# US 2015/0104882 A1 · Fabrication method for high-density mram using thin hard mask

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0104882 A1
- Document ID: US20150104882A1
- Status: Published application
- Kind: A1
- Application number: 14/051,327
- Filed: 2013-10-10
- Published: 2015-04-16
- Earliest claimed: 2013-10-10
- Assignees: Avalanche Technology, Inc.
- Applicants: Avalanche Technology Inc.
- Inventors: Dong Ha Jung; Kimihiro Satoh; Jing Zhang; Yuchen Zhou; Yiming Huai
- Web page: https://patentgrep.com/patent/US20150104882A1

## CPC

- H10N 50/01: Manufacture or treatment
- H10B 61/00: Magnetic memory devices, e.g. magnetoresistive RAM [MRAM] devices
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

Embodiments of the invention are described that use a thin metallic hard mask, which can be a bi-layer film, to increase the incident IBE angle for MTJ sidewall cleaning without losing the process margin for the subsequent interconnection process. The patterned metallic hard mask pads also serve as the top electrode for the MTJ cells. Using a thin metallic hard mask is possible when the hard mask material acts as a CMP stopper without substantial loss of thickness. In the first embodiment, the single layer hard mask is preferably ruthenium. In the second embodiment, the lower layer of the bi-layer hard mask is preferably ruthenium. The wafer is preferably rotated during the IBE process for uniform etching. A capping layer under the hard mask is preferably used as the etch stopper during hard mask etch process in order not to damage or etch through the upper magnetic layer.

## Claims

### Claim 1

A method for fabricating an array of magnetic memory cells on a wafer comprising:
depositing a plurality of layers for magnetic memory cells over a wafer, including layers for a bottom electrode, a lower magnetic layer, a junction layer and an upper magnetic layer;
depositing a capping layer over the plurality of layers for magnetic memory cells;
depositing a hard mask with at least a first layer of metallic material;
patterning the hard mask layer into hard mask pads corresponding to the array of magnetic memory cells using the capping layer as an etch stop;
forming an array of pillars by etching using the hard mask pads as a mask;
cleaning sidewalls of the pillars using ion beams with angled incidence while rotating the wafer;
depositing an inter-layer dielectric film over the pillars;
performing chemical mechanical polishing (CMP) on the wafer to expose tops of the hard mask pads through the inter-layer dielectric film, using the hard mask pads as a CMP stopper; and
performing a bit line interconnection process using the exposed tops of the hard mask pads as top electrodes for the magnetic memory cells.

### Claim 2 (depends on 1)

The method of claim 1 wherein the first layer of metallic material in the hard mask layer is ruthenium.

### Claim 3 (depends on 2)

The method of claim 2 wherein a feature size of the magnetic memory cells is less than or equal to 40 nm.

### Claim 4 (depends on 3)

The method of claim 3 wherein a thickness of the hard mask pads is approximately between 10 nm and 40 nm when the cleaning step begins.

### Claim 5 (depends on 1)

The method of claim 1 wherein an angle of incidence of the ion beams is greater than or equal to 25 degrees.

### Claim 6 (depends on 5)

The method of claim 5 wherein the angle of incidence of the ion beams is selected to target the junction layer and one of the magnetic layers.

### Claim 7 (depends on 1)

The method of claim 1 wherein performing chemical mechanical polishing ends without significant loss of thickness of the hard mask pads.

### Claim 8 (depends on 1)

The method of claim 1 wherein the capping layer is Ta, Ti, TiN, TaN, W, WN, Cr, or Al.

### Claim 9 (depends on 1)

The method of claim 1 wherein depositing a hard mask further comprises depositing a second layer over the first layer of metallic material.

### Claim 10 (depends on 2)

The method of claim 2 wherein depositing a hard mask further comprises depositing a second layer over the first layer of metallic material.

### Claim 11 (depends on 10)

The method of claim 10 wherein forming an array of pillars by etching using the hard mask pads as a mask further comprises etching down to the bottom electrode using a first selected set of etching conditions and the second layer has high resistance to the second set of etching conditions.

### Claim 12 (depends on 11)

The method of claim 11 wherein the second layer is Ta, TaN, Ti, TiN, W or WN.

### Claim 13 (depends on 10)

The method of claim 10 wherein patterning the hard mask layer into hard mask pads further comprises etching down to the first layer using a first selected set of etching conditions using the first layer as an etch stop and etching down to the capping layer using a second selected set of etching conditions using the capping layer as an etch stop.

### Claim 14 (depends on 13)

The method of claim 13 wherein the second layer is tantalum and the capping layer is tantalum.

### Claim 15 (depends on 10)

The method of claim 10 wherein the second layer of the hard mask has been removed before the step of cleaning sidewalls of the pillars.

### Claim 16 (depends on 1)

The method of claim 1 wherein cleaning sidewalls of the pillars removes unwanted material re-deposited during the step of forming an array of pillars by etching.