# US 2015/0145160 A1 · Press moulding method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0145160 A1
- Document ID: US20150145160A1
- Status: Published application
- Kind: A1
- Application number: 14/404,659
- Filed: 2013-05-30
- Published: 2015-05-28
- Earliest claimed: 2012-05-30
- Assignees: Gurit (UK) Ltd.
- Applicants: Gurit (UK) Ltd.
- Inventors: Daniel Thomas Jones; Stephen Patrick Main; Martin James Starkey; Peter Jennings; Gregory Aratoon
- Web page: https://patentgrep.com/patent/US20150145160A1

## CPC

- B29C 70/465: {and impregnating by melting a solid material, e.g. sheets, powders of fibres}
- B29C 43/00: Compression moulding, i.e. applying external pressure to flow the moulding material; Apparatus therefor {(by liberation of internal stresses B29C61/006)}
- B29C 43/18: incorporating preformed parts or layers, e.g. compression moulding around inserts or for coating articles {(B29C43/206 takes precedence)}
- B29C 43/203: {Making multilayered articles}
- B29C 70/08: comprising combinations of different forms of fibrous reinforcements incorporated in matrix material, forming one or more layers, and with or without non-reinforced layers
- B29C 70/086: {and with one or more layers of pure plastics material, e.g. foam layers (applying a non-preformed coating, e.g. a gel-coat, B29C37/0025; with foam blocks B29C70/86)}
- B29C 70/345: {using matched moulds}
- B29C 70/443: {and impregnating by vacuum or injection}
- B29C 70/46: using matched moulds, e.g. for deforming sheet moulding compounds [SMC] or prepregs
- B29C 70/467: {and impregnating the reinforcements during mould closing (B29C70/465 takes precedence)}
- B29C 70/66: the filler comprising hollow constituents, e.g. syntactic foam
- B29C 43/20: Making multilayered or multicoloured articles {(B29C43/14 takes precedence)}
- B29C 2043/563: {combined with mechanical pressure, i.e. mould plates, rams, stampers}
- B29K 2063/00: Use of {EP, i.e.} epoxy resins {or derivatives thereof}, as moulding material
- B29K 2105/0872: {Prepregs}
- B29K 2105/0881: {unidirectional}
- B29K 2307/04: Carbon
- B29K 2309/08: Glass
- B29L 2009/00: Layered products
- B29L 2031/3005: {Body finishings}
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

A method of press moulding a moulding material to form a moulded part of fibre-reinforced resin matrix composite material, the method comprising the steps of: i. providing a mould tool having a lower mould part and an upper mould part, the upper mould part having a first moulding surface for moulding a first moulded surface of the moulded part and the lower mould part having a second moulding surface for moulding a second moulded surface of the moulded part; ii. providing a multilaminar panel of moulding material comprising at least one layer of dry fibres and at least one layer of resin, the multilaminar panel having first and second opposite major surfaces; iii. locating the moulding material in the mould tool; iv. closing the mould tool to define a substantially closed mould cavity containing the moulding material, the closing step including a compression stage, in which the first moulding surface contacts the first major surface and the second moulding surface contacts the second major surface, the compression stage compressing the moulding material to cause progressive resin impregnation of the dry fibres without increasing the resin pressure to a minimum threshold value to cause excessive resin bleed out from the cavity, optionally to reduce any resin bleed out to no more than 600 grams of resin per square metre of the moulding material; v. applying pressure to the moulding material in the mould cavity to configure the moulding material in a fully moulded shape; and vi. substantially fully curing the resin to form a moulded part from the moulding material.

## Claims

### Claim 1

A method of press moulding a moulding material to form a moulded part of fibre-reinforced resin matrix composite material, the method comprising the steps of:
i. providing a mould tool having a lower mould part and an upper mould part, the upper mould part having a first moulding surface for moulding a first moulded surface of the moulded part and the lower mould part having a second moulding surface for moulding a second moulded surface of the moulded part;
ii. providing a multilaminar panel of moulding material comprising at least one layer of dry fibres and at least one layer of resin, the multilaminar panel having first and second opposite major surfaces;
iii. locating the moulding material in the mould tool;
iv. closing the mould tool to define a substantially closed mould cavity containing the moulding material, the closing step including a compression stage, in which the first moulding surface contacts the first major surface and the second moulding surface contacts the second major surface, the compression stage compressing the moulding material to cause progressive resin impregnation of the dry fibres without increasing the resin pressure to a minimum threshold value to cause excessive resin bleed out from the cavity, optionally to reduce any resin bleed out to no more than 600 grams of resin per square metre of the moulding material;
v. applying pressure to the moulding material in the mould cavity to configure the moulding material in a fully moulded shape; and
vi. substantially fully curing the resin to form a moulded part from the moulding material.

### Claim at position 2

-3. (canceled)

### Claim 4 (depends on 1)

A method according to claim 1 wherein the closing step iv includes:
I. a first stage prior to both the first moulding surface contacting the first major surface and the second moulding surface contacting the second major surface and
II. a second stage which comprises the compression stage,
the closure speed of relative movement between the lower and upper mould parts being higher in the first stage than in the second compression stage.

### Claim 5 (depends on 4)

A method according to claim 4 wherein the first stage I of the closing step iv includes the sub-steps of: a. partially closing the mould tool to define a closed intermediate cavity containing the moulding material, the closed intermediate cavity being larger than the moulded part and the first moulding surface of the upper mould part being spaced from the first major surface by a spacing distance, the upper mould part being at an elevated temperature as compared to the temperature of the moulding material; and
b. at least partially evacuating air from the closed intermediate cavity at least while the first moulding surface of the upper mould part is spaced from the first major surface.

### Claim at position 5

-8. (canceled)

### Claim 9 (depends on 5)

A method according to claim 5 wherein prior to the closing step iv the lower and upper mould parts are initially separate, and at an end of a preliminary closing phase in the closing step iv the lower and upper mould parts are mutually engaged to define an initial cavity containing the moulding material.

### Claim 10 (depends on 9)

A method according to claim 9 wherein at the end of the preliminary closing phase a vacuum seal is engaged between the lower mould part and the upper mould part.

### Claim 11 (depends on 10)

A method according to claim 10 wherein the vacuum seal is engaged when the first moulding surface of the upper mould part is spaced from the first major surface by a distance of from 10 to 100 mm.

### Claim 12 (depends on 9)

A method according to claim 9 wherein after the initial cavity has been formed the mould tool is continuously closed to form the substantially closed mould cavity.

### Claim 13 (depends on 5, 9)

A method according to claim 9 when appendant on claim 5 wherein after the initial cavity has been formed the mould tool is discontinuously closed, there being a dwell period at the spacing distance.

### Claim 14 (depends on 1)

A method according to claim 1 wherein a dry fibre layer of the multilaminar panel forms the second major surface, in the locating step iii the second major surface is disposed on the second moulding surface of the lower mould part, and the lower mould part is at an elevated temperature as compared to the temperature of the moulding material and after the applying pressure step v resin in the multilaminar panel fully impregnates the dry fibres.

### Claim 15 (depends on 1)

A method according to claim 1 wherein the closing step iv includes:
c. a preliminary closing phase to achieve mutual engagement between the lower and upper mould parts,
d. “a secondary closing phase after engagement between the lower and upper mould parts with the mould tool partially closed to define a closed intermediate cavity containing the moulding material, the closed intermediate cavity being larger than the moulded part and the first moulding surface of the upper mould part being spaced from the first major surface by a spacing distance, in the secondary phase air being at least partially evacuated from the closed intermediate cavity while the first moulding surface of the upper mould part is spaced from the first major surface to provide a vacuum pressure; and
e. a tertiary closing phase after the vacuum pressure has been provided in the closed intermediate cavity, the tertiary phase including the compression stage.

### Claim 16

(canceled)

### Claim 17 (depends on 15)

A method according to claim 15 wherein at an end of the preliminary closing phase a vacuum seal is engaged between the lower mould part and the upper mould part.

### Claim at position 15

-22. (canceled)

### Claim 23 (depends on 1)

A method according to claim 1 wherein in the applying pressure step v the pressure is applied by gradually increasing the pressure.

### Claim at position 17

-26. (canceled)

### Claim 27 (depends on 1)

A method according to claim 1 further comprising the steps of: vii. separating the upper and lower mould parts; and viii. removing the moulded part from the mould tool.

### Claim 28 (depends on 27)

A method according to claim 27 wherein the removing step viii is carried out while the moulded part is at a temperature which is at least 5° C., optionally at least 10° C., lower than the glass transition temperature Tg of the cured resin.

### Claim 29 (depends on 1)

A method according to claim 1 wherein the mould tool is at a temperature which is within +/−10° C. of a target mould tool temperature throughout the moulding cycle.

### Claim 30 (depends on 27)

A method according to claim 27 wherein the method includes successive moulding cycles for moulding successive moulded parts and the locating step iii of a later cycle directly follows a removing step viii of an earlier cycle.

### Claim 31 (depends on 30)

A method according to claim 30 wherein in the locating step iii of the later cycle the mould tool is at a temperature which is within +/−10° C. of the mould tool temperature during removing step viii of the earlier cycle.

### Claim 32 (depends on 1)

A method according to claim 1 wherein a vacuum pressure is applied during the closing step iv and the pressure applying step v.

### Claim 33 (depends on 32)

A method according to claim 32 wherein the vacuum pressure is released during the curing step vi.

### Claim 34 (depends on 1)

A method according to claim 1 wherein the method forms a vehicle body panel of fibre-reinforced resin matrix composite material, the vehicle body panel having a front A-surface and a rear B-surface, the mould is heated and the first moulding surface moulds a front A-surface of the vehicle body panel and the second moulding surface moulds a rear B-surface of the vehicle body panel, the vehicle body panel having a front A-surface formed from the first major surface and a rear B-surface formed from the second major surface.

### Claim 35 (depends on 1)

A method according to claim 1 wherein the moulding material further comprises a syntactic layer comprising a polymer matrix and a plurality of hollow particles distributed within the polymer matrix.

### Claim 36 (depends on 38)

A method according to claim 38 wherein the syntactic layer is a core layer between first and second dry fibre layers.

### Claim 37 (depends on 35)

A method according to claim 35 wherein in locating step iii the moulding material drapes by bending about a neutral axis substantially centrally located with respect to the thickness of the moulding material, the neutral axis being located within the syntactic layer.

### Claim 38 (depends on 1)

A method according to claim 1 wherein the resin comprises a thermosetting resin, optionally an epoxy resin.

### Claim 39 (depends on 1)

A method according to claim 1 wherein in locating step iii the moulding material is heated to cause the viscosity of the resin initially to decrease as a result of an increase in resin temperature and then to increase as a result of initiation of curing prior to step vi.

### Claim 40 (depends on 1)

A method according to claim 1 wherein in locating step iii the second major surface is draped onto the second moulding surface.

### Claim 41 (depends on 1)

A method according to claim 1 wherein locating step iii to curing step vi are carried out at an elevated temperature above the curing temperature of the resin.

### Claim 42 (depends on 1)

A method according to claim 1 wherein in locating step iii a reduced pressure is applied to the mould cavity to increase the drape of the moulding material.

### Claim 43 (depends on 1)

A method according to claim 1 wherein in the moulding material a layer of carbon fibres is adjacent to a respective layer of resin.

### Claim 44 (depends on 43)

A method according to claim 43 wherein the moulding material comprises a syntactic core layer between a first carbon fibre layer and a second dry glass fibre layer defining the second major surface, each fibre layer being adjacent to a layer of resin.

### Claim 45 (depends on 44)

A method according to claim 44 wherein the surface resin layer is on the first major surface of the moulding material and is adjacent to the first carbon fibre layer.

### Claim 46 (depends on 1)

A method according to claim 1 wherein the moulding material comprises the surface resin layer, a syntactic core layer, a carbon fibre layer and a first resin layer between the surface resin layer and the syntactic core layer, a dry glass fibre layer defining the second major surface, and a second resin layer between the syntactic core layer and the dry glass fibre layer.

### Claim 47 (depends on 1)

A method according to claim 1 wherein the first moulding surface faces substantially downwardly and the second moulding surface faces substantially upwardly.

### Claim 48 (depends on 1)

A method according to claim 1 wherein the moulding material located in the mould tool in the locating step iii has a greater thickness than the moulded part and the closing step iv compresses the moulding material in the substantially closed mould cavity prior to the applying pressure step v.

### Claim 49 (depends on 1)

A method according to claim 1 wherein in the moulding material the at least one layer of resin comprises thermosetting resin and the at least one layer of fibres comprises a woven fabric of carbon or glass fibres, optionally at least one or each woven fabric being substantially unimpregnated with any resin.

### Claim 50 (depends on 1)

A method according to claim 1 in the moulding material at least one layer of resin is adjacent to at least one layer of fibres, optionally at least one or each layer of fibres being substantially unimpregnated with any resin.

### Claim 51 (depends on 1)

A method according to claim 1 wherein the moulding material does not comprise a sheet moulding compound (SMC).