# US 2015/0144503 A1 · Methods and systems for treating petroleum feedstock containing organic acids and sulfur

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0144503 A1
- Document ID: US20150144503A1
- Status: Published application
- Kind: A1
- Application number: 14/551,410
- Filed: 2014-11-24
- Published: 2015-05-28
- Earliest claimed: 2013-11-26
- Assignees: Ceramatec, Inc.
- Applicants: Ceramatec, Inc.
- Inventors: John Howard Gordon
- Web page: https://patentgrep.com/patent/US20150144503A1

## CPC

- C10G 53/12: including at least one alkaline treatment step
- C10G 3/40: {Thermal non-catalytic treatment}
- C10G 29/04: Metals, or metals deposited on a carrier
- C10G 53/02: plural serial stages only
- C10G 53/14: including at least one oxidation step
- C10G 67/02: plural serial stages only
- C25B 1/00: Electrolytic production of inorganic compounds or non-metals
- C25C 1/02: of light metals
- C25C 3/02: of alkali or alkaline earth metals
- C25C 7/04: Diaphragms; Spacing elements
- C10G 2300/202: Heteroatoms content, i.e. S, N, O, P
- C10G 2300/203: Naphthenic acids, TAN
- Y02P 30/20: using bio-feedstock
- C10G: CRACKING HYDROCARBON OILS; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVE HYDROGENATION, OLIGOMERISATION, POLYMERISATION (cracking to hydrogen or synthesis gas C01B; cracking or pyrolysis of hydrocarbon gases to individual hydrocarbons or mixtures thereof of definite or specified constitution C07C; cracking to cokes C10B); RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, OR GASES; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS; REFORMING OF NAPHTHA; MINERAL WAXES
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)
- C25C: PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY OR REFINING OF METALS; APPARATUS THEREFOR
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Methods and systems of treating petroleum feedstock contaminated with naphthenic acids and sulfur are disclosed. The methods and systems include heating the petroleum feedstock to decompose the naphthenic acids, pressurizing to minimize the portion in the vapor phase, sweeping water vapor and carbon dioxide into a headspace with a non-oxidizing gas, removing water vapor and carbon dioxide from the headspace, reacting the sulfur with an alkali metal and a radical capping gas to convert the sulfur into alkali sulfides, and removing the alkali sulfides. Also disclosed is reacting the naphthenic acid with water and an oxide or hydroxide of an alkaline earth element to convert the naphthenic acid into naphthenates, removing water, ketonizing, removing oxides or carbonates, reacting the sulfur with an alkali metal and a radical capping gas to convert the sulfur into alkali sulfides, and removing the alkali sulfides.

## Claims

### Claim 1

A method for treating petroleum feedstock comprising:
providing a petroleum feedstock comprising naphthenic acids and sulfur;
heating the petroleum feedstock to decompose the naphthenic acids;
pressurizing the petroleum feedstock to minimize a portion of the petroleum feedstock in a vapor phase;
sweeping water vapor and carbon dioxide from the petroleum feedstock into a headspace with a non-oxidizing gas;
removing water vapor and carbon dioxide from the headspace to promote naphthenic acid decomposition;
reacting the sulfur with an alkali metal and a radical capping gas to convert the sulfur into alkali sulfides; and
removing the alkali sulfide.

### Claim 2 (depends on 1)

The method of claim 1, wherein the petroleum feedstock is heated in a range of about 200° C. to about 425° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein the petroleum feedstock is heated in a range of about 300° C. to about 400° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein the non-oxidizing gas comprises hydrogen, light hydrocarbon gas, pyrolysis gas, or combinations thereof.

### Claim 5 (depends on 1)

The method of claim 1, wherein the alkali metal comprises lithium, sodium, potassium, or combinations thereof.

### Claim 6 (depends on 1)

The method of claim 1, wherein the radical capping gas comprises one or more of the following: methane, ethane, propane, butane, pentane, hexane, heptane, octane, ethene, propene, butane, pentene, hexene, heptene, octene, and isomers of the foregoing, natural gas, shale gas, liquid petroleum gas, ammonia, primary, secondary, and tertiary ammines, thiols, mercaptans, and hydrogen sulfide.

### Claim 7 (depends on 1)

The method of claim 1, further comprising regenerating the alkali metal from the alkali metal sulfide.

### Claim 8 (depends on 7)

The method of claim 7, wherein regenerating the alkali metal from the solids comprises an electrolytic process using an alkali metal ion conductive ceramic membrane.

### Claim 9

A method for treating petroleum feedstock comprising:
providing a petroleum feedstock comprising naphthenic acids and sulfur;
reacting the naphthenic acid an aqueous solution or slurry containing an oxide or hydroxide of an alkaline earth element while heating to convert the naphthenic acid into alkaline earth naphthenates, thereby generating an alkaline earth naphthenate mixture;
removing water from the alkaline earth naphthenate mixture to generate a dewatered mixture;
reacting the sulfur in the dewatered mixture with an alkali metal and a radical capping gas to convert the sulfur into alkali sulfides; and
removing the alkali sulfides.

### Claim 10 (depends on 9)

The method of claim 9, wherein the alkaline earth mixture is heated in a range of about 80° C. to about 95° C.

### Claim 11 (depends on 9)

The method of claim 9, wherein the dewatered mixture is heated in a range of about 300° C. to about 400° C.

### Claim 12 (depends on 9)

The method of claim 9, wherein the alkali metal comprises sodium and the alkaline earth element comprises one or more of calcium, strontium, or barium.

### Claim 13 (depends on 9)

The method of claim 9, further comprising regenerating the alkali metal from the alkali metal sulfide.

### Claim 14 (depends on 7)

The method of claim 7, wherein regenerating the alkali metal from the solids comprises an electrolytic process using an alkali metal ion conductive ceramic membrane.

### Claim 15

A method for treating petroleum feedstock comprising:
providing a petroleum feedstock comprising naphthenic acids and sulfur;
reacting the naphthenic acid with an aqueous solution or slurry containing an oxide or hydroxide of an alkaline earth element while heating to convert the naphthenic acid into an alkaline earth naphthenate, thereby generating an alkaline earth naphthenate mixture;
removing water from the alkaline earth naphthenate mixture to generate a dewatered mixture;
heating the dewatered mixture to convert alkaline earth naphthenates into ketones and alkaline earth oxides or alkaline earth carbonates, thereby generating a ketone mixture;
removing alkaline earth oxides or alkaline earth carbonates from the ketone mixture;
reacting the sulfur in the ketone mixture with an alkali metal and a radical capping gas to convert the sulfur into alkali sulfides; and
removing the alkali sulfide.

### Claim 16 (depends on 15)

The method of claim 15, wherein the dewatered mixture is heated in a range of about 166° C. to about 312° C.

### Claim 17 (depends on 15)

The method of claim 15, wherein heating the dewatered mixture to convert alkaline earth naphthenates into ketones and alkaline earth oxides or alkaline earth carbonates and reacting the sulfur with an alkali metal and a radical capping gas to convert the sulfur into an alkali sulfide is carried out at the same time in a single reaction vessel.

### Claim 18 (depends on 17)

The method of claim 17, wherein the alkali metal comprises sodium and the alkaline earth element comprises one or more of calcium, strontium, or barium.

### Claim 19 (depends on 15)

The method of claim 15, further comprising regenerating the alkaline earth carbonates with heat to form alkaline earth oxides.

### Claim 20 (depends on 15)

The method of claim 15, wherein removing the alkaline earth oxides or alkaline earth carbonates and the alkali sulfide comprises filtration, centrifugation, hydrocyclonic separation, or combinations thereof.