# US 2015/0140215 A1 · Durable conformal wear-resistant carbon-doped metal oxide-comprising coating

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0140215 A1
- Document ID: US20150140215A1
- Status: Published application
- Kind: A1
- Application number: 14/539,172
- Filed: 2014-11-12
- Published: 2015-05-21
- Earliest claimed: 2007-02-23
- Assignees: Applied Microstructures, Inc.
- Applicants: Applied Microstructures, Inc.
- Inventors: Boris Kobrin; Romuald Nowak; Jeffrey D. Chinn
- Web page: https://patentgrep.com/patent/US20150140215A1

## CPC

- C09D 1/00: Coating compositions, e.g. paints, varnishes or lacquers, based on inorganic substances
- B81B 3/0075: {For improving wear resistance}
- C23C 16/403: {of aluminium, magnesium or beryllium}
- C23C 16/405: {of refractory metals or yttrium}
- C23C 16/45525: {Atomic layer deposition [ALD]}
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B81B: MICROSTRUCTURAL DEVICES OR SYSTEMS, e.g. MICROMECHANICAL DEVICES (piezoelectric, electrostrictive or magnetostrictive elements per se H10N30/00, H10N35/00)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

The present invention is related to carbon-doped metal oxide films. A method of depositing a low friction metal oxide film on a substrate is provided, including: using an atomic layer deposition technique, wherein said metal oxide film is deposited using at least an organo-metallic precursor, and wherein said substrate is at a temperature of 150° C. or lower during deposition of said metal oxide film, whereby a carbon-doped metal oxide film is obtained. The carbon-doped metal oxide films provide a low coefficient of friction, for example ranging from about 0.05 to about 0.4. In addition, the carbon-doped metal oxide films provide anti-stiction properties, where the measured work of adhesion is less than 10 μJ/m2. In addition, the carbon-doped metal oxide films provide unexpectedly good water vapor transmission properties. The carbon content in the carbon-doped metal oxide films ranges from about 5 atomic % to about 20 atomic %.

## Claims

### Claim 1

A method of depositing a low friction metal oxide film on a substrate, said method comprising:
using an atomic layer deposition technique, wherein said metal oxide film is deposited using at least an organo-metallic precursor, and wherein said substrate is at a temperature of 150° C. or lower during deposition of said metal oxide film, whereby a carbon-doped metal oxide film is obtained.

### Claim 2 (depends on 1)

A method in accordance with claim 1, wherein said metal oxide film is deposited using an organo-metallic precursor and a water vapor precursor.

### Claim 3 (depends on 1)

A method in accordance with claim 1, wherein said substrate temperature ranges from about 25° C. to about 150° C.

### Claim 4 (depends on 3)

A method in accordance with claim 3, wherein said substrate temperature ranges from about 25° C. to about 120° C.

### Claim 5 (depends on 4)

A method in accordance with claim 4, wherein said substrate temperature ranges from about 55° C. to about 80° C.

### Claim 6 (depends on 1)

A method in accordance with claim 1, wherein said organo-metallic precursor contains a metal selected from the group consisting of aluminum, indium, titanium, zirconium, hafnium, tantalum, and combinations thereof.

### Claim 7 (depends on 6)

A method in accordance with claim 6, wherein said metal is selected from the group consisting of aluminum, titanium, and combinations thereof.

### Claim 8 (depends on 1)

A method in accordance with claim 1, wherein a pressure in a processing chamber in which said carbon-doped metal oxide film is deposited ranges from about 0.01 Torr to about 1 Torr during the deposition of said organo-metallic precursor upon said substrate and ranges from about 0.01 Torr to about 5 Torr during the deposition of said water vapor precursor.

### Claim 9 (depends on 8)

A method in accordance with claim 8, wherein the time duration of exposure of said substrate to each precursor ranges from about 0.05 seconds to about 30 seconds.

### Claim 10 (depends on 9)

A method in accordance with claim 9, wherein deposition of an organometallic precursor followed by deposition of a water vapor precursor is considered to comprise one cycle, and wherein the number of cycles carried out to form said low friction carbon-doped metal oxide film ranges from about 10 to about 100.

### Claim 11

A method of depositing a film providing a coefficient of friction less than or equal to about 0.4 on a substrate, said method comprising:
depositing a carbon-doped metal oxide film by an atomic layer deposition technique, wherein said carbon-doped metal oxide film is deposited using at least an organo-metallic precursor, and wherein said substrate is at a temperature of 150° C. or lower during deposition of said metal oxide film;
wherein said metal is selected from the group consisting of aluminum, indium, titanium, zirconium, hafnium, tantalum, and combinations thereof;
wherein a carbon content of said carbon-doped metal oxide film ranges from about 5 atomic % to about 20 atomic %;
wherein the carbon-doping provides for a measured work of adhesion less than or equal to 10 μJ/m2.

### Claim 12 (depends on 11)

A method in accordance with claim 11, wherein said coefficient of friction ranges from about 0.05 to about 0.4.

### Claim 13 (depends on 11)

A method in accordance with claim 11, wherein said metal is selected from the group consisting of aluminum, titanium, and combinations thereof.

### Claim 14 (depends on 11)

A method in accordance with claim 11, wherein said carbon content of said carbon-doped film ranges from about 10 atomic % to about 20 atomic %.

### Claim 15 (depends on 11)

A method in accordance with claim 11, wherein said film thickness ranges from about 20 Å to about 400 Å.

### Claim 16 (depends on 11)

A method in accordance with claim 11, wherein said measured work of adhesion ranges from 10 μJ/m2 to about 0.5 μJ/m2.

### Claim 17 (depends on 11)

A method in accordance with claim 11, wherein said substrate defines at least one MEMS device.

### Claim 18 (depends on 17)

A method in accordance with claim 17, wherein said MEMS device is selected from the following: bio-MEMS device, microfluidic device, ink-jet head, thin film head, or optical device.

### Claim 19 (depends on 11)

A method in accordance with claim 11, wherein said substrate defines at least one of the following devices: a bio-MEMS device, a microfluidic device, an ink-jet head, a thin film head, or an optical device.

### Claim 20

A method of depositing a film providing a coefficient of friction less than about 0.4 on a substrate, said method comprising:
depositing a carbon-doped metal oxide film by an atomic layer deposition technique, wherein said carbon-doped metal oxide film is deposited using at least an organo-metallic precursor, and wherein said substrate is at a temperature of 150° C. or lower during deposition of said metal oxide film;
wherein said metal is selected from the group consisting of aluminum, titanium, and combinations thereof;
wherein a carbon content of said carbon-doped metal oxide film ranges from about 10 atomic % to about 20 atomic %;
wherein the carbon-doping provides for a measured work of adhesion less than or equal to 10 μJ/m2.

### Claim 21 (depends on 20)

A method in accordance with claim 20, wherein a thickness of said film ranges from about 20 Å to about 100 Å.

### Claim 22 (depends on 20)

A method in accordance with claim 20, wherein the carbon-doping provides for a measured work of adhesion of less than 1 μJ/m2.