# US 2015/0105531 A1 · Method for direct ammonolysis of polycarbonate-containing materials and products

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0105531 A1
- Document ID: US20150105531A1
- Status: Published application
- Kind: A1
- Application number: 14/053,954
- Filed: 2013-10-15
- Published: 2015-04-16
- Earliest claimed: 2013-10-15
- Assignees: Saudi Basic Industries Corporation
- Applicants: Saudi Basic Industries Corporation
- Inventors: Alexander Stanislaus; Venkata Ramanarayanan Ganapathy Bhotla; PS Sreenivasan; Philip Wesley Bell
- Web page: https://patentgrep.com/patent/US20150105531A1

## CPC

- C07C 37/685: {Processes comprising at least two steps in series}
- C07C 37/00: Preparation of compounds having hydroxy or O-metal groups bound to a carbon atom of a six-membered aromatic ring
- C08G 64/38: using other monomers
- C08J 11/16: by treatment with inorganic material (C08J11/14 takes precedence)
- C08J 2369/00: Characterised by the use of polycarbonates; Derivatives of polycarbonates
- Y02W 30/62: Plastics recycling; Rubber recycling
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A method for recovering a dihydroxy aromatic compound and urea from a polycarbonate-containing composition comprising a polycarbonate and a phosphorus-containing flame retardant, comprising contacting the composition with ammonia in the presence of a swelling solvent for a time sufficient to depolymerize the polycarbonate producing a dihydroxy aromatic compound and urea.

## Claims

### Claim 1

A method for recovering a dihydroxy aromatic compound from a polycarbonate-containing composition comprising contacting the polycarbonate-containing composition with ammonia and a solvent at a temperature of from 20° C. to 100° C. for a time sufficient to depolymerize the polycarbonate to provide a dihydroxy aromatic compound and urea.

### Claim 2 (depends on 1)

The method of claim 1, wherein the composition comprises from 10 to 90 weight percent polycarbonate.

### Claim 3 (depends on 1)

The method of claim 1, wherein the composition comprises from 10 to 70 weight percent polycarbonate.

### Claim 4 (depends on 1)

The method of claim 1, wherein the composition comprises from 20 to 50 weight percent polycarbonate.

### Claim 5 (depends on 1)

The method of claim 1, wherein the composition comprises from 12 to 30 weight percent polycarbonate.

### Claim 6 (depends on 1)

The method of claim 1, wherein the solvent is a C1-10 alcohol or a ketone.

### Claim 7 (depends on 6)

The method of claim 6, wherein the solvent is methanol.

### Claim 8 (depends on 1)

The method of claim 1, wherein the method further comprises separating the dihydroxy aromatic compound and the urea from the solid residual polymeric composition by filtration.

### Claim 9 (depends on 1)

The method of claim 1, further comprising separating a blend of the alcohol and the urea from the dihydroxy aromatic compound by distillation.

### Claim 10 (depends on 1)

The method of claim 1, wherein the polycarbonate is bisphenol A polycarbonate, and the dihydroxy aromatic compound is bisphenol-A.

### Claim 11 (depends on 1)

The method of claim 1, wherein the phosphorus-containing flame retardant is bisphenol A bis(diphenyl phosphate), resorcinol bis(diphenyl phosphate), or a combination thereof.

### Claim 12 (depends on 1)

A method for the manufacture of a polycarbonate, the method comprising recovering the dihydroxy aromatic compound generated in claim 1, and polymerizing the dihydroxy aromatic compound and a carbonyl source to provide the polycarbonate.

### Claim 13 (depends on 12)

A polycarbonate manufactured by the method of claim 12.

### Claim 14 (depends on 1)

The method of claim 1, wherein the urea is isolated.

### Claim 15 (depends on 1)

The method of claim 1, wherein the urea is reacted to form CO2 and NH3.

### Claim 16 (depends on 15)

The method of claim 15, wherein the NH3 is reused in the process.

### Claim 17 (depends on 15)

The method of claim 15, wherein the CO2 is reacted with the dihydroxy aromatic compound to make a polycarbonate.

### Claim 18 (depends on 1)

The method of claim 1, wherein the dihydroxy aromatic compound is further processed to reduce the color thereof.

### Claim 19 (depends on 18)

The method of claim 18, wherein the further process is selected from the group of solvent recrystallization or exposure to adsorbent or chelants to bind impurities.

### Claim 20 (depends on 1)

A method for recovering a dihydroxy aromatic compound according to claim 1, wherein the polycarbonate-containing composition contains from 10 weight percent to 90 weight percent of a polycarbonate and the polycarbonate-containing composition is contacted with ammonia and a swelling solvent during substantially coextensive periods for a time sufficient to depolymerize the polycarbonate to provide a dihydroxy aromatic compound and urea.

### Claim 21 (depends on 1)

A method for recovering a dihydroxy aromatic compound according to claim 1, wherein the polycarbonate-containing composition contains from 10 weight percent to 90 weight percent of a polycarbonate and the contacting of the polycarbonate-containing composition with a swelling solvent is from 1 to 10 hours, and contacting the polycarbonate-containing composition with ammonia for a time sufficient to depolymerize the polycarbonate and provide a dihydroxy aromatic compound and urea.

### Claim 22

A method for recovering a dihydroxy aromatic compound from a polycarbonate-containing composition comprising a polycarbonate and a component comprising a phosphorus-containing flame retardant, or acrylonitrile-butadiene-styrene, or a combination of the phosphorus-containing flame retardant and acrylonitrile-butadiene-styrene, the method comprising:
contacting the polycarbonate-containing composition with ammonia for a time sufficient to depolymerize the polycarbonate to provide a dihydroxy aromatic compound and urea in a liquid phase and a solid residual polymeric composition having dihydroxy aromatic compound adhering to its surface;
separating the solid residual polymeric composition from the liquid phase; and
washing the solid polymeric composition with a C1-10 alcohol to recover additional dihydroxy aromatic compound.