# US 2015/0145378 A1 · Quartz vibrator and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0145378 A1
- Document ID: US20150145378A1
- Status: Published application
- Kind: A1
- Application number: 14/209,544
- Filed: 2014-03-13
- Published: 2015-05-28
- Earliest claimed: 2013-11-26
- Assignees: Samsung Electro-Mechanics Co., Ltd.
- Applicants: Samsung Electro-Mechanics Co., Ltd.
- Inventors: Je Hong KYOUNG
- Web page: https://patentgrep.com/patent/US20150145378A1

## CPC

- H03H 3/04: for obtaining desired frequency or temperature coefficient
- H03H 9/02023: {consisting of quartz}
- H03H 9/19: consisting of quartz
- H03H 2003/0428: {of an electrode}
- Y10T 29/42: Piezoelectric device making
- H03H: IMPEDANCE NETWORKS, e.g. RESONANT CIRCUITS; RESONATORS (waveguides, resonators, lines or other devices of the waveguide type H01P)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Embodiments of the invention provide a quartz vibrator and a method for manufacturing the same. The quartz vibrator includes a quartz substrate vibrating depending on an electrical signal, first and second electrodes formed on both surfaces of the quartz substrate, and a first protective layer including an opening corresponding to a trimming region of the first electrode and formed on the first electrode.

## Claims

### Claim 1

A quartz vibrator, comprising:
a quartz substrate vibrating depending on an electrical signal;
first and second electrodes formed on both surfaces of the quartz substrate; and
a first protective layer including an opening corresponding to a trimming region of the first electrode and formed on the first electrode.

### Claim 2 (depends on 1)

The quartz vibrator as set forth in claim 1, wherein the quartz substrate is an AT cut quartz substrate in which based on an X axis of an orthogonal coordinate system formed of the X axis as an electrical axis, a Y axis as a mechanical axis, and a Z axis as an optical axis which are a crystal axis of a quartz, an axis formed by leaning the Z axis in a −Y direction of the Y axis is set to be a Z′ axis and an axis formed by leaning the Y axis in a +Z axis direction of the Z axis is set to be a Y′ axis, a surface parallel with the X axis and the Z′ axis is formed, and a direction parallel with the Y′ axis is set to be a thickness.

### Claim 3 (depends on 1)

The quartz vibrator as set forth in claim 1, wherein the quartz substrate comprises:
an exciting part having a rectangular plate shape; and
a peripheral part having a thickness smaller than that of the exciting part and formed around the exciting part.

### Claim 4 (depends on 3)

The quartz vibrator as set forth in claim 3, further comprising:
a first pad formed at the peripheral part; and
a first drawing electrode connecting the first pad to the first electrode,
wherein the first protective layer is formed on the first drawing electrode.

### Claim 5 (depends on 3)

The quartz vibrator as set forth in claim 3, further comprising:
a second protective layer including an opening corresponding to a trimming region of the second electrode and formed on the second electrode.

### Claim 6 (depends on 5)

The quartz vibrator as set forth in claim 5, further comprising:
a second pad formed at the peripheral part; and
a second drawing electrode connecting the second pad to the second electrode,
wherein the second protective layer is formed on the second drawing electrode.

### Claim 7 (depends on 4)

The quartz vibrator as set forth in claim 4, wherein the first protective layer comprises an opening corresponding to a central portion of the first pad and formed on the first pad.

### Claim 8 (depends on 6)

The quartz vibrator as set forth in claim 6, wherein the second protective layer comprises an opening corresponding to a central portion of the second pad and formed on the second pad.

### Claim 9 (depends on 1)

The quartz vibrator as set forth in claim 1, wherein the first protective layer is formed on a surface of the first electrode.

### Claim 10 (depends on 1)

The quartz vibrator as set forth in claim 1, wherein the first protective layer is formed on the surface and a side of the first electrode.

### Claim 11 (depends on 5)

The quartz vibrator as set forth in claim 5, wherein the second protective layer is formed on a surface of the second electrode.

### Claim 12 (depends on 5)

The quartz vibrator as set forth in claim 5, wherein the second protective layer is formed on the surface and a side of the second electrode.

### Claim 13 (depends on 1)

The quartz vibrator as set forth in claim 1, wherein the first electrode is provided with a depressed part corresponding to the opening of the first protective layer.

### Claim 14 (depends on 1)

The quartz vibrator as set forth in claim 1, wherein the first protective layer is made of any one selected from the group consisting of aluminum oxide (Al2O3), aluminum nitride (AlN), aluminum oxynitride (AlON), silicon oxide (SiOx), silicon nitride (SiNx), silicon oxynitride (SiOxNy), silicon carbide (SiC), and titanium oxide (TiOx).

### Claim 15

A method for manufacturing a quartz vibrator, comprising:
(A) forming a plurality of reserved first and second electrodes on both surfaces of a reserved quartz substrate;
(B) dividing the reserved quartz substrate into the quartz substrate including one reserved first and second electrodes and formed of an exciting part and a peripheral part by using a metal mask; and
(C) forming a first electrode and a second electrode formed with a first protective layer and a second protective layer after the metal mask and the reserved first and second electrodes are removed.

### Claim 16 (depends on 15)

The method as set forth in claim 15, wherein the step (A) includes:
(A-1) forming a first metal layer and a second metal layer on both surfaces of a reserved quartz substrate;
(A-2) forming a first resist layer on the first metal layer and forming a second resist layer on the second metal layer;
(A-3) patterning the first resist layer and the second resist layer as an electrode pattern; and
(A-4) forming the reserved first and second electrodes by etching the first metal layer and the second metal layer using the first resist layer and the second resist layer.

### Claim 17 (depends on 15)

The method as set forth in claim 15, wherein the step (B) comprises:
(B-1) forming a first metal mask on the reserved first electrode of the quartz substrate and a second metal mask on the reserved second electrode;
(B-2) dividing the reserved quartz substrate into the quartz substrate including one reserved first and second electrodes by using the first and second metal masks and the first and second electrodes; and
(B-3) forming the quartz substrate including the exciting part and the peripheral part by performing half etching using the first and second metal masks.

### Claim 18 (depends on 15)

The method as set forth in claim 15, wherein the step (C) comprises:
(C-1) removing the metal mask and the reserved first and second electrodes;
(C-2) forming a third metal layer on both surfaces of the quartz substrate;
(C-3) forming the first electrode on one surface of the quartz substrate and the second electrode on the other surface thereof by patterning the third metal layer; and
(C-4) forming a first protective layer including an opening corresponding to a trimming region in the first electrode and a second protective layer including an opening corresponding to a trimming region in the second electrode.

### Claim 19 (depends on 18)

The method as set forth in claim 18, wherein the step (C-4) comprises:
forming a first insulating layer stacked on the first electrode on one surface of the quartz substrate;
forming a second insulating layer stacked on the second electrode on the other surface of the quartz substrate;
forming a patterned third resist layer on the first insulating layer;
forming a patterned fourth resist layer on the second insulating layer;
forming a first protective layer by etching the first insulating layer using the third resist layer; and
forming a second protective layer by etching the second insulating layer using the fourth resist layer.

### Claim 20 (depends on 17)

The method as set forth in claim 17, wherein the exciting part of the quartz substrate has a rectangular plate shape, and the peripheral part has a thickness smaller than that of the exciting part and formed around the exciting part.

### Claim 21 (depends on 20)

The method as set forth in claim 20, wherein in the step (C), the first pad formed at the peripheral part and a first drawing electrode connecting the first pad to the first electrode are further formed and the first protective layer is formed on the first drawing electrode.

### Claim 22 (depends on 20)

The method as set forth in claim 20, wherein in the step (C), the second pad formed at the peripheral part and a second drawing electrode connecting the second pad to the second electrode are further formed and the second protective layer is formed on the second drawing electrode.