# US 2015/0144954 A1 · Method for heteroepitaxial growth of iii metal-face polarity iii-nitrides on substrates with diamond crystal structure and iii-nitride semiconductors

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0144954 A1
- Document ID: US20150144954A1
- Status: Published application
- Kind: A1
- Application number: 14/396,842
- Filed: 2013-04-24
- Published: 2015-05-28
- Earliest claimed: 2012-04-25
- Assignees: Foundation for Research and Technology
- Applicants: Foundation for Research and Technology
- Inventors: Alexandros Georgakilas; Kleopatra Aretouli; Katerina Tsagaraki
- Web page: https://patentgrep.com/patent/US20150144954A1

## CPC

- H10P 14/3416: {Nitrides}
- C30B 23/02: Epitaxial-layer growth
- C30B 29/403: {AIII-nitrides}
- H10D 30/475: {having wider bandgap layer formed on top of lower bandgap active layer, e.g. undoped barrier HEMTs such as i-AlGaN/GaN HEMTs}
- H10D 62/8503: {Nitride Group III-V materials, e.g. AlN or GaN}
- H10P 14/22: using physical deposition, e.g. vacuum deposition or sputtering
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/274: {using seed materials}
- H10P 14/2902: {being Group IVA materials}
- H10P 14/2903: {Carbon, e.g. diamond-like carbon}
- H10P 14/2904: {Silicon carbide}
- H10P 14/2924: {Structures}
- H10P 14/2926: {Crystal orientations}
- H10P 14/3216: {Nitrides}
- H10P 14/3248: {consisting of two layers}
- H10P 14/3258: {Crystal orientation}
- H10P 14/3602: {In-situ cleaning}
- H10P 14/6506: {Formation of intermediate materials}
- H10P 14/6514: {by exposure to a plasma}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

The present invention discloses a method of heteroepitaxial growth enabling the successful growth of thin films of GaN and III-nitride semiconductor heterostructures of (0001) orientation with III metal-face polarity on diamond substrates being either polycrystalline or single crystal with various crystallographic orientations. The method uses a thin AlN nucleation layer on the diamond substrate with thickness equal or less than 5 nm, grown by Molecular Beam Epitaxy (MBE) using a nitrogen plasma source. The invention enables the development of very high power metal-face III-nitride devices, such as High Electron Mobility Transistors, on single crystal or polycrystalline diamond substrates. The method is also applicable for other element IV substrates with diamond crystal structure.

## Claims

### Claim at position 1

1-16. (canceled)

### Claim 17

A method of heteroepitaxial growth of III-Nitride semiconductors on a substrate achieving (0001) orientation and metal-face polarity for a first nucleation layer and the subsequent layers, comprising the following steps:
utilizing an N2 gas plasma source for epitaxy to deposit an Al-face polarity (0001) AlN nucleation layer less than 5 nm in deposited layer thickness to minimize degradation of the epitaxial growth of the AlN layer and inversion of its polarity;
depositing said AlN layer on a substrate independent of the crystalline surface orientation of said substrate, said substrate being selected from the group of a single-crystal diamond, a polycrystalline diamond, silicon, germanium or an alloy with chemical formula SixCyGe1−(x+y), whereby 0≦x, y≦1, 0≦x+y≦1 and x or y less than 0.5; and
by the cooperation between said utilizing an N2 gas plasma source for epitaxy and said depositing of said AlN layer less than 5 nm thickness, enabling the subsequent depositing on said AlN layer of one or more additional layers while preserving said (0001) orientation and III metal-face polarity.

### Claim 18 (depends on 17)

The method according to claim 17, further comprising:
said substrate being any one of a single-crystal diamond or polycrystalline diamond.

### Claim 19 (depends on 18)

The method according to claim 18, further comprising:
exposing said substrate to active nitrogen species produced by a nitrogen plasma source before the growth of said AlN layer.

### Claim 20 (depends on 17)

The method according to claim 17, further comprising:
between steps of depositing of said AlN layer and overgrowing of said layer by a III-nitride compound layer, exposing said AlN layer to active nitrogen species produced by a nitrogen plasma source.

### Claim 21 (depends on 20)

The method according to claim 20, further comprising:
said III-nitride compound layer being a GaN layer.

### Claim 22 (depends on 21)

The method according to claim 21, further comprising:
said overgrowing by said GaN layer being carried out by Molecular Beam Epitaxy (MBE) using a solid evaporation source for the Ga beam, maintaining the temperature of said substrate at 710±40° C. and maintaining the Ga/N flux ratio in a range of 1.5±0.5, where the flux of N atoms corresponds to said active nitrogen species produced by a nitrogen plasma source and which flux of N atoms are incident on said substrate.

### Claim 23 (depends on 17)

The method according claim 17, further comprising:
overgrowing said AlN layer by a III-Nitride compound layer, and overgrowing said III-Nitride compound layer by at least one layer of a III-Nitride compound.

### Claim 24 (depends on 23)

The method according to claim 23, further comprising:
between said overgrowing of said layers of said one or more III-Nitride compounds, interrupting said overgrowing and during said interrupting, exposing the surface of at least one of said layers to active nitrogen species produced by a nitrogen plasma source.

### Claim 25 (depends on 17)

The method according to claim 17, further comprising:
utilizing for the growth of said AlN layer Molecular Beam Epitaxy (MBE) using a solid evaporation source for the beam of Al, and maintaining the temperature of said substrate at 800±50° C.;
utilizing an Al/N flux ratio equal to 1.0±0.1, where the flux of N atoms corresponds to the active nitrogen species produced by said plasma source and which flux of N atoms is incident on the substrate; and
depositing by said solid evaporation source a thickness of said AlN layer equal to 1.7±0.1 nm.

### Claim 26 (depends on 17)

The method according claim 17, further comprising:
said AlN layer being less than 3.5 nm.

### Claim 27

A III-Nitride semiconductor device comprising:
a substrate, said substrate being selected from the group of a single-crystal diamond, a polycrystalline diamond, silicon, germanium or an alloy with chemical type SixCyGe1−(x+y), whereby 0≦x, y≦1, 0≦x+y≦1 and x or y less than 0.5;
an Al-face polarity (0001) AlN nucleation layer on said substrate having a thickness of less than 5 nm; and
at least one III-Nitride compound layer over said AlN layer, said cooperation resulting in (0001) orientation and III metal-face polarity.

### Claim 28 (depends on 27)

The III-Nitride semiconductor device according to claim 27, further comprising:
said substrate being selected from the group of single-crystal diamond or polycrystalline diamond.

### Claim 29 (depends on 27)

The III-Nitride semiconductor device according to claim 27, further comprising:
said III-Nitride compound layer being a GaN layer.

### Claim 30 (depends on 28)

The III-Nitride semiconductor device according to claim 28, further comprising:
said III-Nitride compound layer being a GaN layer.

### Claim 31 (depends on 27)

The III-Nitride semiconductor device according to claim 27, further comprising:
said AlN layer having a thickness of 1.7±0.1 nm.

### Claim 32 (depends on 27)

The III-Nitride semiconductor device according to claim 27, further comprising:
said AlN layer having a thickness of less than 3.5 nm.

### Claim 33 (depends on 27)

A III-Nitride semiconductor device according to claim 27, further comprising:
having at least two layers of compounds selected from the group of III-Nitride compounds over said AlN layer.

### Claim 34

A III-Nitride semiconductor device comprising:
a substrate, said substrate being a polycrystalline diamond;
an Al-face polarity (0001) AlN nucleation layer on said substrate having a thickness of less than 5 nm; and
at least one III-Nitride compound layer over said AlN layer, said cooperation resulting in (0001) orientation and III metal-face polarity.

### Claim 35 (depends on 34)

The III-Nitride semiconductor device according to claim 34, further comprising:
said III-Nitride compound layer being a GaN layer.

### Claim 36 (depends on 34)

The III-Nitride semiconductor device according to claim 34, further comprising:
said AlN layer having a thickness of less than 3.5 nm.