# US 2015/0144226 A1 · Method for manufacturing wooden billet, wooden baseball bat and billiard/snooker cues

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0144226 A1
- Document ID: US20150144226A1
- Status: Published application
- Kind: A1
- Application number: 14/406,562
- Filed: 2013-07-17
- Published: 2015-05-28
- Earliest claimed: 2012-07-24
- Inventors: Prakashkumar Narmadashankar Suthar
- Web page: https://patentgrep.com/patent/US20150144226A1

## CPC

- B27M 3/22: of sport articles, e.g. bowling pins, frames of tennis rackets, skis, paddles
- A63B 59/50: Substantially rod-shaped bats for hitting a ball in the air, e.g. for baseball
- A63B 59/52: made of wood or bamboo
- A63B 60/00: Details or accessories of golf clubs, bats, rackets or the like
- A63D 15/08: Cues
- B27K 1/00: Damping wood
- B27M 1/02: by compressing
- A63B 2102/18: Baseball, rounders or similar games
- A63B 2243/002: Billiards
- B27M: WORKING OF WOOD NOT PROVIDED FOR IN SUBCLASSES B27B - B27L; MANUFACTURE OF SPECIFIC WOODEN ARTICLES
- A63B: APPARATUS FOR PHYSICAL TRAINING, GYMNASTICS, SWIMMING, CLIMBING, OR FENCING; BALL GAMES; TRAINING EQUIPMENT (apparatus for passive exercising, massage A61H)
- A63D: BOWLING GAMES, e.g. SKITTLES, BOCCE OR BOWLS; INSTALLATIONS THEREFOR; BAGATELLE OR SIMILAR GAMES; BILLIARDS (balls A63B37/00)
- B27K: PROCESSES, APPARATUS OR SELECTION OF SUBSTANCES FOR IMPREGNATING, STAINING, DYEING, BLEACHING OF WOOD OR SIMILAR MATERIALS, OR TREATING OF WOOD OR SIMILAR MATERIALS WITH PERMEANT LIQUIDS, NOT OTHERWISE PROVIDED FOR (applying liquids or other fluent materials to surfaces in general B05; coating wood or similar material B44D); CHEMICAL OR PHYSICAL TREATMENT OF CORK, CANE, REED, STRAW OR SIMILAR MATERIALS

## Abstract

A process for manufacturing wooden billets, baseball bats and billiard/snooker cues is disclosed. The process comprises softening the hardwoods and willow, which are typically North American Hardwoods and English and Kashmir willow having moisture content between 30-70%, by steaming, and then compressing the softened hardwoods and willow by longitudinal compression processes along the length to cause the axial fibres to cross-link. The process aims at providing wooden billets, baseball bats and snooker cues having uniform performance standardization, improvement in durability, strength, acceptability, anti-breakage and flexibility.

## Claims

### Claim 1

A process for manufacturing wooden baseball bat billets, wooden baseball bats and billiard/snooker cues, said process comprising the following steps:
scanning a wood to determine characteristics of the wood by means of at least one parameter selected from moisture content, bending strength, elastic modulus, compression modulus, hardness and softness;
steaming said scanned wood by heating for obtaining a heated softened wood;
compressing said heated softened wood by means of longitudinal compression processes adapted as per the wood characteristics by compressing along the length of said softened wood to cause the axial fibers of said softened wood to cross-link and thereby strengthening the wood to produce a processed wood;
shaping the processed wood to obtain wooden baseball bat billet, baseball bat or snooker cue.

### Claim 2 (depends on 1)

The process as claimed in claim 1, which comprises cooling the processed wood prior to shaping.

### Claim 3 (depends on 1)

The process as claimed in claim 1, which comprises drying the processed wood prior to shaping by a process selected from traditional drying and vacuum drying, to adjust the final uniform weight of the wooden billet, baseball bat and billiard/snooker cues.

### Claim 4 (depends on 1)

The process as claimed in claim 1, wherein the wood is selected from English willow, Kashmir willow, North American Hardwoods, Hard Maple, American Northern White Ash and the like.

### Claim 5 (depends on 4)

The process as claimed in claim 4, wherein the hardwoods and willow are green wood.

### Claim 6 (depends on 4)

The process as claimed in claim 4, wherein the willow has moisture content between 30-70%.