# US 2015/0144055 A1 · Process for the production of crystalline titanium powder

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0144055 A1
- Document ID: US20150144055A1
- Status: Published application
- Kind: A1
- Application number: 14/406,166
- Filed: 2013-05-29
- Published: 2015-05-28
- Earliest claimed: 2012-06-06
- Assignees: Csir
- Applicants: Csir
- Inventors: David Steyn Van Vuuren; Salomon Johannes Oosthuizen; Jaco Johannes Swanepoel
- Web page: https://patentgrep.com/patent/US20150144055A1

## CPC

- B22F 1/06: Metallic powder characterised by the shape of the particles (nanosized particles B22F1/054)
- B22F 3/24: After-treatment of workpieces or articles {(B22F3/1146 takes precedence)}
- C30B 9/00: Single-crystal growth from melt solutions using molten solvents (by normal or gradient freezing C30B11/00; by zone-melting C30B13/00; by crystal pulling C30B15/00; on immersed seed crystal C30B17/00; by liquid phase epitaxial growth C30B19/00; under a protective fluid C30B27/00)
- C30B 29/02: Elements
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

The invention provides a process for the production of crystalline titanium powder containing single crystals or agglomerates of single crystals having an average crystal size (by volume) greater than 1 μm, said process including reacting a titanium chloride species, preferably titanium dichloride, and reducing metal in a continuous back-mix reactor to produce a free flowing suspension of titanium powder in molten chloride salt wherein: i. both the titanium chloride species and the reducing metal are dissolved in a molten chloride salt and fed to the reactor containing a chloride salt of the reducing metal; ii. the average feed ratio of the titanium chloride species and reducing metal to the continuous back-mix reactor is within 1%, preferably within 0.1%, of the stoichiometric ratio required to fully reduce the titanium chloride salt to titanium metal; iii. the concentration of titanium powder in the fluid suspension of titanium powder in molten salt in the continuous back-mix reactor is between 2 and 23 mass %; and iv. The reducing metal is lithium, sodium, magnesium, or calcium.

## Claims

### Claim 1

A process for the production of crystalline titanium powder containing single crystals or agglomerates of single crystals having an average crystal size (by volume) greater than 1 μm, said process including reacting a titanium chloride species, and reducing metal in a continuous back-mix reactor to produce a free flowing suspension of titanium powder in molten chloride salt wherein:
i. both the titanium chloride species and the reducing metal are dissolved in a molten chloride salt including suspended titanium powder and fed to the reactor containing a chloride salt of the reducing metal;
ii. the average feed ratio of the titanium chloride species and reducing metal to the continuous back-mix reactor is within 1% of the stoichiometric ratio required to fully reduce the titanium chloride salt to titanium metal;
iii. the concentration of titanium powder in the fluid suspension of titanium powder in molten salt in the continuous back-mix reactor is between 2 and 23 mass %; and
iv. the reducing metal is lithium, sodium, magnesium, or calcium.

### Claim 2 (depends on 1)

A process as claimed in claim 1, wherein some molten salt and titanium powder product is withdrawn together from the continuous back-mix reactor and they are separated from each other outside the reactor.

### Claim 3 (depends on 1)

A process as claimed in claim 1, wherein the feed of the dissolved titanium chloride species is produced in a separate vessel external to the continuous back-mix reactor.

### Claim 4 (depends on 3)

A process as claimed in claim 3, wherein the feed of the dissolved titanium chloride species is produced in a separate vessel external to the continuous back-mix reactor by reacting TiCl4 with metallic titanium dispersed in molten chloride salt recycled from the continuous back-mix reactor.

### Claim 5 (depends on 1)

A process as claimed in claim 1, wherein the reducing metal is pre-dissolved in molten chloride salt prior to feeding to the continuous back-mix reactor.

### Claim 6 (depends on 5)

A process as claimed in claim 5, wherein the reducing metal is pre-dissolved in molten chloride salt prior to feeding to the continuous back-mix reactor by recycling molten salt from the continuous back-mix reactor to a vessel where the reducing metal is dissolved in the chloride salt.

### Claim 7 (depends on 1)

A process as claimed in claim 1, wherein vessels to produce the dissolved titanium chloride salt and the dissolved reducing metal are electrically isolated from each other and also from the continuous back-mix reactor.

### Claim 8 (depends on 1)

A process as claimed in claim 1, wherein the molar concentration of dissolved titanium cations of the titanium chloride salt is less than 25% of the molar concentration of chloride anions in the molten salt feed solution.

### Claim 9 (depends on 8)

A process as claimed in claim 8, wherein the molar concentration of dissolved titanium cations of the titanium chloride salt is less than 5% of the molar concentration of chloride anions in the molten salt feed solution.

### Claim 10 (depends on 1)

A process as claimed in claim 1, wherein the molar concentration of dissolved reducing metal atoms in the molten chloride salt feed is less than 3.5% of the chloride anions of the molten salt solution.

### Claim 11 (depends on 10)

A process as claimed in claim 10, wherein, the molar concentration of dissolved reducing metal atoms in the molten chloride salt feed is less than 0.5% of the chloride anions of the molten salt solution.

### Claim 12 (depends on 1)

A process as claimed in claim 1, wherein the feed of dissolved reducing metal to the continuous back-mix reactor is in excess of the stoichiometric requirement to reduce all the titanium sub-chloride in the feed to the continuous back-mix reactor.

### Claim 13 (depends on 1)

A process as claimed in claim 1, wherein the temperature of the continuous back-mix reactor is less than 800° C.

### Claim 14 (depends on 13)

A process as claimed in claim 13, wherein the temperature of the continuous back-mix reactor is less than 650° C.

### Claim 15 (depends on 1)

A process as claimed in claim 1, wherein the residence time in said reactor is expressed as a ratio of the volume of titanium powder inside the continuous back-mix reactor to the volumetric rate of titanium powder produced in the continuous back-mix reactor, and is more than five minutes.

### Claim 16 (depends on 15)

A process as claimed in claim 15, wherein the residence time in the reactor is expressed as a ratio of the volume of titanium powder inside the continuous back-mix reactor to the volumetric rate of titanium powder produced in the continuous back-mix reactor, and is more than twenty minutes.

### Claim 17 (depends on 1)

A process as claimed in claim 1, wherein there is an excess of dispersed titanium recycled to the vessel producing the dissolved titanium halide species relative to the stoichiometric requirement to fully reduce TiCl4 feed to titanium dichloride.

### Claim 18 (depends on 1)

A process as claimed in claim 1, wherein the titanium chloride species is titanium dichloride.

### Claim 19 (depends on 1)

A process as claimed in claim 1, wherein the average feed ratio of the titanium chloride species and reducing metal to the continuous back-mix reactor is within 0.1% of the stoichiometric ratio required to fully reduce the titanium chloride salt to titanium metal.