# US 2015/0104953 A1 · High uv curing efficiency for low-k dielectrics

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0104953 A1
- Document ID: US20150104953A1
- Status: Published application
- Kind: A1
- Application number: 14/053,727
- Filed: 2013-10-15
- Published: 2015-04-16
- Earliest claimed: 2013-10-15
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Po-Cheng Shih; Hui-Chun Yang; Chung-Chi Ko; Kuang-Yuan Hsu
- Web page: https://patentgrep.com/patent/US20150104953A1

## CPC

- H10P 14/6328: {Deposition from the gas or vapour phase}
- H10P 14/6536: {by exposure to radiation, e.g. visible light}
- H10P 14/6538: {by exposure to UV light}
- H10P 14/665: {Porous materials}
- H10P 14/6682: {the compound being a silane, e.g. disilane, methylsilane or chlorosilane}
- H10P 72/0436: {mainly by radiation}
- H10P 72/7621: {characterised by supporting two or more semiconductor substrates}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

One embodiment is a method for semiconductor processing. In this method, a precursor film is provided over a semiconductor substrate, where the precursor film is made of a structural former and porogen. Prior to cross-linking, the porogen is removed by exposure to UV radiation having one or more wavelengths in the range of 150 nm to 300 nm, while a temperature of 300° C. to 500° C. is applied to the semiconductor substrate. Meanwhile, a Argon:Helium flow rate of 80>Ar>10 slm, 80>He>10 slm is set for the ambient substrate environment where the ratio of Ar:He ranges from 0:1 to 1:0 by volume or molality.

## Claims

### Claim 1

A multi-station tool for semiconductor processing and formation of an extreme low-k dielectric, comprising:
a first station where porogen is removed from a precursor film by exposing the precursor film to ultraviolet (UV) radiation while a substrate on which the precursor film is disposed is kept at a temperature of between 300° C. and 500° C. while an Argon gas flow is set to between 10 slm and 80 slm or while a helium gas flow is set to between 10 slm and 80 slm.

### Claim 2 (depends on 1)

The multi-station tool of claim 1, wherein a ratio of argon gas to helium gas (Ar:He) in the flow is set to between (1:0) and (0:1) while the porogen is being removed.

### Claim 3 (depends on 1)

The multi-station tool of claim 1, further comprising:
a second station: where porogen further is removed from the precursor film by exposing the precursor film to ultraviolet (UV) radiation while the substrate on which the precursor film is disposed is kept at a temperature of between 300° C. and 500° C. while an Argon gas flow is set to between 10 slm and 80 slm or while a helium gas flow is set to between 10 slm and 80 slm.

### Claim 4 (depends on 1)

The multi-station tool of claim 1, where the UV radiation has one or more wavelengths between 150 nm and 300 nm.

### Claim 5 (depends on 3)

The multi-station tool of claim 3, further comprising:
a third station on which the substrate is processed prior to the first and second stations, where structural former in the precursor film is cross-linked at the third station by applying infra-red (IR) radiation having one or more wavelengths of between 500 nm and 700 nm to the precursor film.

### Claim 6 (depends on 5)

The multi-station tool of claim 5, a temperature of approximately 385° C. is applied while the substrate is at the third station during cross-linking.

### Claim 7 (depends on 6)

The multi-station tool of claim 6, wherein during the cross-linking, an Argon gas flow is set to between 10 slm and 80 slm or while a helium gas flow is set to between 10 slm and 80 slm.

### Claim 8 (depends on 5)

The multi-station tool of claim 5, further comprising:
a fourth station on which the substrate is processed prior to the first and second stations and after the third station, where the structural former in the precursor film is further cross-linked at the fourth station by applying infra-red (IR) radiation having one or more wavelengths of between 500 nm and 700 nm to the precursor film at a temperature of approximately 385° C.

### Claim 9

A multi-station tool for semiconductor processing and formation of an extreme low-k dielectric, comprising:
a first station: where structural former in a precursor film is cross-linked by applying infra-red (IR) radiation having one or more wavelengths of between 500 nm and 700 nm to the precursor film while a substrate on which the precursor film is disposed is kept at a temperature of approximately 385° C.; and
a second station where porogen is removed from the precursor film by exposing the precursor film to ultraviolet (UV) radiation while the substrate is kept at a temperature of approximately 300° C. while an Argon gas flow is set to between 10 slm and 80 slm or while a helium gas flow is set to between 10 slm and 80 slm.

### Claim 10 (depends on 9)

The multi-station tool of claim 9, wherein the first and second station share a common chamber.

### Claim 11 (depends on 9)

The multi-station tool of claim 9, wherein the first and second stations have separate chambers that are hermetically isolated from one another during processing.

### Claim 12 (depends on 9)

The multi-station tool of claim 9, further comprising:
a third station: where the porogen is further removed from the precursor film by exposing the precursor film to UV radiation at the third station while the substrate on which the precursor film is disposed is kept at a temperature of approximately 385° C.

### Claim 13 (depends on 12)

The multi-station tool of claim 12, wherein an Argon gas flow is set to between 10 slm and 80 slm or where a helium gas flow is set to between 10 slm and 80 slm during processing on the first and third stations.

### Claim 14 (depends on 12)

The multi-station tool of claim 12, further comprising:
a fourth station: where the porogen further is removed from the precursor film by exposing the precursor film to UV radiation at the fourth station while the substrate on which the precursor film is disposed is kept at a temperature of approximately 385° C.

### Claim 15

A method for semiconductor processing, comprising:
providing an etch stop layer over a semiconductor substrate;
providing a tetraethyl orthosilicate (TEOS) layer over the etch stop layer;
providing a precursor film over the TEOS layer, wherein the precursor film includes a structural former and porogen;
removing the porogen from the precursor film in a chamber by exposing the precursor film to ultraviolet (UV) radiation having a wavelength of between 150 nm and 300 nm while an Argon flow of between 10 slm and 80 slm or a Helium flow of between 10 slm and 80 slm is supplied to the chamber.

### Claim 16 (depends on 15)

The method of claim 15, wherein the UV radiation has a wavelength of between 150 nm and 200 nm.

### Claim 17 (depends on 15)

The method of claim 15, wherein the semiconductor substrate is heated to a temperature of approximately 300° C. while the precursor film is exposed to the UV light.

### Claim 18 (depends on 15)

The method of claim 15, further comprising:
cross-linking the structural former in the precursor film by applying infra-red (IR) radiation having one or more wavelengths of between 500 nm and 700 nm to the precursor film.

### Claim 19 (depends on 18)

The method of claim 18, wherein the IR radiation is applied while the semiconductor substrate is heated to a temperature of approximately 385° C.

### Claim 20 (depends on 18)

The method of claim 18, wherein the IR radiation is applied while an Argon flow of between 10 slm and 80 slm or a Helium flow of between 10 slm and 80 slm is supplied to the chamber.