# US 2015/0129803 A1 · Stannate fluorescent material and method for preparing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0129803 A1
- Document ID: US20150129803A1
- Status: Published application
- Kind: A1
- Application number: 14/399,005
- Filed: 2012-07-31
- Published: 2015-05-14
- Earliest claimed: 2012-07-31
- Assignees: Ocean's King Lighting Science & Technology Co., Ltd.; Shenzhen Ocean's King Lighting Engineering Co., Ltd.
- Inventors: Mingjie Zhou; Rong Wang; Guitang Chen
- Web page: https://patentgrep.com/patent/US20150129803A1

## CPC

- C09K 11/025: {non-luminescent particle coatings or suspension media}
- C09K 11/7731: {with alkaline earth metals}
- H01J 29/20: characterised by the luminescent material
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

The present invention provides a stannate fluorescent material having a formula: A2-xSnO4:Eux@SnO2@My; wherein A is selected from the group consisting of Ca, Sr, and Ba; M is at least one metal nanoparticles selected from the group consisting of Ag, Au, Pt, Pd, and Cu; 0<x≦0.05; y is a mole ratio of M to Sn, and 0<y≦1×10−2; @represents coating, in the stannate fluorescent material, M serves as a core, SnO2 serves as an intermediate layer shell, and A2-xSnO4:Eux serves as an outer layer shell. In the stannate fluorescent material, a core-shell structure is formed by coating at least one metal nanoparticles selected from the group consisting of Ag, Au, Pt, Pd, and Cu, since metal nanoparticles can improve the internal quantum efficiency of the fluorescent material, the stannate fluorescent material exhibits a higher luminous intensity.

## Claims

### Claim 1

A stannate fluorescent material, having a formula: A2-xSnO4:Eux@SnO2@My wherein A is selected from the group consisting of Ca, Sr, and Ba;
M is at least one metal nanoparticles selected from the group consisting of Ag, Au, Pt, Pd, and Cu;
0<x≦0.05;
y is a mole ratio of M to Sn, and 0<y≦1×10−2;
@ represents coating, in the stannate fluorescent material, M serves as a core, SnO2 serves as an intermediate layer shell, and A2-xSnO4:Eux serves as an outer layer shell.

### Claim 2

A method of preparing a stannate fluorescent material, comprising the following steps:
preparing a sol containing M, wherein M is at least one metal nanoparticles selected from the group consisting of Ag, Au, Pt, Pd, and Cu;
surface-treating the sol containing M, adjusting the pH value of the sol containing M to 10 to 12, heating and stirring the sol containing M at a temperature of 60° C. to 90° C., adding sodium stannate, potassium stannate, or tin tetrachloride according to a mole ratio y of M to Sn of formula A2-xSnO4:Eux@SnO2@My, stirring and reacting, separating and drying to obtain SnO2@M powder coating M, wherein 0<y≦1×10−2;
mixing an A compound, an Eu compound, and the SnO2@M powder according to a stoichiometric ratio of formula of A2-xSnO4:Eu@SnO2@My to obtain a mixture;
heating the mixture, cooling and grinding the mixture to obtain the stannate fluorescent material having the formula A2-xSnO4:Eux@SnO2@My;
wherein A is selected from the group consisting of Ca, Sr, and Ba; 0<x≦0.05; in the stannate fluorescent material, M serves as a core, SnO2 serves as an intermediate layer shell, and A2-xSnO4:Eux serves as an outer layer shell.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the step of preparing the sol containing M comprises:
mixing a salt solution of at least one metal selected from the group consisting of Ag, Au, Pt, Pd, and Cu, with an additive and a reductant, and reacting for 10 to 45 minutes to obtain the sol containing M.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the concentration of the salt solution of at least one metal selected from the group consisting of Ag, Au, Pt, Pd, and Cu ranges from 1×10−3 mol/L to 5×10−2 mol/L;
the additive is at least one selected from the group consisting of polyvinylpyrrolidone, sodium citrate, cetyl trimethyl ammonium bromide, sodium lauryl sulfate, and sodium dodecyl sulfate;
the concentration of the additive in the sol containing M ranges from 1×10−4 g/mL to 5×102 g/mL;
the reductant is at least one selected from the group consisting of hydrazine hydrate, ascorbic acid, sodium citrate, and sodium borohydride;
a mole ratio between the reductant and metal ion of the salt solution of at least one metal selected from the group consisting of Ag, Au, Pt, Pd, and Cu ranges from 3.6:1 to 18:1.

### Claim 5 (depends on 2)

The method according to claim 2, wherein the step of surface-treating the sol containing M comprises: adding the sol containing M into an aqueous solution of polyvinyl pyrrolidone and stirring for 12 to 24 hours.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the concentration of the aqueous solution of polyvinyl pyrrolidone ranges from 0.005 g/mL to 0.01 g/mL.

### Claim 7 (depends on 2)

The method according to claim 2, wherein the step of adjusting the pH value of the sol containing M to 10 to 12 comprises adjusting the pH value using sodium hydroxide or ammonia.

### Claim 8 (depends on 2)

The method according to claim 2, wherein the stirring and reacting time takes 1 to 5 hours.

### Claim 9 (depends on 2)

The method according to claim 2, wherein the step of heating the mixture comprises:
precalcining the mixture at a temperature of 800° C. to 1200° C. for 2 to 12 hours, and then calcining the mixture at 1000° C. to 1400° C. for at 0.5 to 6 hours.

### Claim 10 (depends on 2)

The method according to claim 2, wherein the A compound is oxides, carbonates, acetates or oxalates corresponding to A; the Eu compound is oxides, carbonates, acetates or oxalates corresponding to Eu.