# US 2015/0144228 A1 · Quenched steel pipe member, vehicle axle beam using quenched steel pipe member, and method for manufacturing quenched steel pipe member

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0144228 A1
- Document ID: US20150144228A1
- Status: Published application
- Kind: A1
- Application number: 14/409,061
- Filed: 2013-09-12
- Published: 2015-05-28
- Earliest claimed: 2012-09-20
- Assignees: Nippon Steel & Sumitomo Metal Corporation
- Applicants: Nippon Steel & Sumitomo Metal Corporation
- Inventors: Takaaki Fukushi; Koichi Sato; Satoshi Kato; Hideki Hamatani; Yoshiaki Hirota
- Web page: https://patentgrep.com/patent/US20150144228A1

## CPC

- C21D 9/08: for tubular bodies or pipes
- B32B 15/013: {one layer being formed of an iron alloy or steel, another layer being formed of a metal other than iron or aluminium}
- B60B 35/02: Dead axles, i.e. not transmitting torque
- C21D 1/34: Methods of heating (C21D1/06 takes precedence)
- C21D 1/60: Aqueous agents
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/14: containing titanium or zirconium
- C23C 2/06: Zinc or cadmium or alloys based thereon
- C23C 2/28: Thermal after-treatment, e.g. treatment in oil bath
- C23C 2/29: {Cooling or quenching}
- C23C 2/38: Wires; Tubes
- B60B 2360/102: Steel
- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- C21D 9/0068: {for particular articles not mentioned below}
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- B60B: VEHICLE WHEELS (making wheels or wheel parts by rolling B21H1/00, by forging, hammering or pressing B21K1/28); CASTORS; AXLES FOR WHEELS OR CASTORS; INCREASING WHEEL ADHESION
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A quenched steel pipe member is formed of a GI galvanized steel pipe, in a middle section in a longitudinal direction of the GI galvanized steel pipe, a cross-section perpendicular to the longitudinal direction has a substantially V shape including a contact section at which opposite parts of an inner circumferential surface of the GI galvanized steel pipe come into contact with each other, the contact section is bonded using a Fe—Zn alloy phase, and a micro Vickers hardness at a location 50 μm deep from a base material surface layer is 95% or more of a micro Vickers hardness at a location 200 μm deep from the base material surface layer.

## Claims

### Claim 1

A quenched steel pipe member,
wherein the quenched steel pipe member is formed of a GI galvanized steel pipe,
in a middle section in a longitudinal direction of the GI galvanized steel pipe, a cross-section perpendicular to the longitudinal direction has a substantially V shape including a contact section at which opposite parts of an inner circumferential surface of the GI galvanized steel pipe come into contact with each other,
the contact section is bonded using a Fe—Zn alloy phase, and
a micro Vickers hardness at a location 50 μm deep from a base material surface layer is 95% or more of a micro Vickers hardness at a location 200 μm deep from the base material surface layer.

### Claim 2 (depends on 1)

The quenched steel pipe member according to claim 1,
wherein the micro Vickers hardness at the location 50 μm deep from the base material surface layer of the GI galvanized steel pipe is 500 Hv or more.

### Claim 3 (depends on 1, 2)

The quenched steel pipe member according to claim 1 or 2,
wherein the contact section is formed throughout a length that is 50% or more of a total length of the GI galvanized steel pipe.

### Claim 4 (depends on 1, 2, 3)

A vehicle axle beam,
wherein the quenched steel pipe member according to any one of claims 1 to 3 is used.

### Claim 5

A method for manufacturing a quenched steel pipe member, the method comprising:
press-forming a GI galvanized steel pipe so that, in a middle section in a longitudinal direction of the GI galvanized steel pipe, a cross-section perpendicular to the longitudinal direction has a substantially V shape including a contact section at which opposite parts of an inner circumferential surface of the GI galvanized steel pipe come into contact with each other;
heating and holding the press-formed GI galvanized steel pipe under conditions in which a plated zinc amount A (g/m2), a maximum heating temperature T (° C.) that is 850° C. or higher, and a holding time t (hr) at the maximum heating temperature satisfy the following formula (I); and
cooling the heated and held GI galvanized steel pipe through water cooling, thereby bonding the contact section using a Fe—Zn alloy phase,
(T+273.15)×(log t+20)/A≦340 Formula (I).

### Claim 6 (depends on 5)

The method for manufacturing a quenched steel pipe member according to claim 5,
wherein, in the cooling, the heated and held GI galvanized steel pipe is water-cooled to 200° C. or lower at a cooling rate of 30° C./s or more.

### Claim 7 (depends on 5, 6)

The method for manufacturing a quenched steel pipe member according to claim 5 or 6,
wherein the plated zinc amount A is 60 g/m2 or more.

### Claim 8 (depends on 5, 6, 7)

The method for manufacturing a quenched steel pipe member according to any one of claims 5 to 7,
wherein, in the press-forming, the GI galvanized steel pipe is press-formed so that the contact section is formed throughout a length that is 50% or more of a total length of the GI galvanized steel pipe.

### Claim 9 (depends on 5, 6, 7, 8)

The method for manufacturing a quenched steel pipe member according to any one of claims 5 to 8,
wherein, in the heating and holding, the GI galvanized steel pipe is electrically heated.

### Claim 10 (depends on 5, 6, 7, 8, 9)

The method for manufacturing a quenched steel pipe member according to any one of claims 5 to 9,
wherein, in the heating and holding, the press-formed GI galvanized steel pipe is electrically heated so as to be held in a temperature range of an Ac3 point of steel or higher for 3 seconds to 30 seconds.

### Claim 11 (depends on 5, 6, 7, 8, 9, 10)

The method for manufacturing a quenched steel pipe member according to any one of claims 5 to 10,
wherein the GI galvanized steel pipe has chemical composition having an Ac3 point of 850° C. or lower.