# US 2015/0104952 A1 · Method and composition for selectively removing metal hardmask and other residues from semiconductor device substrates comprising low-k dielectric material and copper

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0104952 A1
- Document ID: US20150104952A1
- Status: Published application
- Kind: A1
- Application number: 14/103,303
- Filed: 2013-12-11
- Published: 2015-04-16
- Earliest claimed: 2013-10-11
- Assignees: EKC Technology, Inc.
- Applicants: EKC Technology, Inc.
- Inventors: Hua Cui
- Web page: https://patentgrep.com/patent/US20150104952A1

## CPC

- H10P 50/283: {by chemical means}
- B08B 3/08: the liquid having chemical or dissolving effect
- B08B 3/10: with additional treatment of the liquid or of the object being cleaned, e.g. by heat, by electricity or by vibration
- C11D 3/2082: {Polycarboxylic acids-salts thereof}
- C11D 3/3942: {Inorganic per-compounds (C11D3/3902 takes precedence)}
- C11D 3/3947: {Liquid compositions}
- C11D 7/04: Water-soluble compounds
- C11D 7/265: {Carboxylic acids or salts thereof}
- C11D 7/3209: {Amines or imines with one to four nitrogen atoms; Quaternized amines}
- C11D 7/3218: {Alkanolamines or alkanolimines}
- C11D 7/3245: {Aminoacids}
- C11D 7/3281: {Heterocyclic compounds}
- C23F 1/18: for etching copper or alloys thereof
- C23F 1/26: for etching refractory metals
- C23F 1/28: for etching iron group metals
- C23F 1/34: for etching copper or alloys thereof
- C23F 1/38: for etching refractory metals
- C23F 1/40: for etching other metallic material
- G03F 7/423: {containing mineral acids or salts thereof, containing mineral oxidizing substances, e.g. peroxy compounds}
- G03F 7/425: {containing mineral alkaline compounds; containing organic basic compounds, e.g. quaternary ammonium compounds; containing heterocyclic basic compounds containing nitrogen}
- G03F 7/426: {containing organic halogen compounds; containing organic sulfonic acids or salts thereof; containing sulfoxides}
- H10P 50/667: {by liquid etching only}
- H10P 70/20: {Cleaning during device manufacture}
- H10P 70/234: {the processing being the formation of vias or contact holes}
- H10W 20/081: {by forming openings in the dielectric parts}
- H10W 20/084: {for dual-damascene structures}
- C11D 2111/22: Electronic devices, e.g. PCBs or semiconductors
- H10P 50/73: {using masks for insulating materials}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- B08B: CLEANING IN GENERAL; PREVENTION OF FOULING IN GENERAL
- C11D: DETERGENT COMPOSITIONS; USE OF SINGLE SUBSTANCES AS DETERGENTS; SOAP OR SOAP-MAKING; RESIN SOAPS; RECOVERY OF GLYCEROL
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

An aqueous removal composition having a pH in the range of from 2 to 14 and method for selectively removing an etching mask consisting essentially of TiN, TaN, TiNxOy, TiW, W, or alloy of Ti or W relative to low-k materials from a semiconductor substrate comprising said low-k materials having a TiN, TaN, TiNxOy, TiW, W, or alloy of Ti or W etching mask thereon wherein the removal composition comprises at least one oxidizing agent and a carboxylate compound.

## Claims

### Claim 1

A removal composition having a pH in the range of from 2 to 14 for selectively removing an etching mask consisting essentially of TiN, TaN, TiNxOy, TiW, W, and alloys of Ti and W relative to low-k dielectric material from a semiconductor device substrate which comprises said low-k dielectric material having a TiN, TaN, TiNxOy, TiW, W, or alloy of Ti or W etching mask thereon, wherein said removal composition comprises:
(a) from 0.1 wt % to 90 wt % of an oxidizing agent;
(b) from 0.0001 wt % to 50 wt % of an ammonium carboxylate; and
(c) the balance up to 100 wt % of said removal composition comprising deionized water.

### Claim 2 (depends on 1)

The removal composition of claim 1 further comprising an organic cosolvent that is miscible with water.

### Claim 3 (depends on 1, 2)

The removal composition of claim 1 or claim 2 wherein (a) said oxidizing agent is selected from the group consisting essentially of hydrogen peroxide (H2O2), n-methylmorpholine oxide (NMMO or NMO), benzoyl peroxide, tetrabutylammonium peroxymonosulfate, ozone, ferric chloride, permanganate peroxoborate, perchlorate, persulfate, ammonium peroxydisulfate, per acetic acid, urea hydroperoxide, nitric acid (HNO3), ammonium chlorite (NH4ClO2), ammonium chlorate (NH4ClO3), ammonium iodate (NH4IO3), ammonium perborate (NH4BO3), ammonium perchlorate (NH4ClO4), ammonium periodate (NH4IO3), ammonium persulfate ((NH4)2S2O8), tetramethylammonium chlorite ((N(CH3)4)ClO2), tetramethylammionium chlorate ((N(CH3)4)ClO3), tetramethylammonium iodate ((N(CH3)4)IO3), tetramethylammonium perborate ((N(CH3)4)BO3), tetramethylammonium perchlorate ((N(CH3)4)ClO4), tetramethylammonium periodate ((N(CH3)4)IO4), tetramethylammonium persulfate ((N(CH3)4)S2O8), ((CO(NH2)2)H2O2), peracetic acid (CH3(CO)OOH), and mixtures thereof; and
(b) said ammonium carboxylate is selected from the group comprising ammonium oxalate, ammonium lactate, ammonium tartrate, ammonium citrate tribasic, ammonium acetate, ammonium carbamate, ammonium carbonate, ammonium benzoate, tetraammonium EDTA, ethylenediaminetetraacetic acid diammonium salt, ammonium succinate, ammonium formate, ammonium 1-H-pyrazole-3-carboxylate, and mixtures thereof.

### Claim 4 (depends on 3)

The removal composition of claim 3 wherein said oxidizing agent is hydrogen peroxide.

### Claim 5 (depends on 1)

The removal composition of claim 1 further comprising from 0.001 wt % to 20 wt % of an amino acid, an aminopolycarboxylic acid, a polycarboxylic acid, or a mixture thereof selected from the group consisting essentially of 1,2-cyclohexanediamine-N,N,N′,N′-tetraacetic acid; ethylenediaminetetraacetic acid; nitrilotriacetic acid; diethylene triamine pentaacetic acid; 1,4,7,10-tetraazacyclododecane-1,4,7,10-tetraacetic acid; ethylene glycol tetraacetic acid (EGTA); 1,2-bis(o-aminophenoxy)ethane-N,N,N′,N′-tetraacetic acid; N-{2-[bis(carboxymethyl)amino]ethyl}-N-(2-hydroxyethyl)glycine (HEDTA); and ethylenediamine-N,N′-bis(2-hydroxyphenylacetic acid) (EDDHA).

### Claim 6 (depends on 1)

The removal composition of claim 1 further comprising from 0.0001 wt % up to 50 wt % of a metal corrosion inhibitor.

### Claim 7 (depends on 1)

The removal composition of claim 1 wherein the pH is in the range of from 3 to 13 and said oxidizing agent is hydrogen peroxide.

### Claim 8 (depends on 7)

The removal composition of claim 7 wherein the pH is in the range of from 7 to 12.

### Claim 9

A method for selectively removing an etching mask consisting essentially of TiN, TaN, TiNxOy, TiW, W, or an alloy of Ti or W relative to low-k materials from a semiconductor substrate comprising said low-k materials having an etching mask consisting essentially of TiN, TaN, TiNxOy, TiW, W, or an alloy of Ti or W thereon wherein the method comprises contacting the substrate with a removal composition comprising:
(a) from 0.1 wt % to 90 wt % at least one oxidizing agent,
(b) from 0.0001 wt % to 50 wt % of an ammonium carboxylate; and
(c) the balance up to 100 wt % of said removal composition comprising deionized water at a temperature in the range of from room temperature up to 80° C. and at a pH in the range of from 3 to 13 for a time wherein said removal composition selectively removes said TiN, TaN, TiNxOy, TiW, W, or alloy of Ti or W etching mask relative to said low-k materials, and the achievable etch rate of the composition remains substantially constant over an extended period of time.

### Claim 10 (depends on 9)

The method of claim 9 wherein:
(a) said oxidizing agent is selected from the group consisting essentially of hydrogen peroxide (H2O2), n-methylmorpholine oxide (NMMO or NMO), benzoyl peroxide, tetrabutylammonium peroxymonosulfate, ozone, ferric chloride, permanganate peroxoborate, perchlorate, persulfate, ammonium peroxydisulfate, per acetic acid, urea hydroperoxide, nitric acid (HNO3), ammonium chlorite (NH4ClO2), ammonium chlorate (NH4ClO3), ammonium iodate (NH4IO3), ammonium perborate (NH4BO3), ammonium perchlorate (NH4ClO4), ammonium periodate (NH4IO3), ammonium persulfate ((NH4)2S2O8), tetramethylammonium chlorite ((N(CH3)4)ClO2), tetramethylammionium chlorate ((N(CH3)4)ClO3), tetramethylammonium iodate ((N(CH3)4)IO3), tetramethylammonium perborate ((N(CH3)4)BO3), tetramethylammonium perchlorate ((N(CH3)4)ClO4), tetramethylammonium periodate ((N(CH3)4)IO4), tetramethylammonium persulfate ((N(CH3)4)S2O8), ((CO(NH2)2)H2O2), peracetic acid (CH3(CO)OOH), and mixtures thereof; and
(b) said ammonium carboxylate is selected from the group comprising ammonium oxalate, ammonium lactate, ammonium tartrate, ammonium citrate tribasic, ammonium acetate, ammonium carbamate, ammonium carbonate, ammonium benzoate, tetraammonium EDTA, ethylenediaminetetraacetic acid diammonium salt, ammonium succinate, ammonium formate, ammonium 1-H-pyrazole-3-carboxylate, and mixtures thereof.

### Claim 11 (depends on 10)

The method of claim 10 wherein said removal composition further comprises from 0.0001 wt % up to 20 wt % of a copper corrosion inhibitor.

### Claim 12 (depends on 10)

The method of claim 10 wherein said removal composition further comprises from 0.001 wt % to 20 wt % of an amino acid, an aminopolycarboxylic acid, a carboxylic acid, a polycarboxylic acid, or a mixture thereof selected from the group consisting essentially of 1,2-cyclohexanediamine-N,N,N′,N′-tetraacetic acid; ethylenediaminetetraacetic acid; nitrilotriacetic acid; diethylene triamine pentaacetic acid; 1,4,7,10-tetraazacyclododecane-1,4,7,10-tetraacetic acid; ethylene glycol tetraacetic acid (EGTA); 1,2-bis(o-aminophenoxy)ethane-N,N,N′,N′-tetraacetic acid; N-{2-[bis(carboxymethyl)amino]ethyl}-N-(2-hydroxyethyl)glycine (HEDTA); and ethylenediamine-N,N′-bis(2-hydroxyphenylacetic acid) (EDDHA) whereby the achievable removal rate for the etching mask remains substantially constant over an extended period of time up to at least thirty five hours.

### Claim 13

A method for selectively removing an etching mask consisting essentially of TiN, TaN, TiNxOy, TiW, W, or an alloy of Ti or W relative to low-k materials from a semiconductor substrate comprising said low-k materials having an etching mask consisting essentially of TiN, TaN, TiNxOy, TiW, W, or an alloy of Ti or W thereon wherein the method comprises contacting the substrate with a removal composition comprising:
(a) from 0.1 wt % to 90 wt % of hydrogen peroxide;
(b) from 0.0001 wt % to 50 wt % of an ammonium carboxylate selected from the group comprising ammonium oxalate, ammonium lactate, ammonium tartrate, ammonium citrate tribasic, ammonium acetate, ammonium carbamate, ammonium carbonate, ammonium benzoate, tetraammonium EDTA, ethylenediaminetetraacetic acid diammonium salt, ammonium succinate, ammonium formate, ammonium 1-H-pyrazole-3-carboxylate, and mixtures thereof;
(c) from 0.001 wt % to 20 wt % of an amino acid, an aminopolycarboxylic acid, a carboxylic acid, a polycarboxylic acid, or a mixture thereof selected from the group consisting essentially of 1,2-cyclohexanediamine-N,N,N′,N′-tetraacetic acid; ethylenediaminetetraacetic acid; nitrilotriacetic acid; diethylene triamine pentaacetic acid; 1,4,7,10-tetraazacyclododecane-1,4,7,10-tetraacetic acid; ethylene glycol tetraacetic acid (EGTA); and 1,2-bis(o-aminophenoxy)ethane-N,N,N′,N′-tetraacetic acid; N-{2-[bis(carboxymethyl)amino]ethyl}-N-(2-hydroxyethyl)glycine (HEDTA); and ethylenediamine-N,N′-bis(2-hydroxyphenylacetic acid) (EDDHA); and
(d) the balance up to 100 wt % of said removal composition comprising deionized water at a temperature in the range of from room temperature up to 80° C. and at a pH in the range of from 3 to 13 for a time wherein said removal composition selectively removes said TiN, TaN, TiNxOy, TiW, W, or alloy of Ti or W etching mask relative to said low-k materials whereby the etching mask is selectively removed and the achievable removal rate for the etching mask remains substantially constant over an extended period of time.