherein
the transparent electrode layer is a conductive metal oxide layer containing an indium-tin composite oxide as a main component and having a thickness of 20 nm to 35 nm, and a resistivity of the transparent electrode layer is 5.0×10−4 Ω·cm or less, and
an indium-tin composite oxide in the transparent electrode layer has an average crystal grain size of 110 nm to 700 nm and a crystal grain size variation coefficient of 0.35 or more.

### Claim 16

(canceled)