# US 2015/0144229 A1 · High-Strength Aluminum Alloy Brazing Sheet And Method Of Manufacture

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0144229 A1
- Document ID: US20150144229A1
- Status: Published application
- Kind: A1
- Application number: 14/528,930
- Filed: 2014-10-30
- Published: 2015-05-28
- Earliest claimed: 2010-09-21
- Assignees: Uacj Corporation
- Inventors: Makoto Ando; Akio Niikura; Yoichiro Bekki
- Web page: https://patentgrep.com/patent/US20150144229A1

## CPC

- B23K 35/002: {at least one of the workpieces being of light metal}
- B23K 1/0012: {Brazing of heat exchangers}
- B23K 1/203: {Fluxing, i.e. applying flux onto surfaces}
- B23K 35/0238: {layered}
- B23K 35/286: {Al as the principal constituent}
- B32B 15/016: {all layers being formed of aluminium or aluminium alloys}
- C09K 5/14: Solid materials, e.g. powdery or granular
- C22C 21/00: Alloys based on aluminium
- C22C 21/02: with silicon as the next major constituent
- C22C 21/10: with zinc as the next major constituent
- C22C 21/12: with copper as the next major constituent
- C22C 21/14: with silicon
- C22F 1/00: Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working (apparatus for mechanical working of metal B21, B23, B24)
- C22F 1/04: of aluminium or alloys based thereon
- C22F 1/043: of alloys with silicon as the next major constituent
- B23K 2101/006: {Vehicles}
- B23K 2101/14: Heat exchangers
- F28F 21/084: {from aluminium or aluminium alloys}
- F28F 21/089: {Coatings, claddings or bonding layers made from metals or metal alloys (F28F19/06 takes precedence)}
- Y10T 428/12764: Next to Al-base component
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- F28F: DETAILS OF HEAT-EXCHANGE AND HEAT-TRANSFER APPARATUS, OF GENERAL APPLICATION (water and air traps, air venting F16)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

An aluminum alloy brazing sheet having a core material of an aluminum alloy, and a filler material cladded on the core is disclosed. The core material is an aluminum alloy having about 0.05 to about 1.2 mass Si, about 0.05-about 1.0 mass % Fe, about 0.05-about 1.2 mass % Cu, and about 0.6-about 1.8 mass % Mn, balance Al and the inevitable impurities. The, filler material includes an aluminum alloy having about 2.5-about 13.0 mass % Si. Also, there is provided a method of manufacturing such an aluminum alloy brazing sheet.

## Claims

### Claim 1

A method of manufacturing a high strength aluminum alloy brazing sheet comprising:
casting an aluminum alloy of a core material and a filler material at a casting speed to provide a cast core material and a cast filler material, respectively;
combining the cast core material with the cast filler material so that the cast filler material is cladded to at least one surface of the cast core material to produce a composite material;
a heating process wherein the composite material is heated and held after the combining process to form a heat treated composite material; and
hot clad rolling the heat treated composite material,
wherein the casting speed V (mm/min) and an amount of cooling water W (kg/min×cm) applied during the casting satisfy formula (1) in the casting process for said core material:
25≦0.4×V+W (1);
wherein the composite material is held at a temperature within a range of about 400° C. to about 500° C. over a time period of 0 hrs to about 10 hrs during the heating process;
wherein the time period for the hot clad rolling which is counted from start of the hot clad rolling to the time taken to reduce an initial thickness of the composite material by 50 mm is at most 5 min,
wherein the temperature of the composite material falls within a range of about 400° C. to about 450° C. when the thickness of said composite material is reduced by 50 mm;
wherein a time period counted from the time when the thickness of the composite material is reduced by 50 mm to the time taken to reduce the thickness of the composite material to 20 mm is at most 10 min,
wherein the temperature of the composite material is about 300° C. to about 400° C. when the thickness of the composite material is reduced to 20 mm;
wherein a time period which is counted from the rolling start to a rolling end is at most 40 min, and
wherein the aluminum alloy comprises a core material comprising an aluminum alloy; and a filler material cladded on at least one surface of the core material and comprising an Al/Si-based alloy, wherein the core material is an aluminum alloy which contains Si within a range of about 0.05 mass % to about 1.2 mass %, Fe within a range of about 0.05 mass % to about 1.0 mass %, Cu within a range of about 0.05 mass % to about 1.2 mass %, and Mn within a range of about 0.6 mass % to about 1.8 mass %, and which comprises as balance Al and inevitable impurities; wherein the filler material is an aluminum alloy which contains Si falling within a range of about 2.5 mass % to about 13.0 mass %, and Fe falling within a range of about 0.05 mass % to about 1.0 mass %, and comprises as balance Al and inevitable impurities; wherein an area percentage is occupied with intermetallic compounds having a size falling within a range of about 0.2 μm to about 0.5 μm is at most 5%; and wherein a solid solution amount of Mn is at least 0.2 mass % in the core.

### Claim 2 (depends on 1)

The method of claim 1 wherein the core material further comprises at least one element selected from the group consisting of Mg within a range of about 0.05 mass % to about 0.5 mass %, Ti within a range of about 0.05 mass % to about 0.3 mass %, Zr within a range of about 0.05 mass % to about 0.3 mass %, Cr within a range of about 0.05 mass % to about 0.3 mass %, and V within a range of about 0.05 mass % to about 0.3 mass %.

### Claim 3 (depends on 1)

The method of claim 1 wherein the filler material cladded to the aforesaid one surface of said core material further contains Zn within a range of about 0.3 mass % to about 5.5 mass %.

### Claim 4

A method of manufacturing a high strength aluminum alloy brazing sheet comprising:
casting an aluminum alloy of a core material, a filler material and a sacrificial anode material, respectively, at a casting speed to provide a cast core material, a cast filler material and a cast sacrificial anode material, respectively;
combining the cast core material with the cast filler material and the cast sacrificial anode material whereby the cast filler material is cladded to at least one surface of the cast core material and whereby the cast sacrificial anode material is applied to another surface of the cast core material to produce a composite material;
a heating process wherein the composite material is heated and held after the combining process to form a heat treated composite material; and
hot clad rolling the heat treated composite material,
wherein the casting speed V (mm/min) and an amount of cooling water W (kg/min×cm) applied during the casting formula (1) while the core material:
25≦0.4×V+W (1);
wherein the composite material is held at a temperature within a range of about 400° C. to about 500° C. over a time period of 0 to about 10 hrs during the heating; and
wherein the time period for the hot clad rolling which is counted from start of the hot clad rolling to the time taken to reduce an initial thickness of the composite material by 50 mm is at most 5 min; and
wherein the temperature of said composite material is about 400° C. to about 450° C. when the thickness of said composite material is reduced by 50 mm; and
wherein the time period counted from the time when the thickness of the composite material is reduced by 50 mm to the time taken to reduce the thickness of the composite material to 20 mm is at most 10 min; and
and wherein a temperature of the composite material is about 300° C. to about 400° C. when the thickness of the composite material is reduced to 20 mm; and
wherein a time period counted from the rolling start to a rolling end is up to 40 min, and
wherein the aluminum brazing sheet comprises a core material comprised of an aluminum alloy; a filler material cladded on one surface of said core material and comprised of an Al/Si-based alloy; and a sacrificial anode material cladded on another surface of the core material and comprised of an aluminum alloy,
wherein the core material is an aluminum alloy having Si within a range of about 0.05 mass % to about 1.2 mass %, Fe within a range of about 0.05 mass % to about 1.0 mass %, Cu within a range of about 0.05 mass % to about 1.2 mass %, and Mn within a range of about 0.6 mass % to about 1.8 mass %, and balance Al and inevitable impurities;
wherein the filler material is an aluminum alloy having Si within a range of about 2.5 mass % to about 13.0 mass %, and Fe within a range of about 0.05 mass % to about 1.0 mass %, balance Al and inevitable impurities;
wherein the sacrificial anode material is an aluminum alloy having Zn within a range of about 0.5 mass % to about 6.0 mass %, Si within a range of about 0.05 mass % to about 1.5 mass %, and Fe within a range of about 0.05 mass % to about 2.0 mass %, and balance Al and inevitable impurities; wherein an area percentage is occupied with intermetallic compounds having a size within a range of 0.2 μm to 0.5 μm is at most 5%; and wherein a solid solution amount of Mn is at least 0.2 mass % in the core material.

### Claim 5 (depends on 4)

The method of claim 4 wherein the core material further comprises at least one of Mg within a range of about 0.05 mass % to about 0.5 mass %, Ti within a range of about 0.05 mass % to about 0.3 mass %, Zr within a range of about 0.05 mass % to about 0.3 mass %, Cr within a range of about 0.05 mass % to about 0.3 mass %, and V within a range of about 0.05 mass % to about 0.3 mass %.

### Claim 6 (depends on 4)

The method of claim 4 wherein the filler material cladded to the aforesaid one surface of said core material further comprises Zn within a range of about 0.3 mass % to about 5.5 mass %.

### Claim 7 (depends on 4)

The method of claim 4 wherein the sacrificial anode material further comprises at least one of Mn within a range of about 0.05 mass % to about 1.8 mass %, Mg within a range of about 0.5 mass % to about 3.0 mass %, Ti within a range of about 0.05 mass % to about 0.3 mass %, Zr mass % within a range of about 0.05 mass % to about 0.3 mass %, Cr within a range of about 0.05 mass % to about 0.3 mass %, and V within a range of about 0.05 mass % to about 0.3 mass %.

### Claim 8 (depends on 1)

The method of claim 1 wherein the core material has not been subjected to homogenization.

### Claim 9 (depends on 1)

The method of claim 1 wherein the composite material has a thickness of about 250 mm to about 800 mm prior to hot clad rolling.

### Claim 10 (depends on 4)

The method of claim 4 wherein the composite material has a thickness of about 250 mm to about 800 mm prior to hot clad rolling.