# US 2015/0145157 A1 · Production and reparation of non-porous laminates with assessable low degree of fiber content

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0145157 A1
- Document ID: US20150145157A1
- Status: Published application
- Kind: A1
- Application number: 14/551,350
- Filed: 2014-11-24
- Published: 2015-05-28
- Earliest claimed: 2013-11-25
- Assignees: Airbus Helicopters Deutschland GmbH
- Applicants: Airbus Helicopters Deutschland GmbH
- Inventors: Hannes ROEPLING; Oliver MARTINEZ GANDULLO; Markus ZELLHUBER
- Web page: https://patentgrep.com/patent/US20150145157A1

## CPC

- B29C 70/443: {and impregnating by vacuum or injection}
- B29C 73/10: using patches sealing on the surface of the article (B29C73/14 takes precedence)
- B29K 2063/00: Use of {EP, i.e.} epoxy resins {or derivatives thereof}, as moulding material
- B29K 2307/04: Carbon
- B29L 2031/082: {Blades, e.g. for helicopters}
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

A method of forming a fiber reinforced composite structure having a fiber volume fraction (14) below 50 vol.-% using vacuum bag molding, the method comprising the steps of placing an assembly of fiber laminates (3) on a tool surface (1.1), creating a predetermined maximum difference of pressure (10) between the inside and the outside of an airtight envelope (4), infusing resin into the assembly of fiber laminates (3), reducing the difference of pressure between the inside and the outside of the airtight envelope (4), so that the assembly of fiber laminates (3) expands and the infusion of resin into the assembly of fiber laminates (3) continues thus forming a resin infused assembly of fiber laminates (3), and curing the resin infused assembly of fiber laminates (3).

## Claims

### Claim 1

A method of forming a fiber reinforced composite structure having a fiber volume fraction below 50 vol.-% using vacuum bag molding, the method comprising the steps of:
placing an assembly of fiber laminates on a tool surface;
placing a vacuum bag comprising a resin inlet over said assembly of fiber laminates and sealing the vacuum bag against the tool surface, thus forming an airtight envelope;
creating a predetermined maximum difference of pressure between the inside and the outside of the airtight envelope;
infusing resin into the assembly of fiber laminates through the resin inlet of the vacuum bag while keeping the maximum difference of pressure, until the assembly of fiber laminates is completely filled with resin, during a first infusion time;
during a second infusion time, reducing the difference of pressure between the inside and the outside of the airtight envelope, such difference of pressure reaching during this step a predetermined minimum value, inferior to the predetermined maximum difference of pressure, so that the assembly of fiber laminates expands and infusing resin into the assembly of fiber laminates continues thus forming a resin infused assembly of fiber laminates;
closing the resin inlet;
curing the resin infused assembly of fiber laminates at a minimum value of the difference of pressure between the inside and the outside of the airtight envelope reached during the second infusion time, thus forming a fiber reinforced composite structure having a fiber volume fraction below 50 vol.-%.

### Claim 2 (depends on 1)

A method according to claim 1, wherein there is a linear reduction of the difference of pressure between the inside and the outside of the airtight envelope during the second infusion time.

### Claim 3 (depends on 1)

A method according to claim 1, wherein a reduction of the difference of pressure between the inside and the outside of the airtight envelope during the second infusion time describes a linear decrease followed by a constant pressure interval.

### Claim 4 (depends on 3)

A method according to claim 3, wherein the linear decrease is an instant decrease so that a function described by the difference of pressure between the inside and the outside of the airtight envelope during the second infusion time is a step function.

### Claim 5 (depends on 1)

A method according to claim 1, wherein the second infusion time is comprised between 1 and 7 minutes.

### Claim 6 (depends on 1)

A method according to claim 1, wherein the step of infusing resin into the assembly of fiber laminates during the first and second infusion times is carried out at a temperature between 60° C. and 80° C.

### Claim 7 (depends on 1)

A method according to claim 1, wherein the step of infusing resin into the assembly of fiber laminates during the first and second infusion times is carried out at a temperature between 100° C. and 120° C.

### Claim 8 (depends on 1)

A method according to claim 1, wherein the fiber of the assembly of fiber laminates is carbon fiber.

### Claim 9 (depends on 1)

A method according to claim 1, wherein the assembly of fiber laminates comprises fiber reinforced laminates from a fiber reinforced composite part which is to be repaired and additional fiber preforms.

### Claim 10 (depends on 1)

A method according to claim 1, in which the fiber reinforced composite structure is a rotatory aircraft part.

### Claim 11 (depends on 10)

A method according to claim 10, in which the rotatory aircraft part is a rotor blade.

### Claim 12 (depends on 1)

A method according to claim 1, wherein the predetermined maximum difference of pressure between the inside and the outside of the airtight envelope is between 750 mbar and 1000 mbar.

### Claim 13 (depends on 1)

A method according to claim 1, wherein a predetermined minimum difference of pressure between the inside and the outside of the airtight envelope is between 100 mbar and 750 mbar.

### Claim 14 (depends on 1)

A method according to claim 1, wherein a predetermined maximum difference of pressure between the inside and the outside of the airtight envelope is between 900 mbar and 1000 mbar, and wherein the predetermined minimum difference of pressure between the inside and the outside of the airtight envelope is between 400 mbar and 750 mbar.

### Claim 15 (depends on 1)

A method according to claim 1, wherein the resin is a high temperature epoxy resin.