# US 2015/0104947 A1 · Methods of forming semiconductor devices using hard masks

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0104947 A1
- Document ID: US20150104947A1
- Status: Published application
- Kind: A1
- Application number: 14/510,331
- Filed: 2014-10-09
- Published: 2015-04-16
- Earliest claimed: 2013-10-10
- Assignees: Samsung Electronics Co., Ltd.
- Applicants: Samsung Electronics Co., Ltd.
- Inventors: Dongchan Kim; Gyungjin Min; Minjoon Park; Seunghoon Park; KeunHee Bai; Kisoo Chang
- Web page: https://patentgrep.com/patent/US20150104947A1

## CPC

- H10P 50/283: {by chemical means}
- H10D 30/0227: {having both lightly-doped source and drain extensions and source and drain regions self-aligned to the sides of the gate, e.g. lightly-doped drain [LDD] MOSFET or double-diffused drain [DDD] MOSFET}
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10P 50/285: {of materials not containing Si, e.g. PZT or Al2O3}
- H10P 50/287: {by chemical means}
- H10P 50/71: {using masks for conductive or resistive materials}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

Methods of forming a semiconductor device are provided. The methods may include forming an insulating layer including silicon on a substrate and sequentially forming a first hard mask layer and a second hard mask layer on the substrate. The first hard mask layer may include carbon, and the second hard mask layer may include carbon and impurities. The first and second hard mask layers may expose at least a portion of the insulating layer. The methods may also include performing an etching process to selectively remove the second hard mask layer with respect to the insulating layer. A ratio of etch rates between the second hard mask layer and the insulating layer during the etching process may be in a range of about 100:1 to about 10,000:1.

## Claims

### Claim 1

A method for manufacturing a semiconductor device, the method comprising:
forming a first pattern and a second pattern on a substrate;
forming a first hard mask layer and a second hard mask layer on the first pattern;
performing a first process on the second pattern that is exposed by the first and second hard mask layers; and
removing the second hard mask layer by an etching process,
wherein a ratio of etch rates between the second hard mask layer and the second pattern during the etching process is in a range of about 100:1 to about 10,000:1.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first hard mask layer includes a carbon containing layer formed by a spin coating method.

### Claim 3 (depends on 2)

The method of claim 2, wherein the second hard mask layer includes a carbon containing layer doped with impurities, and the first hard mask layer is disposed between the substrate and the second hard mask layer.

### Claim 4 (depends on 3)

The method of claim 3, wherein the impurities include boron, gallium, phosphorus and/or arsenic.

### Claim 5 (depends on 3)

The method of claim 3, wherein the second hard mask layer is an amorphous carbon layer formed by a chemical vapor deposition (CVD) process or an atomic layer deposition (ALD) process.

### Claim 6 (depends on 1)

The method of claim 1, wherein the etching process is a wet etching process using an etching solution that includes sulfuric acid.

### Claim 7 (depends on 1)

The method of claim 1, wherein the second pattern comprises a spacer on the substrate, and the spacer includes silicon nitride.

### Claim 8 (depends on 1)

The method of claim 1, further comprising forming a third hard mask layer on the second hard mask layer, wherein the third hard mask layer includes a material different from the second hard mask layer.

### Claim 9 (depends on 8)

The method of claim 8, wherein the third hard mask layer includes silicon oxide.

### Claim 10 (depends on 9)

The method of claim 9, further comprising:
patterning the second hard mask layer using the third hard mask layer as an etch mask; and
removing the third hard mask layer by a wet etching process,
wherein the third hard mask layer is removed using a LAL solution, and a ratio of etch rates between the third hard mask layer and the second hard mask layer during the wet etching process is in a range of about 1:1 to about 100:1.

### Claim 11 (depends on 1)

The method of claim 1, further comprising:
removing the first hard mask layer by a wet etching process or an ashing process after removing the second hard mask layer.

### Claim 12

A method of forming a semiconductor device, the method comprising:
forming an insulating layer comprising silicon on a substrate;
sequentially forming a first hard mask layer and a second hard mask layer on the substrate, wherein:
the first hard mask layer comprises carbon,
the second hard mask layer comprises carbon and impurities, and
the first and second hard mask layers expose at least a portion of the insulating layer; and
performing an etching process to selectively remove the second hard mask layer with respect to the insulating layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein a ratio of etch rates between the second hard mask layer and the insulating layer during the etching process is in a range of about 100:1 to about 10,000:1.

### Claim 14 (depends on 13)

The method of claim 13, wherein the impurities in the second hard mask layer comprise boron, gallium, phosphorus and/or arsenic.

### Claim 15 (depends on 14)

The method of claim 14, wherein the second hard mask layer is an amorphous carbon layer formed by a chemical vapor deposition (CVD) process or an atomic layer deposition (ALD) process.

### Claim 16 (depends on 15)

The method of claim 15, wherein performing the etching process comprises performing a wet etching process using an etchant comprising sulfuric acid.

### Claim 17 (depends on 16)

The method of claim 16, wherein the first hard mask layer is a carbon containing layer formed by a spin coating process.

### Claim 18 (depends on 17)

The method of claim 17, wherein the insulating layer is a silicon nitride layer or a silicon oxynitride layer.

### Claim 19 (depends on 18)

The method of claim 18, further comprising performing an ion implantation process using the first and second hard mask layers as an ion implantation mask.

### Claim 20 (depends on 17)

The method of claim 17, wherein the insulating layer has a substantially equivalent thickness before and after performing the etching process.