# US 2015/0105235 A1 · Photocatalyst, preparation method thereof, and photocatalyst apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0105235 A1
- Document ID: US20150105235A1
- Status: Published application
- Kind: A1
- Application number: 14/401,064
- Filed: 2012-12-28
- Published: 2015-04-16
- Earliest claimed: 2012-05-25
- Assignees: LG Hausys, Ltd.
- Applicants: LG Hausys, Ltd.
- Inventors: Dong Il Lee; Seong Moon Jung; Joo-Hwan Seo; Ju-Hyung Lee
- Web page: https://patentgrep.com/patent/US20150105235A1

## CPC

- B01J 23/42: Platinum
- B01J 35/39: Photocatalytic properties
- B01J 35/393: {Metal or metal oxide crystallite size}
- B01J 35/45: Nanoparticles
- B01J 37/0215: {Coating}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- C01G 1/02: Oxides
- C01G 19/02: Oxides
- C01G 23/047: Titanium dioxide
- C01G 33/00: Compounds of niobium
- C01G 41/02: Oxides; Hydroxides
- B01J 21/063: {Titanium; Oxides or hydroxides thereof}
- B01J 23/40: of the platinum group metals
- B01J 23/48: Silver or gold
- B01J 23/72: Copper
- B01J 35/647: {2-50 nm}
- B01J 37/033: {Using Hydrolysis}
- B01J 37/345: {of ultraviolet wave energy}
- B01J 2235/30: Scanning electron microscopy; Transmission electron microscopy
- C01P 2004/64: Nanometer sized, i.e. from 1-100 nanometer
- C01P 2004/84: one phase coated with the other
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

Provided are: a photocatalyst comprising a porous first metal oxide film having pores, and a second metal particle or a second metal oxide particle formed inside the pores; a method for preparing the photocatalyst; and a photocatalyst apparatus using the photocatalyst.

## Claims

### Claim 1

A photocatalyst comprising:
a first porous metal oxide film comprising pores; and
a second metal particle or a second metal oxide particle formed inside the pores.

### Claim 2 (depends on 1)

The photocatalyst according to claim 1, wherein the photocatalyst is activated by visible light of a wavelength from 380 nm to 780 nm.

### Claim 3 (depends on 1)

The photocatalyst according to claim 1, wherein the first metal oxide film comprises first metal oxide particles having an average diameter from 20 nm to 100 nm.

### Claim 4 (depends on 1)

The photocatalyst according to claim 1, wherein the second metal particles and the second metal oxide particles each have an average diameter from about 1 nm to about 10 nm.

### Claim 5 (depends on 1)

The photocatalyst according to claim 1, wherein the first porous metal oxide film has a thickness from 30 nm to 100 nm.

### Claim 6 (depends on 1)

The photocatalyst according to claim 1, wherein the first metal oxide comprised in the first metal oxide film comprises at least one selected from among titanium oxide, tungsten oxide, zinc oxide, niobium oxide, and combinations thereof.

### Claim 7 (depends on 1)

The photocatalyst according to claim 1, wherein the second metal of the second metal particles and the second metal oxide particles comprises at least one selected from among tungsten, chromium, vanadium, molybdenum, copper, iron, cobalt, manganese, nickel, platinum, gold, cerium, cadmium, zinc, magnesium, calcium, strontium, barium, radium, and combinations thereof.

### Claim 8 (depends on 1)

The photocatalyst according to claim 1, wherein a weight ratio of the first porous metal oxide film to the sum total of the second metal particles and the second metal oxide particles is 0.1:99.9 to 1:99 in the photocatalyst.

### Claim 9

A method for preparing a photocatalyst, comprising:
forming a first porous metal oxide film;
dipping the first metal oxide film into a precursor solution of a second metal, followed by allowing the precursor solution of the second metal to permeate inner pores of the first porous metal oxide film; and
forming particles of the second metal in the inner pores of the first porous metal oxide film by reduction of the second metal through light irradiation to the first porous metal oxide film containing the precursor solution of the second metal in the inner pores thereof.

### Claim 10 (depends on 9)

The method according to claim 9, wherein light irradiation is UV irradiation.

### Claim 11 (depends on 9)

The method according to claim 9, wherein the first metal oxide film is formed on a substrate by a sol-gel method using a first metal oxide precursor, or by coating a slurry comprising first metal oxide powder, a binder and a solvent onto the substrate.

### Claim 12 (depends on 9)

The method according to claim 9, further comprising:
performing heat treatment to impart crystallinity to the first metal oxide film or to remove a binder from the first metal oxide film, after the first metal oxide film is formed by a sol-gel method using a first metal oxide precursor or by coating of a slurry comprising first metal oxide powder, the binder and a solvent.

### Claim 13 (depends on 12)

The method according to claim 12, wherein heat treatment is performed at a heating speed from 1° C./min to 2° C./min.

### Claim 14 (depends on 9)

The method according to claim 9, further comprising:
creating a second metal oxide through oxidation of at least a portion of the second metal particles by heat treatment of the first porous metal oxide film containing the second metal particles formed inside the pores thereof.

### Claim 15 (depends on 14)

The method according to claim 14, wherein heat treatment is performed at a heating speed from 1° C./min to 2° C./min.

### Claim 16 (depends on 1)

A photocatalytic apparatus comprising the photocatalyst according to claim 1.

### Claim 17 (depends on 16)

The photocatalytic apparatus according to claim 16, wherein the photocatalytic apparatus is used for purposes of air cleaning, deodorization or antimicrobial effects.