# US 2015/0145130 A1 · Semiconductor packaging and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0145130 A1
- Document ID: US20150145130A1
- Status: Published application
- Kind: A1
- Application number: 14/088,513
- Filed: 2013-11-25
- Published: 2015-05-28
- Earliest claimed: 2013-11-25
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company Ltd.
- Inventors: HSIU-JEN LIN; WEN-HSIUNG LU; CHENG-TING CHEN; HSUAN-TING KUO; WEI-YU CHEN; MING-DA CHENG; CHUNG-SHI LIU
- Web page: https://patentgrep.com/patent/US20150145130A1

## CPC

- H10W 90/701: {characterised by the relative positions of pads or connectors relative to package parts}
- H05K 1/111: {Pads for surface mounting, e.g. lay-out}
- H05K 3/34: by soldering
- H10W 70/65: Shapes or dispositions of interconnections
- H10W 74/129: {forming a chip-scale package [CSP]}
- H10W 70/655: Fan-out layouts
- H10W 70/656: Fan-in layouts
- H10W 70/66: Conductive materials thereof
- H10W 72/012: {of bump connectors, dummy bumps or thermal bumps}
- H10W 72/01204: {using temporary auxiliary members, e.g. using sacrificial coatings or handle substrates}
- H10W 72/01225: {in solid form, e.g. by using a powder or by stud bumping}
- H10W 72/019: {of bond pads}
- H10W 72/01951: {Changing the shapes of bond pads}
- H10W 72/072: {of bump connectors}
- H10W 72/07231: {Techniques}
- H10W 72/07234: {Using a reflow oven}
- H10W 72/07235: {Applying EM radiation, e.g. induction heating or using a laser}
- H10W 72/07236: {Soldering or alloying}
- H10W 72/07253: {changes in shapes}
- H10W 72/07353: {changes in shapes}
- H10W 72/221: {Structures or relative sizes}
- H10W 72/232: {Plan-view shape, i.e. in top view}
- H10W 72/234: {Cross-sectional shape, i.e. in side view}
- H10W 72/241: {Dispositions, e.g. layouts}
- H10W 72/242: {relative to the surface, e.g. recessed, protruding}
- H10W 72/248: {Top-view layouts, e.g. mirror arrays}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/283: {Reinforcing structures, e.g. bump collars}
- H10W 72/29: Bond pads specially adapted therefor
- H10W 72/334: {Cross-sectional shape, i.e. in side view}
- H10W 72/354: {comprising polymers}
- H10W 72/923: {Bond pads having multiple stacked layers}
- H10W 72/925: {Bond pads having a filler embedded in a matrix}
- H10W 72/9415: {relative to the surface, e.g. recessed, protruding}
- H10W 72/942: {relative to underlying supporting features, e.g. bond pads, RDLs or vias}
- H10W 72/952: {comprising metals or metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/953: {not comprising solid metals or solid metalloids, e.g. polymers, ceramics or liquids}
- H10W 74/00: Encapsulations, e.g. protective coatings
- H10W 74/012: {of encapsulations on active surfaces of flip-chip devices, e.g. forming underfills}
- H10W 74/15: on active surfaces of flip-chip devices, e.g. underfills
- H10W 90/722: {between stacked chips}
- H10W 90/724: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W 90/732: {between stacked chips}
- H10W 90/734: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W 99/00: Subject matter not provided for in other groups of this subclass
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

The present disclosure provides a semiconductor package includes a contact pad, a device external to the contact pad and a solder bump on the contact pad. The device has a conductive contact pad corresponding to the contact pad. The solder bump connects the contact pad with the conductive contact pad. The solder bump comprises a height from a top of the solder bump to the contact pad; and a width which is a widest dimension of the solder bump in a direction perpendicular to the height. A junction portion of the solder bump in proximity to the contact pad comprises an hourglass shape.

## Claims

### Claim 1

A semiconductor package, comprising:
a contact pad;
a device external to the contact pad and including a conductive contact pad corresponding to the contact pad;
a solder bump connecting the contact pad with the conductive contact pad, wherein the solder bump comprises:
a height from a top of the solder bump to the contact pad; and
a width which is a widest dimension of the solder bump in a direction perpendicular to the height; and
wherein a junction portion of the solder bump in proximity to the contact pad comprises an hourglass shape.

### Claim 2 (depends on 1)

The semiconductor package in claim 1, further comprising a molding compound surrounding the junction portion and a lower portion of the solder bump, wherein a thickness of the molding compound is from about 0.4 times to about 0.6 times of the height of the solder bump, and wherein the lower portion of the solder bump is in proximity to the contact pad.

### Claim 3 (depends on 2)

The semiconductor package in claim 2, further comprising an underfill layer surrounding an upper portion of the solder bump, wherein the upper portion of the solder bump is in proximity to the top of the solder bump.

### Claim 4 (depends on 1)

The semiconductor package in claim 1, wherein the height to the width ratio of the solder bump is about from 0.85 to about 1.15.

### Claim 5 (depends on 1)

The semiconductor package in claim 1, wherein the junction portion of the solder bump comprises SnX alloys having an alloy melting temperature lower than 165 degrees Celsius.

### Claim 6 (depends on 5)

The semiconductor package in claim 5, wherein the X in the SnX alloys comprises Bi, Sb, Pb, Ge, Al, Ga, In, Tl, and the arbitrary combination thereof

### Claim 7 (depends on 5)

The semiconductor package in claim 5, wherein a concentration of X decreases from the junction portion of the solder bump to the top of the solder bump.

### Claim 8 (depends on 1)

The semiconductor package in claim 1, wherein the solder bump comprises Sn, Ag, Cu, Pb, Bi, Sb, and the arbitrary combination thereof

### Claim 9

A semiconductor package, comprising:
a ball grid array (BGA) including a plurality of contact pads, wherein each of the plurality of contact pads is connected with a solder bump at one end of the solder bump, wherein a finest pitch in the BGA is less than about 0.2 mm; and,
a circuit board including a plurality of conductive contact pads, wherein each of the plurality of conductive contact pads is electrically connected with the BGA at the other end of the solder bump;
wherein the solder bump includes:
a height from a top of the solder bump to the contact pad; and
a width which is a widest dimension of the solder bump in a direction perpendicular to the height; and
wherein a junction portion of the solder bump in proximity to the contact pad comprises an hourglass shape.

### Claim 10 (depends on 9)

The semiconductor package in claim 9, wherein the solder bump comprises a zero curvature.

### Claim 11 (depends on 9)

The semiconductor package in claim 9, an angle between the contact pad and a narrowest point on a contour of the junction portion of the solder bump is less than 90 degrees.

### Claim 12

A method of manufacturing a semiconductor package, comprising:
forming a solder paste layer on a contact pad;
positioning a solder bump on the solder paste layer;
forming a first electrical connection between the solder bump and the contact pad;
encapsulating the solder paste layer and a lower portion of the solder bump, wherein the lower portion of the solder bump is in proximity to the contact pad; and
forming a second electrical connection between the solder bump and an external device.

### Claim 13 (depends on 12)

The method of manufacturing a semiconductor package in claim 12, further comprising forming an underfill layer surrounding an upper portion of the solder bump, wherein the upper portion of the solder bump is in proximity to the external device.

### Claim 14 (depends on 12)

The method of manufacturing a semiconductor package in claim 12, wherein the forming the first electrical connection between the solder bump and the contact pad comprises heating the solder paste layer to a first temperature.

### Claim 15 (depends on 14)

The method of manufacturing a semiconductor package in claim 14, wherein a melting point of the solder paste is lower than the first temperature, and wherein the first temperature is lower than a melting point of the solder bump.

### Claim 16 (depends on 15)

The method of manufacturing a semiconductor package in claim 15, wherein the first temperature is lower than 170 degrees Celsius.

### Claim 17 (depends on 12)

The method of manufacturing a semiconductor package in claim 12, wherein the forming the second electrical connection between the solder bump and the external device comprises heating the solder paste layer and the solder bump to a second temperature.

### Claim 18 (depends on 17)

The method of manufacturing a semiconductor package in claim 17, wherein a melting point of the solder paste is lower than a melting point of the solder bump, and wherein the melting point of the solder bump is lower than the second temperature.

### Claim 19 (depends on 18)

The method of manufacturing a semiconductor package in claim 18, wherein the second temperature is at least 50 degrees Celsius greater than the first temperature.

### Claim 20 (depends on 12)

The method of manufacturing a semiconductor package in claim 12, wherein
the forming the solder paste layer on the contact pad comprises forming the solder paste with a thickness of T, and
the positioning the solder bump on the solder paste layer comprises positioning the solder bump with a width of W, wherein the width W is a widest dimension of the solder bump in a horizontal direction, and
wherein a W/T ratio is of from about 2 to about 5.