# US 2015/0105583 A1 · Catalyst For Methacrylic Acid Production, Process For Producing The Same, And Process For Producing Methacrylic Acid Using The Catalyst

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0105583 A1
- Document ID: US20150105583A1
- Status: Published application
- Kind: A1
- Application number: 14/401,560
- Filed: 2013-05-16
- Published: 2015-04-16
- Earliest claimed: 2012-05-18
- Assignees: Nippon Kayaku Kabushiki Kaisha
- Applicants: Nippon Kayaku Kabushiki Kaisha
- Inventors: Hideomi Sakai; Eiji Nishimura; Tomoyuki Ejiri
- Web page: https://patentgrep.com/patent/US20150105583A1

## CPC

- B01J 27/24: Nitrogen compounds
- B01J 23/002: {Mixed oxides other than spinels, e.g. perovskite}
- B01J 27/199: with chromium, molybdenum, tungsten or polonium
- B01J 37/0009: {Use of binding agents; Moulding; Pressing; Powdering; Granulating; Addition of materials ameliorating the mechanical properties of the product catalyst}
- B01J 37/0045: {Drying a slurry, e.g. spray drying}
- C07C 51/235: of —CHO groups or primary alcohol groups
- C07C 51/252: {of propene, butenes, acrolein or methacrolein}
- C07C 51/377: by splitting-off hydrogen or functional groups; by hydrogenolysis of functional groups {(C07C51/36 - C07C51/373 take precedence)}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 2523/00: Constitutive chemical elements of heterogeneous catalysts
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS

## Abstract

An object of the present invention is to provide a process for producing a catalyst for gas-phase contact oxidation of methacrolein, isobutyraldehyde or isobutyric acid to produce methacrylic acid in a high yield and a high selectivity, and a catalyst wherein an alkali metal element, particularly cesium among alkali metal elements, is added by a specific method in a partially neutralized salt of a hetero polyacid which contains Mo, V, P, an alkali metal element and NH4 as essential active ingredients, the catalyst being characterized by having extremely high catalytic performance.

## Claims

### Claim 1

A process for producing a catalyst for methacrylic acid production, comprising the following steps:
Step a): a step of preparing a slurry containing at least molybdenum, phosphorus and vanadium;
Step b): a step of cooling the slurry obtained in Step a) and subsequently adding an alkali metal compound with stirring of the slurry to prepare a slurry of a partially neutralized salt of a hetero polyacid;
Step c): a step of adding an ammonium compound to the slurry obtained in Step b);
Step d): a step of drying the slurry, to which the ammonium compound has been added, obtained in Step c) to obtain a dry powder having a composition shown by the following (Formula 1);
Step e): a step of shaping the dry powder obtained in Step d); and
Step f): a step of calcinating the shaped product obtained in Step e):
Mo10VaPb(NH4)cXdYeOf (Formula 1)
wherein Mo represents molybdenum; V represents vanadium; P represents phosphorus; (NH4) represents an ammonium group; X represents at least one alkali metal element selected from the group consisting of K, Rb and Cs; Y represents at least one element selected from the group consisting of Sb, As, Cu, Ag, Mg, Zn, Al, B, Ge, Sn, Pb, Ti, Zr, Cr, Re, Bi, W, Fe, Co, Ni, Ce and Th; O represents oxygen; a to e represents atomic ratios of respective elements, a: 0.1≦a≦6.0, b: 0.5≦b≦6.0, c: 0.1≦c≦10.0, d: 0.1≦d≦3.0, e: 0≦e≦3, and f is a value other than 0, which is determined depending on oxidation states and atomic ratios of individual elements.

### Claim 2 (depends on 1)

The process for producing a catalyst for methacrylic acid production according to claim 1,
wherein in the Step b), the alkali metal compound is added with stirring at a power requirement for stirring per unit volume Pv [kW/m3] of 0.01 to 4.00 [kW/m3].

### Claim 3 (depends on 1)

The process for producing a catalyst for methacrylic acid production according to claim 1,
wherein temperature of the slurry containing at least molybdenum, phosphorus and vanadium is controlled to 0 to 35° C. at the time of adding the alkali metal compound in the above Step b).

### Claim 4 (depends on 1)

The process for producing a catalyst for methacrylic acid production according to claim 1,
wherein the above Step e) is a step of coating an inert support with the dry powder using a binder to form a coated catalyst.

### Claim 5 (depends on 4)

The process for producing a catalyst for methacrylic acid production according to claim 4,
wherein the binder is at least one kind of liquid selected from the group consisting of water and organic compounds having a boiling point of 150° C. or lower under 1 atm.

### Claim 6 (depends on 1)

The process for producing a catalyst for methacrylic acid production according to claim 1,
wherein calcination temperature in Step f) is from 100 to 450° C.

### Claim 7 (depends on 1)

A catalyst for methacrylic acid production, which is obtained by the process for producing a catalyst for methacrylic acid production according to claim 1.

### Claim 8 (depends on 7)

A process for producing methacrylic acid, the process comprising:
conducting gas-phase contact oxidation of at least one selected from the group consisting of methacrolein, isobutyraldehyde and isobutyric acid using the catalyst according to claim 7.