# US 2015/0105262 A1 · Magnetoelectric effect material and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0105262 A1
- Document ID: US20150105262A1
- Status: Published application
- Kind: A1
- Application number: 14/376,276
- Filed: 2012-02-03
- Published: 2015-04-16
- Earliest claimed: 2012-02-03
- Assignees: Yao Cheng
- Inventors: Yao Cheng; Ben-Li Young; Chih-Hao Lee
- Web page: https://patentgrep.com/patent/US20150105262A1

## CPC

- H01F 1/0009: {Antiferromagnetic materials, i.e. materials exhibiting a Néel transition temperature (H01F1/0036 takes precedence)}
- C22B 34/24: Obtaining niobium or tantalum
- C22C 27/02: Alloys based on vanadium, niobium, or tantalum
- H01F 41/00: Apparatus or processes specially adapted for manufacturing or assembling magnets, inductances or transformers; Apparatus or processes specially adapted for manufacturing materials characterised by their magnetic properties
- H10N 60/0156: {of devices comprising Nb or an alloy of Nb with one or more of the elements of group IVB, e.g. titanium, zirconium or hafnium}
- H10N 60/85: Superconducting active materials
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR

## Abstract

The invention provides the Magnetoelectric Effect Material consisted of a single isotope, the alloy of isotopes, or the compound of isotopes. The invention applies enrichment and purification to increase the isotope abundance, to create the density of nuclear exciton by irradiation, and therefore increase the magnetoelectric effect of the crystal of single isotope, the alloy crystal of isotopes and the compound crystal of isotopes. The invention provides the manufacturing method including the selection rules of isotopes, the fabrication processes and the structure of composite materials. The invention belongs to the area of the nuclear science and the improvement of material character. The invention using the transition of entangled multiple photons to achieve the delocalized nuclear exciton. The mix of selected isotopes adjusts the decay lifetime of nuclear exciton and the irradiation efficiency to generate the nuclear exciton.

## Claims

### Claim 1

A magnetoelectric material, wherein the said material is made by isotope crystals, isotope alloy crystals or the compound crystals of particular isotope, which is enriched and/or purified to increase the purity of the said isotope, such that the crystal of the isotope, of the alloy isotopes, or of the chemical compound of isotopes to achieve the delocalized nuclear exciton for the magnetoelectric effects.

### Claim 2 (depends on 1)

The magnetoelectric material of claim 1, wherein the enrichment of isotope in the magnetoelectric material applies the centrifugal process.

### Claim 3 (depends on 1)

The magnetoelectric material of claim 1, wherein the purification of isotope in the magnetoelectric material applies the floating zone method to drive the impurities from inside to the edge of a sample by moving the local melting zone.

### Claim 4 (depends on 1)

The magnetoelectric material of claim 1, wherein the isotope to generate the delocalized nuclear exciton in the magnetoelectric material has the transition from the first low-lying excited state to the ground state containing the quantum number change of angular momentum unequal to 1, i.e. greater than 2 or equal to 0.

### Claim 5 (depends on 1)

The magnetoelectric material of claim 1, wherein the abundance of each isotope in the isotope crystal or the isotope-compound crystal of the magnetoelectric material is 90%-100%.

### Claim 6 (depends on 5)

The magnetoelectric material of claim 5, wherein the abundance of each isotope in the isotope crystal or the isotope-compound crystal of the magnetoelectric material is 99%-100%.

### Claim 7 (depends on 1)

The magnetoelectric material of claim 1, wherein the oxygen isotope in the oxide compound crystal of the magnetoelectric material is 16O, the abundance of which is 99.76%-100%.

### Claim 8 (depends on 1)

The magnetoelectric material of claim 1, wherein the carbon isotope in the carbide compound crystal of the magnetoelectric material is 12C, the abundance of which is 98.89%-100%.

### Claim 9 (depends on 1)

The magnetoelectric material of claim 1, wherein the sulfur isotope in the sulfide compound crystal of the magnetoelectric material is 32S, the abundance of which is 95.02%-100%.

### Claim 10 (depends on 1)

The magnetoelectric material of claim 1, wherein the isotopes in the crystal of the magnetoelectric material, are selected from 12C, 16O, 19F, 27Al, 28Si, 32Si, 32S, 40Ca, 45Ca, 45Sc, 52Cr, 56Fe, 59Co, 89Y, 93Nb, 103Rh, 115In, 232Th and/or 238U.

### Claim 11

A manufacturing process of the magnetoelectric material, comprising the step to generate the nuclear exciton in the magnetoelectric material consisting of a single isotope, multiple isotopes or an isotope compound.

### Claim 12 (depends on 11)

The manufacturing process of claim 11, wherein the manufacturing means to generate the nuclear exciton in the magnetoelectric material include irradiation by the radiation sources, radioactive nuclides, and natural sources.

### Claim 13 (depends on 12)

The manufacturing process of claim 12, wherein the radiation sources in the manufacturing processes include the electron beam, x-rays, neutron, or proton, the radiation energy of which is greater than the energy of nuclear exciton.

### Claim 14 (depends on 12)

The manufacturing process of claim 12, wherein the internal irradiation by the radioactive nuclides in the manufacturing processes implants the particular radioactive nuclides into the crystal consisting of a single isotope, multiple isotopes, or the isotope compound; the long-lived radioactive isotope contain the multipolar gamma transition via entangled multiple photons.

### Claim 15 (depends on 14)

The manufacturing process of claim 14, wherein the radioactive nuclides are selected from 178mHf, 93mNb, or 113mCd.

### Claim 16 (depends on 12)

The manufacturing process of claim 12, wherein the natural methods are the excitation by the vacuum fluctuation or background radiation.

### Claim 17 (depends on 11)

The manufacturing process of claim 11, further comprising the step of the enrichment or/and the purification of isotope for the crystal of one isotope, multiple isotopes or isotope compound before the creation of nuclear exciton.

### Claim 18 (depends on 14)

The manufacturing process of claim 14, wherein the insert or removal or certain isotope impurities can adjust the decay lifetime of nuclear exciton.

### Claim 19 (depends on 11)

The manufacturing process of claim 11, wherein the abundance of isotope in the isotope crystal or compound crystal is 90%-100%.

### Claim 20 (depends on 19)

The manufacturing process of claim 19, wherein the abundance of isotope in the isotope crystal or in each element of compound crystal is 99%-100%.

### Claim 21 (depends on 11)

The manufacturing process of claim 11, wherein the isotope compound is oxide, the oxygen isotope of which is 16O with abundance of 99.76%-100%.

### Claim 22 (depends on 11)

The manufacturing process of claim 11, wherein the isotope compound is carbide, the carbon isotope of which is 12C with abundance of 98.89%-100%.

### Claim 23 (depends on 11)

The manufacturing process of claim 11, wherein the isotope compound is sulfide, the sulfur isotope of which is 32S with abundance of 95.02%-100%.

### Claim 24 (depends on 11)

The manufacturing process of claim 11, wherein the isotopes are selected from 12C, 16O, 19F, 27Al, 28Si, 32Si, 32S, 40Ca, 45Ca, 45Sc, 52Cr, 56Fe, 59Co, 89Y, 93Nb, 103Rh, 115In, 232Th and/or 238U.

### Claim 25

A method to manufacture the Magnetoelectric Effect Material, comprising:
irradiation by the radiation sources to generate the metastable nuclear excitation;
manufacturing the irradiated isotopes to be the crystal of single isotope or multiple isotopes or the isotope compound;
wherein the radiation sources are electron, x-rays, neutron, or proton, the energy of which is higher than the energy of nuclear exciton.

### Claim 26 (depends on 25)

The method of claim 25, further comprising mixing the excitation of metastable state into the incubating materials before the irradiation to form alloy or compound crystals; the said incubating materials are those isotopes have the quantum change of angular momentum for the transition from the first low-lying state to the ground state not equal to 1, i.e. >2 or =0.

### Claim 27 (depends on 25)

The method of claim 25, further comprising the step of the crystal of a single isotope, multiple isotopes, or the isotope compound being fabricated into crystal of particular size, of different dimensionality, of different topological structure to achieve different magnetoelectric effect.

### Claim 28 (depends on 27)

The method of claim 27, wherein the particular size of the crystal means two dimensional layer with a thickness about the size of nuclear exciton, and with the length and the width to be much greater than the size of nuclear exciton.

### Claim 29 (depends on 27)

The method of claim 27, wherein the said particular size of the crystal means one dimensional line with a diameter about the size of nuclear exciton, and with the length to be much greater than the size of nuclear exciton.

### Claim 30 (depends on 27)

The method of claim 27, wherein the said particular size of the crystal means two dimensional tube with a thickness about the size of nuclear exciton, and with the length and diameter to be much greater than the size of nuclear exciton.

### Claim 31 (depends on 27)

The method of claim 27, wherein the said particular size of the crystal means one dimensional circle with a diameter about the size of nuclear exciton, and with the circumference to be much greater than the size of nuclear exciton.

### Claim 32 (depends on 27)

The method of claim 27, wherein the said composition of different dimensionality and topological structures means the interface between different three-dimensional materials, multilayer of different materials, and the junction between different materials of one-dimensional rods.

### Claim 33 (depends on 32)

The method of claim 32, wherein the said composite structure of different materials include dielectric, magnetic, magnetoelectric, multiferroics to provide the required electric field and/or magnetic field.

### Claim 34 (depends on 32)

The method of claim 32, wherein the said composite structure of different materials has different magnetoelectric effects at different temperature.

### Claim 35 (depends on 32)

The method of claim 32, wherein the composite structure of different materials includes two superconductors, which have different magnetic flux quanta.

### Claim 36 (depends on 32)

The method of claim 32, wherein the composite structure of different materials includes the photoelectric material and the magnetoelectric material.

### Claim 37 (depends on 32)

The method of claim 32, wherein the composite structure of different materials includes the piezoelectric material and the magnetoelectric material.

### Claim 38 (depends on 32)

The method of claim 32, wherein the composite structure of different materials includes the semiconductor material and the magnetoelectric material.

### Claim 39 (depends on 32)

The method of claim 32, wherein the composite structure of different materials includes the material of the topological insulator and the magnetoelectric material.

### Claim 40 (depends on 32)

The method of claim 32, wherein the composite structure of different materials includes the metallic material and the magnetoelectric material.