# US 2015/0144681 A1 · Method for Making Corrosion Resistant Fluid Conducting Parts

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0144681 A1
- Document ID: US20150144681A1
- Status: Published application
- Kind: A1
- Application number: 14/608,558
- Filed: 2015-01-29
- Published: 2015-05-28
- Earliest claimed: 2004-08-02
- Assignees: ATI Properties, Inc.
- Applicants: ATI Properties, Inc.
- Inventors: Richard C. Sutherlin; Brett J. Herb; Ronald A. Graham
- Web page: https://patentgrep.com/patent/US20150144681A1

## CPC

- B23K 15/04: for welding annular seams
- B01J 19/02: Apparatus characterised by being constructed of material selected for its chemically-resistant properties
- B01J 19/2415: {Tubular reactors}
- B21C 23/085: {Making tubes (B21C23/10 take precedence)}
- B21C 23/22: Making metal-coated products; Making products from two or more metals
- B23K 13/01: by induction heating
- B23K 15/0006: {specially adapted for particular articles or work}
- B23K 20/10: making use of vibrations, e.g. ultrasonic welding
- B23K 20/129: {specially adapted for particular articles or work}
- B23K 20/233: without ferrous layer
- B23K 31/027: {Making tubes by soldering or welding}
- B24C 1/003: {using material which dissolves or changes phase after the treatment, e.g. ice, CO2}
- C22F 1/183: {of titanium or alloys based thereon}
- C22F 1/186: {of zirconium or alloys based thereon}
- F16L 9/18: Double-walled pipes; Multi-channel pipes or pipe assemblies
- F28F 9/18: by welding
- F28F 11/00: Arrangements for sealing leaky tubes and conduits (stopping flow from or in pipes in general F16L55/10)
- F28F 19/06: of metal
- H05B 6/10: Induction heating apparatus, other than furnaces, for specific applications
- B01J 2219/0236: Metal based
- B01J 2219/0277: Metal based
- B23K 2103/05: {Stainless steel}
- B23K 2103/08: Non-ferrous metals or alloys
- B23K 2103/14: Titanium or alloys thereof
- B23K 2103/18: Dissimilar materials
- F28F 2275/062: by impact pressure or friction welding
- Y02P 20/141: Feedstock
- Y10T 29/4935: Heat exchanger or boiler making
- Y10T 428/12292: Workpiece with longitudinal passageway or stopweld material [e.g., for tubular stock, etc.]
- Y10T 428/31808: Cellulosic is paper
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- B21C: MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES, PROFILES OR LIKE SEMI-MANUFACTURED PRODUCTS OTHERWISE THAN BY ROLLING; AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKING WITHOUT ESSENTIALLY REMOVING MATERIAL
- B24C: ABRASIVE OR RELATED BLASTING WITH PARTICULATE MATERIAL
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- F16L: PIPES; JOINTS OR FITTINGS FOR PIPES; SUPPORTS FOR PIPES, CABLES OR PROTECTIVE TUBING; MEANS FOR THERMAL INSULATION IN GENERAL
- F28F: DETAILS OF HEAT-EXCHANGE AND HEAT-TRANSFER APPARATUS, OF GENERAL APPLICATION (water and air traps, air venting F16)
- H05B: ELECTRIC HEATING; ELECTRIC LIGHT SOURCES NOT OTHERWISE PROVIDED FOR; CIRCUIT ARRANGEMENTS FOR ELECTRIC LIGHT SOURCES, IN GENERAL
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for making a tube is described in which a multi-layer billet is extruded to provide a tube having a wall comprising an inner layer metallurgically bonded to an outer layer.

## Claims

### Claim 1

A method for making a tube, the method comprising:
providing a hollow first cylinder comprising zirconium or a zirconium alloy, the first cylinder having an outer surface;
providing a hollow second cylinder comprising titanium or a titanium alloy, the second cylinder having an inner surface, wherein the first cylinder can fit within the second cylinder;
positioning the first cylinder within the second cylinder, wherein the outer surface of the first cylinder opposes the inner surface of the second cylinder;
welding together end joints between the first cylinder and the second cylinder to provide a multi-layer billet;
induction heating the multi-layer billet to an extrusion temperature;
extruding the heated multi-layer billet, thereby metallurgically bonding the outer surface of the first cylinder to the inner surface of the second cylinder, and providing a tube having a wall comprising an inner layer comprising zirconium or a zirconium alloy metallurgically bonded to an outer layer comprising titanium or a titanium alloy; and
cold working the tube to reduce the wall thickness and/or diameter of the tube.

### Claim 2 (depends on 1)

The method of claim 1, wherein the tube lacks an interdiffusion layer between the inner layer and the outer layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the tube lacks intermetallic compounds and alloying in the metallurgical bond between the inner layer and the outer layer.

### Claim 4 (depends on 1)

The method of claim 1, wherein cold working the tube comprises cold pilgering the tube.

### Claim 5 (depends on 1)

The method of claim 1, wherein cold working the tube comprises cold pilgering the tube to a reduction in area of 20% to 90%.

### Claim 6 (depends on 1)

The method of claim 1, wherein cold working the tube comprises cold drawing the tube.

### Claim 7 (depends on 1)

The method of claim 1, further comprising heat treating the tube after extruding the multi-layer billet and/or after cold working the tube.

### Claim 8 (depends on 7)

The method of claim 7, wherein heat treating the tube comprises annealing the tube at a temperature in the range of 500° C. to 750° C. for 1 to 12 hours.

### Claim 9 (depends on 1)

The method of claim 1, wherein cold working the tube comprises at least two cold pilgering passes, wherein the tube is annealed at a temperature in the range of 500° C. to 750° C. for 1 to 12 hours after each pilgering pass and before any subsequent pilgering pass.

### Claim 10 (depends on 1)

The method of claim 1, comprising extruding the billet in an extrusion apparatus comprising an extrusion ram that is advanced at a rate in the range of 50 mm/minute to 900 mm/minute during an extrusion cycle.

### Claim 11 (depends on 1)

The method of claim 1, comprising extruding the billet at an extrusion ratio in the range of 3:1 to 30:1.

### Claim 12 (depends on 1)

The method of claim 1, wherein the multi-layer billet is induction heated to a temperature in the range of 550° C. to 900° C.

### Claim 13 (depends on 1)

The method of claim 1, wherein the end joints are welded together with an electron beam weld.

### Claim 14 (depends on 13)

The method of claim 13, wherein the electron beam weld penetrates the end joints to a depth ranging from 5 mm to 50 mm.

### Claim 15 (depends on 1)

The method of claim 1, further comprising reducing surface roughness of at least one of the outer surface of the first cylinder and the inner surface of the second cylinder to no greater than 63 micro-inches RA before positioning the first cylinder within the second cylinder.

### Claim 16 (depends on 1)

The method of claim 1, further comprising ice blasting at least one of the outer surface of the first cylinder and the inner surface the second cylinder by propelling crystalline water against the surface(s), thereby mechanically scrubbing and liquid flushing the surface(s).

### Claim 17 (depends on 1)

The method of claim 1, further comprising inertia welding a zirconium or zirconium alloy tube segment to the tube having a wall comprising an inner layer comprising zirconium or a zirconium alloy metallurgically bonded to an outer layer comprising titanium or a titanium alloy.

### Claim 18

A method for making a tube, the method comprising:
providing a hollow first cylinder comprising zirconium, a zirconium alloy, hafnium, a hafnium alloy, vanadium, a vanadium alloy, niobium, a niobium alloy, tantalum, or a tantalum alloy, the first cylinder having an outer surface;
providing a hollow second cylinder comprising stainless steel, titanium, or a titanium alloy, the second cylinder having an inner surface, wherein the first cylinder can fit within the second cylinder;
positioning the first cylinder within the second cylinder, wherein the outer surface of the first cylinder opposes the inner surface of the second cylinder;
welding together end joints between the first cylinder and the second cylinder to provide a multi-layer billet;
heating the multi-layer billet to an extrusion temperature;
extruding the heated multi-layer billet, thereby metallurgically bonding the outer surface of the first cylinder to the inner surface of the second cylinder, and providing a tube having a wall comprising an inner layer metallurgically bonded to an outer layer; and
cold working the tube to reduce the wall thickness and/or diameter of the tube.

### Claim 19 (depends on 18)

The method of claim 18, wherein cold working the tube comprises cold pilgering the tube to a reduction in area of 20% to 90%.

### Claim 20 (depends on 18)

The method of claim 18, further comprising annealing the tube at a temperature in the range of 500° C. to 750° C. for 1 to 12 hours, wherein the annealing is performed after extruding the multi-layer billet and/or after cold working the tube.

### Claim 21 (depends on 18)

The method of claim 18, comprising extruding the billet at an extrusion ratio in the range of 3:1 to 30:1 in an extrusion apparatus comprising an extrusion ram that is advanced at a rate in the range of 50 mm/minute to 900 mm/minute during an extrusion cycle.

### Claim 22 (depends on 18)

The method of claim 18, wherein the multi-layer billet is induction heated to a temperature in the range of 550° C. to 900° C.

### Claim 23 (depends on 18)

The method of claim 18, wherein the end joints are welded together with an electron beam weld that penetrates the end joints to a depth ranging from 5 mm to 50 mm.

### Claim 24 (depends on 18)

The method of claim 18, further comprising reducing surface roughness of at least one of the outer surface of the first cylinder and the inner surface of the second cylinder to no greater than 63 micro-inches RA before positioning the first cylinder within the second cylinder.

### Claim 25 (depends on 18)

The method of claim 18, further comprising ice blasting at least one of the outer surface of the first cylinder and the inner surface the second cylinder by propelling crystalline water against the surface(s), thereby mechanically scrubbing and liquid flushing the surface(s).

### Claim 26 (depends on 1)

A method for replacing a tube in chemical processing equipment, the method comprising:
providing a tube made in accordance with the method of claim 1; and
fusion welding the tube to a tubesheet in the chemical processing equipment.

### Claim 27 (depends on 26)

The method of claim 26, wherein the chemical processing equipment comprises a urea stripper, a heat exchanger, or a condenser.