# US 2015/0144523 A1 · Blow-molded container with pinch-off part

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0144523 A1
- Document ID: US20150144523A1
- Status: Published application
- Kind: A1
- Application number: 14/400,713
- Filed: 2013-05-08
- Published: 2015-05-28
- Earliest claimed: 2012-05-14
- Assignees: Kuraray Co., Ltd.
- Applicants: Kuraray Co., Ltd.
- Inventors: Wataru Hirose
- Web page: https://patentgrep.com/patent/US20150144523A1

## CPC

- B65D 1/0207: {characterised by material, e.g. composition, physical features}
- B65D: CONTAINERS FOR STORAGE OR TRANSPORT OF ARTICLES OR MATERIALS, e.g. BAGS, BARRELS, BOTTLES, BOXES, CANS, CARTONS, CRATES, DRUMS, JARS, TANKS, HOPPERS, FORWARDING CONTAINERS; ACCESSORIES, CLOSURES, OR FITTINGS THEREFOR; PACKAGING ELEMENTS; PACKAGES

## Abstract

There is provided a blow-molded container having a pinch-off part and having, as an innermost layer, a layer of resin composition comprising an ethylene-vinyl alcohol copolymer (A) and a soft resin (B), characterized in that the soft resin (B) is a thermoplastic styrenic elastomer or α-olefinic polymer; a mass ratio of the ethylene-vinyl alcohol copolymer (A) to the soft resin (B) [(A)/(B)] is within the range of 75/25 to 90/10; the resin composition has a matrix and domain structure in which the ethylene-vinyl alcohol copolymer (A) is a matrix phase and the soft resin (B) is a domain phase; and a surface-to-surface interparticle distance in the domain phase is 0.3 μm or less.

## Claims

### Claim 1

A blow-molded container having a pinch-off part and having, as an innermost layer, a layer of resin composition comprising an ethylene-vinyl alcohol copolymer (A) and a soft resin (B), characterized in that
the soft resin (B) is a thermoplastic styrenic elastomer or α-olefinic polymer;
a mass ratio of the ethylene-vinyl alcohol copolymer (A) to the soft resin (B) [(A)/(B)] is within the range of 75/25 to 90/10;
the resin composition has a matrix and domain structure in which the ethylene-vinyl alcohol copolymer (A) is a matrix phase and the soft resin (B) is a domain phase; and
a surface-to-surface interparticle distance in the domain phase is 0.3 μm or less.

### Claim 2 (depends on 1)

The blow-molded container as claimed in claim 1, wherein a melt flow rate (MFR) of the resin composition measured under a load of 2160 g at 210° C. is ⅔ or less of a melt flow rate (MFR) of the ethylene-vinyl alcohol copolymer (A).

### Claim 3 (depends on 1)

The blow-molded container as claimed in claim 1, wherein the soft resin (B) is a mixture of an acid-modified soft resin (b1) and an unmodified soft resin (b2).

### Claim 4 (depends on 1)

The blow-molded container as claimed in claim 1, wherein a hardness of the soft resin (B) as measured by a durometer type A in accordance with ISO 7619 is 90 or less.

### Claim 5 (depends on 1)

The blow-molded container as claimed in claim 1, which is a chemical bottle.

### Claim 6 (depends on 5)

The blow-molded container as claimed in claim 5, wherein the chemical is an agrochemical.