# US 2015/0104883 A1 · Semiconductor devices and methods for fabricating the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0104883 A1
- Document ID: US20150104883A1
- Status: Published application
- Kind: A1
- Application number: 14/306,976
- Filed: 2014-06-17
- Published: 2015-04-16
- Earliest claimed: 2013-10-15
- Assignees: Samsung Electronics Co., Ltd.
- Inventors: Whankyun KIM; Woojin KIM; Woo Chang LIM
- Web page: https://patentgrep.com/patent/US20150104883A1

## CPC

- H10N 50/01: Manufacture or treatment
- C23C 14/046: {Coating cavities or hollow spaces, e.g. interior of tubes; Infiltration of porous substrates}
- C23C 14/35: by application of a magnetic field, e.g. magnetron sputtering {(C23C14/3457 takes precedence)}
- H01J 37/3408: {Planar magnetron sputtering}
- H10B 61/22: {of the field-effect transistor [FET] type}
- H10N 50/10: Magnetoresistive devices
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A method of fabricating a semiconductor device includes providing a wafer in a chamber of a point-cusp magnetron physical vapor deposition (PCM-PVD) apparatus, the chamber including a metal target. The method further includes providing an inert gas and a reactive gas in the chamber and forming an amorphous conductive layer on the wafer by reacting the reactive gas with a metal atom separated from the metal target by the inert gas.

## Claims

### Claim 1

A method for fabricating a semiconductor device, the method comprising:
providing a wafer in a chamber of a point-cusp magnetron physical vapor deposition (PCM-PVD) apparatus, the chamber including a metal target;
providing an inert gas and a reactive gas in the chamber; and
forming an amorphous conductive layer on the wafer by reacting the reactive gas with a metal atom separated from the metal target by the inert gas.

### Claim 2 (depends on 1)

The method of claim 1, wherein
the wafer comprises an interlayer dielectric layer formed thereon, the interlayer dielectric layer including a recess region, and
the forming forms one of an amorphous metal nitride layer and an amorphous metal oxide layer filling the recess region.

### Claim 3 (depends on 2)

The method of claim 2, wherein the recess region comprises a contact hole, the method further comprising:
forming a crystalline conductive pattern filling a lower part of the contact hole before the forming an amorphous conductive layer.

### Claim 4 (depends on 3)

The method of claim 3, wherein the forming forms the crystalline conductive pattern by a chemical vapor deposition process.

### Claim 5 (depends on 1)

The method of claim 1, wherein the providing an inert gas and a reactive gas provides the reactive gas including at least one of nitrogen, ammonia, oxygen, and vapor.

### Claim 6 (depends on 1)

The method of claim 1, wherein the forming forms an amorphous metal nitride layer, the amorphous metal nitride layer including an amorphous titanium nitride layer having an amount of nitrogen that is 3/10 or less than an amount of titanium.

### Claim 7 (depends on 6)

The method of claim 6, further comprising:
unloading the wafer from the chamber; and
forming one of a magnetic tunnel junction pattern and a metal line pattern on the amorphous titanium nitride layer.

### Claim at position 8

8-14. (canceled)

### Claim 15

A method for fabricating a magnetic memory device, the method comprising:
patterning an interlayer dielectric layer on a substrate to form a recess region therein;
forming a contact plug filling the recess region, the contact plug including an amorphous titanium nitride layer; and
forming a magnetic tunnel junction pattern on the contact plug.

### Claim 16 (depends on 15)

The method of claim 15, wherein the forming a contact plug fauns the amorphous titanium nitride layer to include an amount of nitrogen that is 3/10 or less than an amount of titanium.

### Claim 17 (depends on 15)

The method of claim 15, wherein the forming a contact plug forms the amorphous titanium nitride layer constituting a lower electrode.

### Claim 18 (depends on 17)

The method of claim 17, wherein the forming a contact plug forms the amorphous titanium nitride layer including a sidewall aligned with a sidewall of the magnetic tunnel junction pattern.

### Claim 19 (depends on 15)

The method of claim 15, wherein
the forming a magnetic tunnel junction pattern forms a first magnetic layer, a tunnel barrier layer, and a reference layer on the amorphous titanium nitride layer,
the reference layer including a second magnetic layer, a capping layer, a first pinned layer, an exchange-coupling layer, and a second pinned layer that are sequentially stacked on the tunnel barrier layer.

### Claim 20 (depends on 15)

The method of claim 15, wherein the forming a contact plug forms a crystalline conductive pattern under the amorphous titanium nitride layer.

### Claim 21

A method for fabricating a magnetic memory device, the method comprising:
forming at least one interlayer dielectric layer on a substrate;
forming a lower contact plug penetrating at least a first portion of the at least one interlayer dielectric layer by a chemical vapor deposition process (CVD);
forming an upper contact plug penetrating at least a second portion of the at least one interlayer dielectric layer by a point-cusp magnetron physical vapor deposition (PCM-PVD) process;
forming a lower electrode on the at least one interlayer dielectric layer; and
forming a magnetic tunnel junction pattern on the lower electrode.

### Claim 22 (depends on 21)

The method of claim 21, wherein
the forming a lower contact plug forms the lower contact plug having a crystalline structure, and
the forming an upper contact plug forms the upper contact plug having an amorphous structure.

### Claim 23 (depends on 21)

The method of claim 21, further comprising:
patterning the at least one interlayer dielectric layer to form a contact hole in the at least one interlayer dielectric layer prior to the forming a lower contact plug,
wherein the lower contact plug fills the contact hole.

### Claim 24 (depends on 23)

The method of claim 23, further comprising:
performing an etch-back process to recess an upper portion of the lower contact plug prior to the forming an upper contact plug,
wherein the upper contact plug is formed in the recessed upper portion.

### Claim 25 (depends on 21)

The method of claim 21, wherein
the forming at least one interlayer dielectric layer forms first and second interlayer dielectric layers on the substrate,
the forming a lower contact plug forms the lower contact plug to penetrate the first interlayer dielectric layer, and
the forming an upper contact plug forms the upper contact plug to penetrate the second interlayer dielectric layer.

### Claim 26 (depends on 21)

The method of claim 21, wherein the forming a lower electrode forms the lower electrode including an amorphous titanium nitride layer having an amount of nitrogen that is 3/10 or less than an amount of titanium.

### Claim 27 (depends on 21)

The method of claim 21, wherein
the forming a magnetic tunnel junction pattern forms a first magnetic layer, a tunnel barrier layer, and a reference layer on the lower electrode,
the reference layer including a second magnetic layer, a capping layer, a first pinned layer, an exchange-coupling layer, and a second pinned layer that are sequentially stacked on the tunnel barrier layer.