# US 2015/0104893 A1 · Method of producing photo-alignment layer of liquid crystal display

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0104893 A1
- Document ID: US20150104893A1
- Status: Published application
- Kind: A1
- Application number: 14/445,241
- Filed: 2014-07-29
- Published: 2015-04-16
- Earliest claimed: 2013-10-15
- Assignees: Samsung Display Co., Ltd.
- Applicants: Samsung Display Co., Ltd.
- Inventors: Mi Hwa LEE; Suk Hoon KANG; Yeong Rong PARK; Jun-Woo LEE; Baek Kyun JEON
- Web page: https://patentgrep.com/patent/US20150104893A1

## CPC

- G02F 1/133788: {by light irradiation, e.g. linearly polarised light photo-polymerisation}
- G02F 1/133345: {Insulating layers (G02F1/1335, G02F1/1337, G02F1/135, G02F1/136 take precedence)}
- G02F 1/133707: {Structures for producing distorted electric fields, e.g. bumps, protrusions, recesses, slits in pixel electrodes}
- G02F 1/133723: {Polyimide, polyamide-imide}
- G02F 1/1368: in which the switching element is a three-electrode device {(G02F1/136277 takes precedence)}
- H10D 86/021: {of multiple TFTs}
- G02F 1/133715: {by first depositing a monomer}
- G02F 1/134372: {for fringe field switching [FFS] where the common electrode is not patterned}
- G02F 2202/025: thermocurable
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method of manufacturing a photo-alignment layer, includes: disposing a polymer material on a substrate; pre-baking the polymer material disposed on the substrate; irradiating a light to the pre-baked polymer material, to photo-align the pre-baked polymer material; and thermal-treating the irradiated pre-baked polymer material, to harden the irradiated pre-baked polymer material. The thermal-treating includes a first thermal-treatment, and a second thermal-treatment at a higher temperature than the first thermal-treatment.

## Claims

### Claim 1

A method of manufacturing a photo-alignment layer, comprising:
disposing a polymer material on a substrate;
pre-baking the polymer material disposed on the substrate;
irradiating a light to the pre-baked polymer material, to photo-align the pre-baked polymer material; and
thermal-treating the irradiated pre-baked polymer material, to harden the irradiated pre-baked polymer material,
wherein the thermal-treating comprises a first thermal-treatment, and a second thermal-treatment at a higher temperature than that of the first thermal-treatment.

### Claim 2 (depends on 1)

The method of claim 1, wherein
the polymer material comprises a main chain and a side chain.

### Claim 3 (depends on 1)

The method of claim 1, wherein
the polymer material comprises a polyimide or polyamic acid.

### Claim 4 (depends on 3)

The method of claim 3, wherein
the first thermal-treatment is performed at a temperature of about 140 degrees Celsius to about 180 degrees Celsius, and
the second thermal-treatment is performed at a temperature of about 190 degrees Celsius to about 230 degrees Celsius.

### Claim 5 (depends on 4)

The method of claim 4, wherein
the first thermal-treatment and the second thermal-treatment are performed for about 20 minutes to about 40 minutes.

### Claim 6 (depends on 4)

The method of claim 4, wherein
the first thermal-treatment stabilizes a polymer shape and increases anisotropy of the polymer material.

### Claim 7 (depends on 4)

The method of claim 4, wherein
the second thermal-treatment imidizes the polyimide or the polyamic acid of the polymer material.

### Claim 8 (depends on 1)

The method of claim 1, wherein
the pre-baking is performed at a temperature of about 70 degrees Celsius to about 80 degrees Celsius.

### Claim 9 (depends on 8)

The method of claim 8, wherein
the pre-baking is performed for about 60 seconds to about 80 seconds.

### Claim 10 (depends on 1)

The method of claim 1, wherein
the light comprises ultraviolet rays.

### Claim 11

A method of manufacturing a liquid crystal display, comprising:
forming a thin film transistor on a first substrate;
forming a passivation layer on the thin film transistor;
forming a first electrode and a second electrode positioned via an insulating layer interposed therebetween, on the passivation layer; and
forming a first photo-alignment layer on the first electrode or the second electrode,
wherein the forming the first photo-alignment layer comprises:
disposing a polymer material on the first electrode or the second electrode,
pre-baking the polymer material disposed on the first electrode or the second electrode,
irradiating a light to the pre-baked polymer material, to photo-align the pre-baked polymer material, and
thermal-treating the irradiated pre-baked polymer material, to harden the irradiated pre-baked polymer material,
wherein the thermal-treating comprises a first thermal-treatment, and a second thermal-treatment at a higher temperature than that of the first thermal-treatment.

### Claim 12 (depends on 11)

The method of claim 11, further comprising
forming a second photo-alignment layer on a second substrate facing the first substrate.

### Claim 13 (depends on 11)

The method of claim 11, wherein
the polymer material comprises a polyimide or polyamic acid.

### Claim 14 (depends on 13)

The method of claim 13, wherein,
the first thermal-treatment is performed at a temperature of about 140 degrees Celsius to about 180 degrees Celsius, and
the second thermal-treatment is performed at a temperature of about 190 degrees Celsius to about 230 Celsius.

### Claim 15 (depends on 14)

The method of claim 14, wherein
the first thermal-treatment and the second thermal-treatment are performed for about 20 minutes to about 40 minutes.

### Claim 16 (depends on 14)

The method of claim 14, wherein:
the first thermal-treatment stabilizes a polymer shape and increases anisotropy of the polymer material.

### Claim 17 (depends on 14)

The method of claim 14, wherein
the second thermal-treatment imidizes the polyimide or the polyamic acid of the polymer material.

### Claim 18 (depends on 11)

The method of claim 11, wherein
the pre-baking is performed at a temperature of about 70 degrees Celsius to about 80 degrees Celsius.

### Claim 19 (depends on 18)

The method of claim 18, wherein
the pre-baking is performed for about 60 seconds to about 80 seconds.

### Claim 20 (depends on 11)

The method of claim 11, wherein
the light comprises ultraviolet rays.