# US 2015/0145099 A1 · Formation Of Semiconductor Device With Resistors

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0145099 A1
- Document ID: US20150145099A1
- Status: Published application
- Kind: A1
- Application number: 14/091,643
- Filed: 2013-11-27
- Published: 2015-05-28
- Earliest claimed: 2013-11-27
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing CO., LTD.
- Inventors: Yu-Jen Chen; Ping-Pang Hsieh; Hsin-Chi Chen
- Web page: https://patentgrep.com/patent/US20150145099A1

## CPC

- H10D 84/209: {of only resistors}
- H10D 1/47: Resistors having no potential barriers
- H10D 62/115: {Dielectric isolations, e.g. air gaps}
- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/212: {Through-implantation}
- H10P 30/28: characterised by an annealing step, e.g. for activation of dopants
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor device includes a semiconductor substrate, trench isolations, a sacrificial layer, a first resist protect oxide (RPO) layer, a second RPO layer and a silicide layer. The semiconductor substrate has first portions and second portions which are alternately disposed, and each of the second portions includes a first resist region with a first resistance, a second resist region with a second resistance and a silicide region. The second resistance is greater than the first resistance. The trench isolations are in the first portions. The sacrificial layer is on the first resist region. The first RPO layer is on the sacrificial layer. The first RPO layer together with the sacrificial layer have a first thickness. The second RPO layer is on the second resist region, in which the second RPO layer has a second thickness smaller than the first thickness. The silicide layer is on the silicide region.

## Claims

### Claim 1

A method for fabricating a semiconductor device, the method comprising:
providing a semiconductor substrate with a plurality of first portions and a plurality of second portions which are alternately disposed, wherein each of the second portions comprises a first resist region and a second resist region;
forming a plurality of trench isolations in the first portions of the semiconductor substrate;
forming a first sacrificial layer and a second sacrificial layer respectively on the first resist region and on the second resist region;
implanting doping ions into the second portions of the semiconductor substrate;
removing the second sacrificial layer from the second resist region with the first resist region still covered by the first sacrificial layer; and
annealing the semiconductor substrate to homogenize the doping ions in the first resist region and the second resist region, and to diffuse a portion of the doping ions out of the second resist region, thereby having the second resist region with a remaining doping concentration, wherein a resistance of the second resist region is greater than that of the first resist region.

### Claim 2 (depends on 1)

The method of claim 1, wherein the operation of implanting the doping ions forms the second portions of the semiconductor substrate with a doping concentration, and the doping concentration is substantially in a range from 1014 to 1016/cm3.

### Claim 3 (depends on 2)

The method of claim 2, wherein the remaining doping concentration of the second resist region is substantially in a range from 1011/cm3 to 1014/cm3.

### Claim 4 (depends on 1)

The method of claim 1, wherein the operation of annealing the semiconductor substrate comprises annealing the semiconductor substrate using a rapid thermal annealing (RTA) process.

### Claim 5 (depends on 1)

The method of claim 1, wherein the operation of annealing the semiconductor substrate comprises annealing the semiconductor substrate using an annealing temperature substantially in a range from 700° C. to 1200° C. for a period of annealing time substantially greater than 0 and smaller than or equal to 1 hour.

### Claim 6 (depends on 1)

The method of claim 1, wherein the implanting doping ions comprise boron, phosphor, carbon or arsenic.

### Claim 7

A method for fabricating a semiconductor device, the method comprising:
providing a semiconductor substrate with a plurality of first portions and a plurality of second portions which are alternately disposed, wherein each of the second portions comprises a first resist region, a second resist region and a silicide region;
forming a plurality of trench isolations in the first portions of the semiconductor substrate;
forming a first sacrificial layer, a second sacrificial layer and a third sacrificial layer respectively on the first resist region, the second resist region and the silicide region;
implanting doping ions into the second portions of the semiconductor substrate;
removing the second sacrificial layer from the second resist region with the first resist region still covered by the first sacrificial layer;
annealing the semiconductor substrate to homogenize the doping ions in the first resist region, the second resist region and the silicide region, and to diffuse a portion of the doping ions out of the second resist region, thereby having the second resist region with a remaining doping concentration, wherein a resistance of the second resist region is greater than that of the first resist region;
removing the third sacrificial layer from the silicide region;
forming a first resist protect oxide layer and a second resist protect oxide layer respectively on the first sacrificial layer and on the second resist region; and
forming a silicide layer on the silicide region.

### Claim 8 (depends on 7)

The method of claim 7, wherein the operation of implanting the doping ions forms the second portions of the semiconductor substrate with a doping concentration, and the doping concentration is substantially in a range from 1014 to 1016/cm3.

### Claim 9 (depends on 8)

The method of claim 8, wherein the remaining doping concentration of the second resist region is substantially in a range from 1011/cm3 to 1014/cm3.

### Claim 10 (depends on 7)

The method of claim 7, wherein the operation of annealing the semiconductor substrate comprises annealing the semiconductor substrate using a rapid thermal annealing (RTA) process.

### Claim 11 (depends on 7)

The method of claim 7, wherein the operation of annealing the semiconductor substrate comprises annealing the semiconductor substrate using an annealing temperature substantially in a range from 700° C. to 1200° C. for a period of annealing time substantially greater than 0 and smaller than or equal to 1 hour.

### Claim 12 (depends on 7)

The method of claim 7, wherein the implanting doping ions comprise boron, phosphor, carbon or arsenic.

### Claim 13 (depends on 7)

The method of claim 7, wherein the operation of forming the silicide layer comprises forming the silicide layer on the silicide region using a self-aligned silicide (salicide) process.

### Claim at position 14

14-20. (canceled)

### Claim 21 (depends on 7)

The method of claim 7, wherein the operation of forming the first resist protect oxide layer and the second resist protect oxide layer further comprises the first resist protect oxide layer together with the first sacrificial layer have a first thickness, and the second resist protect oxide layer has a second thickness smaller than the first thickness.

### Claim 22 (depends on 21)

The method of claim 21, wherein the first thickness is substantially in a range from 10 to 110 nm and the second thickness is substantially greater than 0 and smaller than or equal to 30 nm.

### Claim 23 (depends on 21)

The method of claim 21, wherein the first resist protect oxide layer has a third thickness the same with the second thickness.

### Claim 24 (depends on 7)

The method of claim 7, wherein after the operation of annealing the semiconductor substrate, the resistance of the first resist region is substantially in a range from 100 Ohm/sqr to 400 Ohm/sqr.

### Claim 25 (depends on 7)

The method of claim 7, wherein after the operation of annealing the semiconductor substrate, the resistance of the second resist region is substantially in a range from 300 Ohm/sqr to 3000 Ohm/sqr.

### Claim 26 (depends on 1)

The method of claim 1, wherein after the operation of annealing the semiconductor substrate, the resistance of the first resist region is substantially in a range from 100 Ohm/sqr to 400 Ohm/sqr.

### Claim 27 (depends on 1)

The method of claim 1, wherein after the operation of annealing the semiconductor substrate, the resistance of the second resist region is substantially in a range from 300 Ohm/sqr to 3000 Ohm/sqr.