# US 2015/0105600 A1 · Adsorbents for the separation of para-xylene from c8 alkyl aromatic hydrocarbon mixtures, methods for separating para-xylene using the adsorbents and methods for making the adsorbents

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0105600 A1
- Document ID: US20150105600A1
- Status: Published application
- Kind: A1
- Application number: 14/054,687
- Filed: 2013-10-15
- Published: 2015-04-16
- Earliest claimed: 2013-10-15
- Assignees: Uop LLC
- Applicants: Uop LLC
- Inventors: Patrick C. Whitchurch; Santi Kulprathipanja; Gregory F. Maher
- Web page: https://patentgrep.com/patent/US20150105600A1

## CPC

- C07C 7/12: by adsorption, i.e. purification or separation of hydrocarbons with the aid of solids, e.g. with ion-exchangers
- B01J 20/18: Synthetic zeolitic molecular sieves
- B01J 20/186: {Chemical treatments in view of modifying the properties of the sieve, e.g. increasing the stability or the activity, also decreasing the activity}
- B01J 20/3071: {Washing or leaching}
- B01J 20/3078: {Thermal treatment, e.g. calcining or pyrolizing}
- B01J 20/3085: {Chemical treatments not covered by groups B01J20/3007 - B01J20/3078}
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS

## Abstract

Embodiments of adsorbents for separating para-xylene from a mixture of C8 alkyl aromatic hydrocarbons, methods for making such adsorbents, and methods for separating para-xylene using such adsorbents are provided. In one example, an adsorbent comprises a binderless adsorbent. The binderless adsorbent comprises zeolite X and has a K2O/(K2O+BaO+Na2O) molar ratio of from about 0.15 to about 0.4.

## Claims

### Claim 1

An adsorbent for separating para-xylene from a mixture of C8 alkyl aromatic hydrocarbons, the adsorbent comprising:
a binderless adsorbent comprising zeolite X and having a K2O/(K2O+BaO+Na2O) molar ratio of from about 0.15 to about 0.4.

### Claim 2 (depends on 1)

The adsorbent of claim 1, wherein the K2O/(K2O+BaO+Na2O) molar ratio is from about 0.2 to about 0.35.

### Claim 3 (depends on 1)

The adsorbent of claim 1, wherein the binderless adsorbent has a BaO/(K2O+BaO+Na2O) molar ratio of from about 0.6 to about 0.85.

### Claim 4 (depends on 3)

The adsorbent of claim 3, wherein the BaO/(K2O+BaO+Na2O) molar ratio is from about 0.65 to about 0.8.

### Claim 5 (depends on 1)

The adsorbent of claim 1, wherein the binderless adsorbent has a Na2O/(K2O+BaO+Na2O) molar ratio of from about 0.001 to about 0.04.

### Claim 6 (depends on 1)

The adsorbent of claim 1, wherein the binderless adsorbent has a water content of from about 2 to about 5 wt. % of the binderless adsorbent.

### Claim 7 (depends on 1)

The adsorbent of claim 1, wherein the binderless adsorbent has a silica to alumina molar ratio of from about 2 to about 2.6.

### Claim 8 (depends on 1)

The adsorbent of claim 1, wherein the binderless adsorbent has a prepared portion of the zeolite X and a converted portion of the zeolite X, and wherein the prepared portion of the zeolite X has a first silica to alumina molar ratio of from about 2.4 to about 2.6.

### Claim 9 (depends on 8)

The adsorbent of claim 8, wherein the converted portion of the zeolite X has a second silica to alumina molar ratio of from about 2 to about 2.2.

### Claim 10 (depends on 1)

The adsorbent of claim 1, wherein the zeolite X comprises nano-size zeolite X.

### Claim 11 (depends on 10)

The adsorbent of claim 10, wherein the binderless adsorbent has a prepared portion of the zeolite X and a converted portion of the zeolite X, and wherein the converted portion of the zeolite X comprises the nano-size zeolite X.

### Claim 12 (depends on 11)

The adsorbent of claim 11, wherein the prepared portion of the zeolite X has an average crystalline size of from about 1 to about 3 μm.

### Claim 13

A method for separating para-xylene from a mixture of C8 alkyl aromatic hydrocarbons, the method comprising the steps of:
contacting a binderless adsorbent with a feed stream comprising the mixture of C8 alkyl aromatic hydrocarbons to adsorb para-xylene from the feed stream and form a para-xylene-adsorbed binderless adsorbent, wherein the binderless adsorbent comprises zeolite X and has a K2O/(K2O+BaO+Na2O) molar ratio of from about 0.15 to about 0.4; and
desorbing para-xylene from the para-xylene-adsorbed binderless adsorbent.

### Claim 14 (depends on 13)

The method of claim 13, wherein the step of contacting comprises contacting the binderless adsorbent with the feed stream at a temperature of from about 100 to about 160° C.

### Claim 15 (depends on 13)

The method of claim 13, wherein the step of desorbing comprises contacting the para-xylene-adsorbed binderless adsorbent with toluene to desorb para-xylene from the para-xylene-adsorbed binderless adsorbent and form an extract stream comprising toluene and para-xylene.

### Claim 16

A method for making an adsorbent for separating para-xylene from a mixture of C8 alkyl aromatic hydrocarbons, the method comprising the steps of:
forming a particle comprising a zeolite X precursor and a first portion of zeolite X;
activating the zeolite X precursor of the particle at activation conditions effective to form an activated zeolite X precursor;
digesting the particle with a caustic solution to convert the activated zeolite X precursor to a second portion of zeolite X and form a binderless zeolite X particle having ion exchangeable sites with cations; and
exchanging the cations with barium and potassium ions at the ion exchangeable sites to form a binderless adsorbent, wherein the binderless adsorbent comprises the zeolite X and has a K2O/(K2O+BaO+Na2O) molar ratio of from about 0.15 to about 0.4.

### Claim 17 (depends on 16)

The method of claim 16, wherein the step of activating comprises activating the zeolite X precursor at the activation conditions including a temperature of from about 500 to about 700° C.

### Claim 18 (depends on 16)

The method of claim 16, wherein the step of digesting comprises digesting the particle with sodium hydroxide to convert the activated zeolite X precursor to the second portion of zeolite X.

### Claim 19 (depends on 16)

The method of claim 16, wherein the step of exchanging the cations comprises ion exchanging the binderless zeolite X particle using a solution comprising potassium chloride and barium chloride.

### Claim 20 (depends on 16)

The method of claim 16, wherein the step of exchanging the cations comprises forming the binderless adsorbent having the first portion of zeolite X present in an amount of from about 60 to about 95 wt. % of binderless adsorbent and the second portion of zeolite X present in an amount of from about 5 to about 40 wt. % of the binderless adsorbent.