- Assignees: Kabushiki Kaisha Toshiba
- Applicants: Kabushiki Kaisha Toshiba
- Inventors: Yosuke Horiuchi; Shinya Sakurada; Keiko Okamoto; Masaya Hagiwara; Tsuyoshi Kobayashi; Masaki Endo; Tadahiko Kobayashi; Kazuomi Yoshima
- Web page: https://patentgrep.com/patent/US20150143952A1

## CPC

- H01F 1/0557: {sintered}
- C22C 19/07: based on cobalt
- C22C 2202/02: Magnetic
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

In one embodiment, a permanent magnet includes a sintered compact having a composition represented by the composition formula: RpFeqMrCusCo100-p-q-r-s (where R is at least one element selected from rare earth elements, M is at least one element selected from Zr, Ti, and Hf, p is 10.5 atomic % or more and 12.5 atomic % or less, q is 24 atomic % or more and 40 atomic % or less, r is 0.88 atomic % or more and 4.5 atomic % or less, and s is 3.5 atomic % or more and 10.7 atomic % or less. The sintered compact has a structure having crystal grains constituted of a main phase including a Th2Zn17 crystal phase, and a crystal grain boundary. In the structure of the sintered compact, an average grain diameter of the crystal grains is 25 micrometer or more, and a volume fraction of the crystal grain boundary is 14% or less.

## Claims

### Claim 1

A permanent magnet comprising a sintered compact, the sintered compact comprising:
a composition represented by the following composition formula:
RpFeqMrCusCo100-p-q-r-s
wherein R is at least one element selected from the group consisting of rare earth elements,
M is at least one element selected from the group consisting of Zr, Ti, and Hf,
p is 10.5 atomic % or more and 12.5 atomic % or less,
q is 24 atomic % or more and 40 atomic % or less,
r is 0.88 atomic % or more and 4.5 atomic % or less, and
s is 3.5 atomic % or more and 10.7 atomic % or less; and
a structure having crystal grains constituted of a main phase including a Th2Zn17 crystal phase, and a crystal grain boundary existing between the crystal grains,
wherein an average grain diameter of the crystal grains is 25 micrometer or more, and a volume fraction of the crystal grain boundary is 14% or less.

### Claim 2 (depends on 1)

The permanent magnet of claim 1,
wherein the volume fraction of the crystal grain boundary is 5% or more.

### Claim 3 (depends on 1)

The permanent magnet of claim 1,
wherein the average grain diameter of the crystal grains is 200 micrometer or less.

### Claim 4 (depends on 1)

The permanent magnet of claim 1,
wherein, when the Th2Zn17 crystal phase is indexed as a TbCu7 crystal phase, an average distance between crystal grains with a displacement angle of a [0001] direction of the TbCu7 crystal phase being 45 degrees or more is 120 micrometer or more.

### Claim 5 (depends on 1)

The permanent magnet of claim 1,
wherein the main phase has a cell phase having the Th2Zn17 crystal phase and a cell wall phase existing in a form surrounding the cell phase.

### Claim 6 (depends on 1)

The permanent magnet of claim 1,
wherein 50 atomic % or more of the element R is Sm.

### Claim 7 (depends on 1)

The permanent magnet of claim 1,
wherein 50 atomic % or more of the element M is Zr.

### Claim 8 (depends on 1)

The permanent magnet of claim 1,
wherein 20 atomic % or less of the Co element is replaced with at least one kind of element A selected from the group consisting of Ni, V, Cr, Mn, Al, Si, Ga, Nb, Ta, and W.

### Claim 9 (depends on 1)

A motor comprising the permanent magnet of claim 1.

### Claim 10 (depends on 1)

A generator comprising the permanent magnet of claim 1.