# US 2015/0144155 A1 · Method for High Aspect Ratio Photoresist Removal in Pure Reducing Plasma

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0144155 A1
- Document ID: US20150144155A1
- Status: Published application
- Kind: A1
- Application number: 14/406,256
- Filed: 2013-07-16
- Published: 2015-05-28
- Earliest claimed: 2012-07-16
- Assignees: Mattson Technology, Inc.
- Applicants: Mattson Technology, Inc
- Inventors: Li Diao; Robert George Elliston; David Gilbert; Chan-Yun Lee; James Paris; HaiAu PhanVu; Tom Tillery; Vijay Matthew Vaniapura
- Web page: https://patentgrep.com/patent/US20150144155A1

## CPC

- H10P 50/242: {of Group IV materials}
- G03F 7/427: {using plasma means only}
- H01J 37/321: {the radio frequency energy being inductively coupled to the plasma}
- H01J 37/32449: {Gas control, e.g. control of the gas flow}
- H10P 50/287: {by chemical means}
- H10P 70/27: {during, before or after processing of conductive materials, e.g. polysilicon or amorphous silicon layers}
- H01J 2237/334: Etching
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

A method for removing photoresist, an oxidation layer, or both from a semiconductor substrate is disclosed. The method includes placing a substrate in a processing chamber, the processing chamber separate from a plasma chamber for generating a non-oxidizing plasma to be used in treating the substrate; generating a first non-oxidizing plasma from a first reactant gas and a first carrier gas in the plasma chamber, wherein the first non-oxidizing plasma comprises from about 10% to about 40% of the first reactant gas, wherein the first reactant gas has a flow rate of from about 100 standard cubic centimeters per minute to about 15,000 standard cubic centimeters per minute, and wherein the first carrier gas has a flow rate of from about 500 standard cubic centimeters per minute to about 20,000 standard cubic centimeters per minute; and treating the substrate by exposing the substrate to the first non-oxidizing plasma in the processing chamber.

## Claims

### Claim 1

A method for removing photoresist, an oxidation layer, or both from a semiconductor substrate, comprising:
placing a substrate in a processing chamber, the processing chamber located downstream from a plasma chamber for generating a non-oxidizing plasma to be used in treating the substrate;
generating a first non-oxidizing plasma from a first reactant gas and a first carrier gas in the plasma chamber, wherein the first non-oxidizing plasma comprises from about 10% to about 40% of the first reactant gas, wherein the first reactant gas has a flow rate of from about 0.05 standard cubic centimeters per minute per square centimeter of the substrate to about 12.5 standard cubic centimeters per minute per square centimeter of the substrate, and wherein the first carrier gas has a flow rate of from about 0.25 standard cubic centimeters per minute per square centimeter of the substrate to about 15 standard cubic centimeters per minute per square centimeter of the substrate; and
treating the substrate by exposing the substrate to the first non-oxidizing plasma in the processing chamber.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first reactant gas is free from oxygen.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first reactant gas comprises hydrogen.

### Claim 4 (depends on 3)

The method of claim 3, wherein the first reactant gas comprises H2, NH3, or CH4.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first carrier gas is an inert gas that is free from oxygen and hydrogen.

### Claim 6 (depends on 5)

The method of claim 5, wherein the first carrier gas comprises nitrogen or a noble gas.

### Claim 7 (depends on 6)

The method of claim 6, wherein the first carrier gas is N2.

### Claim 8 (depends on 1)

The method of claim 1, wherein the method is carried out at a source power ranging from about 0.4 kilowatts to about 13.5 kilowatts.

### Claim 9 (depends on 1)

The method of claim 1, wherein the method is carried out at a pressure ranging from about 100 milliTorr to about 4000 milliTorr.

### Claim 10 (depends on 1)

The method of claim 1, wherein the substrate is treated at a temperature ranging from about 150° C. to about 350° C.

### Claim 11 (depends on 1)

The method of claim 1, wherein the substrate is treated by exposing the substrate to the first non-oxidizing plasma for a time period ranging from about 10 seconds to about 180 seconds.

### Claim 12 (depends on 1)

The method of claim 1, wherein the substrate has a decrease in thickness ranging from about 0.05 nanometers to about 0.6 nanometers after exposure to the first non-oxidizing plasma.

### Claim 13 (depends on 1)

The method of claim 1, wherein the substrate contains high aspect ratio channels.

### Claim 14 (depends on 13)

The method of claim 13, wherein the channels have an aspect ratio of greater than about 50.

### Claim 15 (depends on 1)

The method of claim 1, further comprising:
generating a second non-oxidizing plasma from a second reactant gas and a second carrier gas in the plasma chamber, wherein the second non-oxidizing plasma comprises from about 10% to about 40% of the second reactant gas, wherein the second reactant gas has a flow rate of from about 0.05 standard cubic centimeters per minute per square centimeter of the substrate to about 12.5 standard cubic centimeters per minute per square centimeter of the substrate, and wherein the second carrier gas has a flow rate of from about 0.25 standard cubic centimeters per minute per square centimeter of the substrate to about 15 standard cubic centimeters per minute per square centimeter of the substrate; and
treating the substrate by exposing the substrate to the second non-oxidizing plasma in the processing chamber.

### Claim 16 (depends on 15)

The method of claim 15, wherein the second reactant gas is free from oxygen and nitrogen.

### Claim 17 (depends on 16)

The method of claim 16, wherein the second reactant gas comprises hydrogen.

### Claim 18 (depends on 15)

The method of claim 15, wherein the second carrier gas is an inert gas that is free from oxygen and nitrogen.

### Claim 19 (depends on 16)

The method of claim 16, wherein the second carrier gas comprises argon or helium.

### Claim 20 (depends on 19)

The method of claim 19, wherein the second carrier gas comprises argon.

### Claim 21 (depends on 1)

The method of claim 1, wherein the substrate has a diameter of from about 100 millimeters to about 500 millimeters.