# US 2015/0105515 A1 · Nitrile rubbers having low emission values

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0105515 A1
- Document ID: US20150105515A1
- Status: Published application
- Kind: A1
- Application number: 14/513,522
- Filed: 2014-10-14
- Published: 2015-04-16
- Earliest claimed: 2013-10-14
- Assignees: LANXESS Deutschland GmbH
- Applicants: LANXESS Deutschland GmbH
- Inventors: Sven BRANDAU; Andreas KAISER; Hans MAGG; Uwe WESTEPPE
- Web page: https://patentgrep.com/patent/US20150105515A1

## CPC

- C08F 36/06: Butadiene
- C08C 1/16: in floc form
- C08F 220/44: Acrylonitrile
- C08F 236/12: with nitriles
- C08J 3/247: {Heating methods}
- C08K 3/04: Carbon
- C08L 9/02: Copolymers with acrylonitrile
- C08J 2309/02: Copolymers with acrylonitrile
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08C: TREATMENT OR CHEMICAL MODIFICATION OF RUBBERS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

An improved polymerization process using a specific molecular weight regulator makes it possible to produce new nitrile rubbers featuring particularly low emission values and giving vulcanizates which have an advantageous profile of properties and which are of outstanding quality, in particular in odour-sensitive applications.

## Claims

### Claim 1

A nitrile rubber comprising repeating units of at least one α,β-unsaturated nitrite monomer and at least one conjugated diene monomer, wherein said nitrite rubber has an emission quotient E according to general formula (I) of less than or equal to 0.25 mg/(kg*Mooney units)
E
=
[
volatile


constituents
]
[
Mooney


viscosity
]
×
[
nitrile


content
]
100
(
I
)
where
[volatile constituents] is the volatile constituents concentration in mg/kg of nitrile rubber determined by TDS GC-MS analysis according to VDA recommendation 278 (version 09/2002) between 28.4 min and 34.0 min,
[Mooney viscosity] is the Mooney viscosity ML 1+4 at 100° C. of the nitrite rubber in Mooney units determined according to ASTM D 1646 and
[nitrile content] is the dimensionless α,β-unsaturated nitrite content in the nitrile rubber, wherein such content is determined in % by weight pursuant to DIN 53 625 according to Kjeldahl.

### Claim 2 (depends on 1)

The nitrile rubber according to claim 1, wherein the emission quotient E according to formula (I) is less than or equal to 0.22 mg/(kg*Mooney units).

### Claim 3 (depends on 2)

The nitrile rubber according to claim 2, wherein the emission quotient E according to formula (I) is less than or equal to 0.20 mg/(kg*Mooney units).

### Claim 4 (depends on 1, 2)

The nitrile rubber according to claim 1 or 2 which further comprises repeating units of one or more additional copolymerizable monomers.

### Claim 5 (depends on 1)

The nitrile rubber according to claim 1, wherein the at least one conjugated diene is selected from (C4-C6) conjugated dienes and mixtures thereof.

### Claim 6 (depends on 5)

The nitrile rubber according to claim 5, wherein the at least one conjugated diene is selected from 1,2-butadiene, 1,3-butadiene, isoprene, 2,3-dimethylbutadiene, piperylene and mixtures thereof.

### Claim 7 (depends on 5)

The nitrile rubber according to claim 5, wherein the at least one conjugated diene is 1,3-butadiene.

### Claim 8 (depends on 1)

The nitrile rubber according to claim 1, wherein the at least one α,β-unsaturated nitrile is selected from (C3-C5) α,β-unsaturated nitriles and mixtures thereof.

### Claim 9 (depends on 8)

The nitrile rubber according to claim 8, wherein the at least one α,β-unsaturated nitrile is selected from acrylonitrile, methacrylonitrile, ethacrylonitrile and mixtures thereof.

### Claim 10 (depends on 9)

The nitrile rubber according to claim 9, wherein the at least one α,β-unsaturated nitrile is acrylonitrile.

### Claim 11 (depends on 1)

The nitrile rubber according to claim 1 having a Mooney viscosity ML 1+4 at 100° C. of from 10 to 150 Mooney units (MU).

### Claim 12 (depends on 11)

The nitrile rubber according to claim 11 having a Mooney viscosity ML 1+4 at 100° C. of from 20 to 100 Mooney units (MU).

### Claim 13 (depends on 1)

A process for producing nitrile rubbers according to claim 1 comprising polymerizing at least one α,β-unsaturated nitrile monomer and at least one conjugated diene monomer in emulsion, wherein the emulsion polymerization is carried out in the presence of tertiary nonyl mercaptan as molecular weight regulator up to a conversion of at least 60% by weight, based on the sum of the monomers used.

### Claim 14 (depends on 13)

The process according to claim 13, wherein the emulsion polymerization is carried out up to a conversion of from 60% to 98%, based on the sum of the monomers used.

### Claim 15 (depends on 14)

The process according to claim 14, wherein the emulsion polymerization is carried out up to a conversion of from 62% to 95%, based on the sum of the monomers used.

### Claim 16 (depends on 14)

The process according to claim 14, wherein the emulsion polymerization is carried out up to a conversion of from 65% to 95%, based on the sum of the monomers used.

### Claim 17 (depends on 13)

The process according to claim 13, wherein the molecular weight regulator in the form of the tertiary nonyl mercaptan is used either
a) in the form of tert-nonyl mercaptan at a purity of at least 95% by weight, or else
b) in the form of a mixture comprising (i) at least 50% by weight but less than 95% by weight of tert-nonyl mercaptan and (ii) the remainder being one or more further isomeric nonyl mercaptans and/or one or more further C10-C16 alkylthiols.

### Claim 18 (depends on 17)

The process according to claim 17, wherein the molecular weight regulator in the form of the tertiary nonyl mercaptan is used
a) in the form of tert-nonyl mercaptan at a purity of at least 97% by weight.

### Claim 19 (depends on 13)

The process according to claim 13, wherein the molecular weight regulator is used in an amount of from 0.05 to 3 parts by weight, based on 100 parts by weight of the monomer mixture.

### Claim 20 (depends on 19)

The process according to claim 19, wherein the molecular weight regulator is used in an amount of from 0.1 to 1.5 parts by weight, based on 100 parts by weight of the monomer mixture.

### Claim 21 (depends on 1)

A vulcanizable mixture comprising the nitrile rubber according to claim 1 and at least one crosslinker.

### Claim 22 (depends on 21)

The vulcanizable mixture according to claim 21 which further comprises one or more fillers and no, one or more additional additive(s).

### Claim 23 (depends on 22)

The vulcanizable mixture according to claim 22, wherein the one or more additional additives are selected from the group consisting of filler activators, antiozonants, ageing stabilizers, antioxidants, processing aids, extender oils, plasticizers, reinforcing materials and mould release agents.

### Claim 24 (depends on 21)

A process for producing the vulcanizable mixture according to claim 21, the process comprising mixing together the nitrile rubber, the at least one crosslinker no, one or more further additive(s).

### Claim 25 (depends on 21, 23)

A process for producing vulcanizates, the process comprising vulcanizing a vulcanizable mixture according to claim 21 or 23.

### Claim 26 (depends on 25)

The process according to claim 25, wherein the vulcanization is performed at a temperature in the range of from 100° C. to 200° C.

### Claim 27 (depends on 25)

The process according to claim 25, wherein the vulcanization is performed at a temperature in the range of from 120° C. to 190° C.

### Claim 28 (depends on 1)

A vulcanizate based on nitrile rubbers according to claim 1.

### Claim 29 (depends on 28)

The vulcanizate according to claim 28, wherein the vulcanizate is a shaped article.

### Claim 30 (depends on 29)

The vulcanizate according to claim 29, wherein the vulcanizate is a drive belt, a roll covering, a seal, a cap, a stopper, a hose, a floor covering, a sealing mat or sheet, a profile or a membrane.