# US 2015/0145155 A1 · Method of manufacturing hydrogel ophthalmic devices with electronic elements

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0145155 A1
- Document ID: US20150145155A1
- Status: Published application
- Kind: A1
- Application number: 14/087,366
- Filed: 2013-11-22
- Published: 2015-05-28
- Earliest claimed: 2013-11-22
- Assignees: Johnson & Johnson Vision Care, Inc.
- Applicants: Johnson & Johnson Vision Care, Inc.
- Inventors: Randall Braxton Pugh; Karson Putt; Michael Ferran; Katherine Rowan Hardy; Daniel B. Otts
- Web page: https://patentgrep.com/patent/US20150145155A1

## CPC

- B29C 43/02: of articles of definite length, i.e. discrete articles {(B29C35/0227 takes precedence)}
- B29D 11/00153: {Differential curing, e.g. by differential radiation}
- B29C 39/18: incorporating preformed parts or layers, e.g. casting around inserts or for coating articles {(B29C39/206 takes precedence)}
- B29D 11/00009: {Production of simple or compound lenses}
- B29D 11/00038: {Production of contact lenses}
- B29D 11/00125: {Auxiliary operations, e.g. removing oxygen from the mould, conveying moulds from a storage to the production line in an inert atmosphere}
- B29D 11/00807: {Producing lenses combined with electronics, e.g. chips}
- B29D 11/00826: {with energy receptors for wireless energy transmission}
- B29K 2083/00: Use of polymers having silicon, with or without sulfur, nitrogen, oxygen, or carbon only, in the main chain, as moulding material
- B29L 2011/0041: {Contact lenses}
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

The present invention provides methods for forming an ophthalmic lens that can include a media insert and/or electronic components. In particular, the present disclosure provides for adhesion promoting functionalization steps for a biocompatible coating to bind a hydrogel material to a plastic surface or electronic component prior to the polymerization of the hydrogel. In some aspects, the media insert can be used to contain energy sources and/or functional electronic components which may be, for example, in a stacked integrated component configuration to permit a generally arcuate shape that can conform to the anterior surface of an eye.

## Claims

### Claim 1

A method of forming an energized ophthalmic device, the method comprising:
pre-dosing a first mold part with a pre-dose amount of a reactive monomer mixture;
functionalizing a media insert so that an adhesion promoter can bind to a surface of said media insert;
applying an adhesion promoter to the functionalized media insert;
coating said media insert including the adhesion promoter;
placing the media insert on said pre-dose of reactive monomer mixture;
pre-curing the pre-dosed reactive monomer mixture to fixedly hold the media insert proximate to the first mold part;
post-dosing the first mold part with a post-dose of a reactive monomer mixture;
placing a second mold part proximate to the first mold part, wherein the placing forms a ophthalmic device mold assembly with a lens forming cavity; and
curing at least the post-dosed reactive monomer mixture to form the ophthalmic lens.

### Claim 2 (depends on 1)

The method of claim 1, wherein the functionalizing step includes providing a plasma treatment in an oxygen environment.

### Claim 3 (depends on 1)

The method of claim 1, wherein the functionalizing step includes exposing the media insert to an ozone environment.

### Claim 4 (depends on 1)

The method of claim 1, wherein the functionalizing step includes crosslinking a chemical with the media insert.

### Claim 5 (depends on 4)

The method of claim 4, wherein the functionalizing step further includes exposing the media insert to a radiation to crosslink said chemical with the media insert.

### Claim 6 (depends on 1)

The method of claim 1, wherein the adhesion promoter includes a methoxy-silane chemical.

### Claim 7 (depends on 6)

The method of claim 6, wherein the methoxy-silane can include one of more of a vinyldimethylethoxysilane, a methoxysilane, a trimethoxysilane, a styrylethyltrimethoxysilane, a bis(trimethoxysilyl)hexane, and a vinylmethoxysiloxane homopolymer.

### Claim 8 (depends on 1)

The method of claim 1, wherein the coating is a parylene coating.

### Claim 9 (depends on 1)

The method of claim 1, wherein the coating is a polymerizable hydrogel coating.

### Claim 10

A method of forming an energized ophthalmic device, the method comprising:
pre-dosing a first mold part with a pre-dose amount of a reactive monomer mixture;
functionalizing an electronic element so that an adhesion promoter can bind to a surface of said electronic element;
applying an adhesion promoter to the functionalized electronic element;
coating said electronic element including the adhesion promoter;
placing the electronic element on said pre-dose of reactive monomer mixture;
pre-curing the pre-dosed reactive monomer mixture to fixedly hold the electronic element proximate to the first mold part;
post-dosing the first mold part with a post-dose of a reactive monomer mixture;
placing a second mold part proximate to the first mold part, wherein the placing forms an ophthalmic device mold assembly with a lens forming cavity; and
curing at least the post-dosed reactive monomer mixture to form the energized ophthalmic lens.

### Claim 11 (depends on 10)

The method of claim 10, wherein the functionalizing step includes providing a plasma treatment in an oxygen environment.

### Claim 12 (depends on 10)

The method of claim 10, wherein the functionalizing step includes exposing the media insert to an ozone environment.

### Claim 13 (depends on 10)

The method of claim 10, wherein the functionalizing step includes crosslinking a chemical with the media insert.

### Claim 14 (depends on 13)

The method of claim 13, wherein the functionalizing step further includes exposing the media insert to a radiation to crosslink said chemical with the media insert.

### Claim 15 (depends on 10)

The method of claim 10, wherein the adhesion promoter includes a methoxy-silane chemical.

### Claim 16 (depends on 15)

The method of claim 15, wherein the methoxy-silane can include one of more of a vinyldimethylethoxysilane, a methoxysilane, a trimethoxysilane, a styrylethyltrimethoxysilane, a bis(trimethoxysilyl)hexane, and a vinylmethoxysiloxane homopolymer.

### Claim 17 (depends on 10)

The method of claim 10, wherein the coating is a parylene coating.

### Claim 18 (depends on 10)

The method of claim 10, wherein the coating is a polymerizable hydrogel coating.

### Claim 19

A method of forming an energized ophthalmic device, the method comprising:
functionalizing an electronic element so that an adhesion promoter can bind to a surface of said electronic element;
applying an adhesion promoter to the functionalized electronic element;
coating said electronic element including the adhesion promoter with a parylene layer; and
fixing said coated electronic element in a hydrogel ophthalmic device.

### Claim 20 (depends on 19)

The method of claim 19, additionally comprising:
depositing coated energy source; and
forming an electrical connection between said coated electronic element and said deposited coated energy source.