# US 2015/0143848 A1 · Method for producing a coated component of transparent or opaque fused silica

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0143848 A1
- Document ID: US20150143848A1
- Status: Published application
- Kind: A1
- Application number: 14/543,718
- Filed: 2014-11-17
- Published: 2015-05-28
- Earliest claimed: 2013-11-28
- Assignees: Heraeus Quarzglas GmbH & Co. KG
- Applicants: Heraeus Quarzglas GmbH & Co. KG
- Inventors: Christian Schenk; Gerrit Scheich; Nils-Christian Nielsen
- Web page: https://patentgrep.com/patent/US20150143848A1

## CPC

- H02K 17/26: having rotors or stators designed to permit synchronous operation
- C03B 20/00: Processes specially adapted for the production of quartz or fused silica articles {, not otherwise provided for (C03B19/01, C03B19/066, C03B19/106, C03B19/12, C03B19/14, C03B37/00 take precedence)}
- C03C 3/06: with more than 90% silica by weight, e.g. quartz {(C03C3/045 takes precedence)}
- C03C 17/04: by fritting glass powder
- H02K 3/28: Layout of windings or of connections between windings (windings for pole-changing H02K17/06, H02K17/14, H02K19/12, H02K19/32)
- H02K 5/225: {Terminal boxes or connection arrangements (specially adapted for submersible motors H02K5/132)}
- H02K 11/0094: {Structural association with other electrical or electronic devices}
- H02K 11/20: for measuring, monitoring, testing, protecting or switching (rectifiers H02K11/04; power electronics H02K11/33)
- H02K 17/22: having rotors with windings connected to slip-rings
- C03C 2217/213: SiO2
- C03C 2218/11: from solutions or suspensions
- H02K: DYNAMO-ELECTRIC MACHINES (dynamo-electric relays H01H53/00; conversion of DC or AC input power into surge output power {H03K3/53})
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A method for producing a coated component consisting of transparent or opaque fused silica comprises a method step in which a SiO2 granulation layer is applied to a coating surface of a substrate, which in the area of the free surface has a relatively great granulation fine fraction. Starting from this, in order to achieve a smooth, preferably also dense surface layer, it is suggested according to the invention that the application of the SiO2 granulation layer comprises (i) providing a dispersion containing a dispersion liquid and amorphous SiO2 particles which form a coarse fraction with particle sizes ranging between 1 μm and 50 μm and a fine fraction of SiO2 nanoparticles having particle sizes of less than 100 nm, wherein the solids content of the dispersion is between 70 and 80 wt.-%, and of which between 2 wt.-% and 15 wt.-% are the SiO2 nanoparticles, (ii) applying the dispersion to the coating surface by casting or spraying it thereonto so as to form a slurry layer having a layer thickness of at least 0.3 mm; and (iii) drying the slurry layer by removing the dispersion liquid at a rate and in a direction such that under the action of the dispersion liquid being removed the fine fraction is enriched in the outer portion of the granulation layer, thereby forming a casting skin.

## Claims

### Claim 1

A method for producing a coated component consisting of transparent or opaque fused silica, the method comprising:
(a) providing a substrate of transparent or of opaque fused silica that comprises a coating surface:
(b) applying a SiO2 granulation layer to the coating surface, said granulation layer having an inner portion adjoining the coating surface and having a first granulation fine fraction, and an outer portion adjoining a free surface of the granulation layer and having a second granulation fine fraction, wherein the second granulation fine fraction is higher than the first granulation fine fraction;
(c) sintering the granulation layer so as to form a dense SiO2 surface layer, wherein the applying the SiO2 granulation layer according to method step (b) comprises:
(I) providing a dispersion containing a dispersion liquid and a solids content that comprises amorphous SiO2 particles, said amorphous SiO2 particles comprising a coarse fraction with particle sizes ranging between 1 μm and 50 μm and a fine fraction of SiO2 nanoparticles having particle sizes of less than 100 nm, wherein the solids content constitutes between 70 and 80 wt.-% of the dispersion, and wherein the SiO2 nanoparticles constitute between 2 wt.-% and 15 wt.-% of the dispersion,
(II) applying the dispersion to the coating surface by casting or spraying it thereonto so as to form a slurry layer having a layer thickness of at least 0.3 mm; and
(III) drying the slurry layer by removing the dispersion liquid at a rate and in a direction such that the removing enriches the fine fraction in the outer portion of the granulation layer, and a casting skin is formed.

### Claim 2 (depends on 1)

The method according to claim 1, wherein a measure is provided that slows the drying of the slurry layer.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the measure comprises moisturizing the coating surface prior to the applying of the dispersion according to method step (II).

### Claim 4 (depends on 1)

The method according to claim 1, wherein the slurry layer is mechanically densified.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the slurry layer is densified with a treatment of the slurry layer by spreading with a doctor blade.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the layer thickness of the slurry layer is not more than 3 mm.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the SiO2 nanoparticles in the dispersion constitute not more than 10% by weight of the dispersion.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the coarse fraction consists of splintery amorphous SiO2 granules with a grain size distribution having a D50 value between 3 μm and 30 μm.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the dispersion liquid consists of an aqueous base.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the solids content of the dispersion is in the range between 74 wt.-% and 78 wt.-%.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the dispersion is free of binders.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the casting skin has a thickness ranging from 3 μm to 15 μm.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the fine fraction of SiO2 nanoparticles with particle sizes of less than 100 μm constitutes a volume fraction of the casting skin of more than 70%.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the layer thickness of the slurry layer is not more than 1.5 mm.

### Claim 15 (depends on 1)

The method according to claim 1, wherein the casting skin has a thickness ranging from 5 μm to 10 μm.

### Claim 16 (depends on 1)

The method according to claim 1, wherein the fine fraction of SiO2 nanoparticles with particle sizes of less than 100 nm accounts for a volume fraction of the casting skin of more than 80%.