# US 2015/0104923 A1 · Mechanism of Forming a Trench Structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0104923 A1
- Document ID: US20150104923A1
- Status: Published application
- Kind: A1
- Application number: 14/092,770
- Filed: 2013-11-27
- Published: 2015-04-16
- Earliest claimed: 2013-10-10
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Chun Hsiung Tsai; Tsan-Chun Wang
- Web page: https://patentgrep.com/patent/US20150104923A1

## CPC

- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 30/6211: {having fin-shaped semiconductor bodies integral with the bulk semiconductor substrates}
- H10D 62/115: {Dielectric isolations, e.g. air gaps}
- H10D 62/60: Impurity distributions or concentrations
- H10D 84/853: {comprising FinFETs}
- H10D 86/215: {comprising FinFETs}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6516: {of treatments performed after formation of the materials}
- H10P 14/6518: {by introduction of substances into an already-existing insulating layer}
- H10P 14/6522: {introduced into a nitride material, e.g. changing SiN to SiON}
- H10P 14/6529: {by exposure to a gas or vapour}
- H10P 14/6689: {the compound being a silazane}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 30/40: into insulating materials
- H10P 32/20: Diffusion for doping of insulating layers
- H10W 10/0148: {comprising introducing impurities in side walls or bottom walls of trenches, e.g. for forming channel stoppers}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10D 30/0241: {doping of vertical sidewalls, e.g. using tilted or multi-angled implants}
- H10D 30/751: {having composition variations in the channel regions}
- H10D 62/151: {of IGFETs (of IGFETs having LDD or DDD structure H10D30/601; of thin film transistors H10D30/6713)}
- H10D 84/0158: {the components including FinFETs}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10P 14/65: {characterised by treatments performed before or after the formation of the materials}
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/21: {of electrically active species}
- H10P 30/28: characterised by an annealing step, e.g. for activation of dopants
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Embodiments of a mechanism for forming a shallow trench isolation (STI) structure filled with a flowable dielectric layer are provided. The mechanism involves using one or more low-temperature thermal anneal processes with oxygen sources and one or more microwave anneals to convert a flowable dielectric material to silicon oxide. The low-temperature thermal anneal processes with oxygen sources and the microwave anneals are performed at temperatures below the ranges that could cause significant dopant diffusion, which help dopant profile control for advanced manufacturing technologies. In some embodiments, an implant to generate passages in the upper portion of the flowable dielectric layer is also used in the mechanism.

## Claims

### Claim 1

A method of forming a semiconductor structure comprising:
depositing a flowable dielectric layer in a trench of a substrate;
performing a first thermal anneal with an oxygen source;
performing a second thermal anneal by microwave anneal (MWA); and
performing a planarization process to remove excess flowable dielectric layer outside the trench.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
performing an implant process on the flowable dielectric layer prior to performing the first thermal anneal with an oxygen source.

### Claim 3 (depends on 2)

The method of claim 2, further comprising:
performing an O3 cure after the flowable dielectric layer is deposited and before the implant process is performed.

### Claim 4 (depends on 2)

The method of claim 2, wherein the implant process implants at least one of H atoms and He atoms.

### Claim 5 (depends on 2)

The method of claim 2, wherein the implant process creates passages in the flowable dielectric layer.

### Claim 6 (depends on 1)

The method of claim 1, wherein an anneal temperature of the first thermal anneal is in a range from about 200° C. to about 400° C.

### Claim 7 (depends on 1)

The method of claim 1, wherein the oxygen source is steam or H2O2.

### Claim 8 (depends on 1)

The method of claim 1, wherein the second thermal anneal by MWA is in a range from about 400° C. to about 600° C.

### Claim 9 (depends on 1)

The method of claim 1, wherein a frequency of the second thermal anneal by MWA is performed in a range from about 2 GHz to about 10 GHz.

### Claim 10 (depends on 1)

The method of claim 1, wherein the second thermal anneal by MWA is performed in a range from about 5000 watts to about 10000 watts.

### Claim 11 (depends on 1)

The method of claim 1, wherein the second thermal anneal by MWA is performed for a duration in a range from about 30 seconds to about 1200 seconds.

### Claim 12 (depends on 1)

The method of claim 1, further comprising:
performing a third thermal anneal with an oxygen source after the planarization process; and
performing a fourth thermal anneal by microwave anneal (MWA).

### Claim 13 (depends on 2)

The method of claim 2, wherein an implant depth of the implant process is in a range from about 1000 Å to about 2500 Å.

### Claim 14 (depends on 2)

The method of claim 2, wherein an implant energy is in a range from about 6 keV to about 25 keV.

### Claim 15 (depends on 2)

The method of claim 2, wherein a ratio of an implant depth to a depth of the trench is in a range from about 1/3 to about 1/2.

### Claim 16 (depends on 1)

The method of claim 1, wherein an anneal time of the first thermal anneal is in a range from about 30 minutes to about 1 hour.

### Claim 17 (depends on 1)

The method of claim 1, wherein the as-deposited flowable dielectric layer includes a network of SiONH, and wherein the first thermal anneal and the second thermal anneal convert the as-deposited flowable dielectric layer into silicon dioxide (SiO2).

### Claim 18

A method of forming a shallow trench isolation (STI) structure in a substrate; comprising:
depositing a flowable dielectric layer in a trench of the substrate by a chemical vapor deposition (CVD) process;
curing the deposited flowable dielectric layer with an oxygen source;
performing an implant process on the flowable dielectric layer, wherein the implant process generates passages in a top portion of the flowable dielectric layer;
performing a first thermal anneal with an oxygen source;
performing a second thermal anneal by microwave anneal (MWA); and
performing a planarization process to remove excess flowable dielectric layer outside the trench.

### Claim 19 (depends on 18)

The method of claim 18, wherein an anneal temperature of the first thermal anneal is in a range from about 200° C. to about 400° C.

### Claim 20

A method of forming a shallow trench isolation (STI) structure in a substrate; comprising:
depositing a flowable dielectric layer in a trench of the substrate, wherein the trench has an aspect ratio greater than about 8;
performing an implant process on the flowable dielectric layer;
performing a first thermal anneal with an oxygen source;
performing a second thermal anneal by microwave anneal (MWA); and
performing a planarization process to remove excess flowable dielectric layer outside the trench.