# US 2015/0143698 A1 · Pulling rolls for making sheet glass and methods of making and using

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0143698 A1
- Document ID: US20150143698A1
- Status: Published application
- Kind: A1
- Application number: 14/611,794
- Filed: 2015-02-02
- Published: 2015-05-28
- Earliest claimed: 2010-07-02
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Dean Veral Neubauer
- Web page: https://patentgrep.com/patent/US20150143698A1

## CPC

- F27D 19/00: Arrangements of controlling devices
- B29D 99/0035: {rollers or cylinders having an axial length of several times the diameter, e.g. for embossing, pressing, or printing}
- C03B 17/068: {Means for providing the drawing force, e.g. traction or draw rollers}
- Y10T 29/49549: Work contacting surface element assembled to core
- Y10T 29/49554: Work contacting surface having annular axial sections
- F27D: DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS OR RETORTS, IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KIND OF FURNACE
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A pulling roll for glass manufacture made from a millboard material fired to minimize or eliminate weight loss during operation. Methods for preparing and using such a pulling roll are also disclosed.

## Claims

### Claim at position 1

1-23. (canceled)

### Claim 24

A method of making a pulling roll, comprising the steps:
a. firing a plurality of millboard disks at a predetermined firing temperature and time;
b. selecting the predetermined firing temperature and time such that the disks do not undergo a weight loss from thermal perturbations of more than 5% upon exposure to an expected pulling roll operating temperature; and
c. assembling the plurality of millboard disks on a pulling roll shaft to form a pulling roll.

### Claim 25 (depends on 24)

The method of claim 24, wherein the firing temperature and time are selected such that the disks exhibit substantially no weight loss from thermal perturbations upon exposure to an expected pulling roll operating temperature.

### Claim 26 (depends on 24)

The method of claim 24, further comprising:
determining the firing temperature and time based on at least one of a thermogravimetric analysis and a differential thermal analysis of the millboard disks from ambient to an upper profile temperature that is higher than the expected pulling roll operating temperature.

### Claim 27 (depends on 26)

The method of claim 26, wherein the upper profile temperature is further characterized by no appreciable weight loss in the disks during the at least one of a thermogravimetric analysis and a differential thermal analysis, and the firing temperature is set at or above the upper profile temperature.

### Claim 28 (depends on 27)

The method of claim 27, wherein the firing temperature is set at approximately 50° C. higher than the upper profile temperature.

### Claim 29 (depends on 24)

The method of claim 24, wherein the millboard disks have a commercially available millboard composition that comprises a refractory fiber, a mica and a clay, the firing temperature is at least 900° C. and the predetermined time is at least 4 hours.

### Claim 30

A method of making pulling roll disks, comprising the steps:
a. firing a plurality of millboard disks at a predetermined firing temperature and time; and
b. selecting the predetermined firing temperature and time such that the disks do not undergo a weight loss from thermal perturbations of more than 5% upon exposure to an expected pulling roll operating temperature.

### Claim 31 (depends on 30)

The method of claim 30, wherein the firing temperature and time are selected such that the disks exhibit substantially no weight loss from thermal perturbations upon exposure to an expected pulling roll operating temperature.

### Claim 32 (depends on 30)

The method of claim 30, further comprising:
determining the firing temperature and time based on a thermal profile of the millboard disks from ambient to an upper profile temperature that is higher than the expected pulling roll operating temperature.

### Claim 33 (depends on 32)

The method of claim 32, wherein the upper profile temperature is further characterized by no appreciable weight loss in the disks during the thermal profile and the firing temperature is set at or above the upper profile temperature.

### Claim 34 (depends on 33)

The method of claim 33, wherein the firing temperature is set at approximately 50° C. higher than the upper profile temperature.

### Claim 35 (depends on 30)

The method of claim 30, wherein the millboard disks have a commercially available millboard composition that comprises a refractory fiber, a mica and a clay, the firing temperature is about 900° C. and the predetermined time is at least 4 hours.

### Claim 36

A method for determining a firing program for a millboard material in a pulling roll, comprising the steps:
a. determining an operating temperature for a pulling roll comprising a millboard material;
b. monitoring the weight of the millboard material while heating the material in a thermal profile, the profile having a profile temperature range from about ambient temperature up to at least about the operating temperature for the pulling roll; and
c. determining a firing temperature and a firing time for the millboard material from the monitoring step such that the pulling roll comprising the millboard material does not undergo a weight loss from thermal perturbations of more than 5% upon exposure to the operating temperature for the pulling roll.

### Claim 37 (depends on 36)

The method of claim 36, wherein the firing temperature and the firing time for the millboard material are such that the pulling roll comprising the millboard material exhibits substantially no weight loss from thermal perturbations upon exposure to the operating temperature for the pulling roll.

### Claim 38 (depends on 36)

The method of claim 36, wherein the monitoring step further comprises monitoring the rate of weight loss of the millboard material while heating the material in the thermal profile.

### Claim 39 (depends on 36)

The method of claim 36, wherein the profile temperature range is from about ambient temperature up to an upper profile temperature that is 50° C. or greater than the operating temperature for the pulling roll.

### Claim 40 (depends on 39)

The method of claim 39, wherein the determining step further comprises determining a firing temperature and a firing time for the millboard material from the monitoring step such that the pulling roll comprising the millboard material does not undergo a weight loss from thermal perturbations of more than 5% upon exposure to the upper profile temperature during operation of the pulling roll.

### Claim 41 (depends on 36)

The method of claim 36, wherein the determining step further comprises selecting the firing temperature such that the firing temperature is between a maximum weight loss temperature in the profile temperature range and the operating temperature for the pulling roll, the maximum weight loss temperature is defined by the maximum temperature in the profile temperature range in which the millboard material has exhibited weight loss during the monitoring step.

### Claim 42 (depends on 41)

The method of claim 41, wherein the maximum weight loss temperature is about 850° C. or lower for the millboard material, and the firing temperature is about 50° C. higher than the maximum weight loss temperature.

### Claim 43 (depends on 41)

The method of claim 41, wherein the millboard material has a commercially available millboard composition that comprises a refractory fiber, a mica and a clay.