# US 2015/0104732 A1 · Method for Repairing a Mask

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0104732 A1
- Document ID: US20150104732A1
- Status: Published application
- Kind: A1
- Application number: 14/052,189
- Filed: 2013-10-11
- Published: 2015-04-16
- Earliest claimed: 2013-10-11
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Yen-Kai Huang; Yuan-Chih Chu
- Web page: https://patentgrep.com/patent/US20150104732A1

## CPC

- G03F 1/72: Repair or correction of mask defects
- G03F 1/22: Masks or mask blanks for imaging by radiation of 100nm or shorter wavelength, e.g. X-ray masks, extreme ultraviolet [EUV] masks; Preparation thereof
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

A method for repairing a mask is disclosed. A mask, having multiple defective regions need to be repaired, is received. Locations and sizes of the defective regions are determined. A pre-repair-passivation-treatment (PRPT) is performed to form a passivation membrane over the mask. With the passivation membrane on the mask, a mask repair process is performed to the defective regions on the mask.

## Claims

### Claim 1

A method for repairing a mask, comprising:
receiving a mask having first and second defective regions;
performing a first pre-repair-passivation-treatment (PRPT) to form a first passivation membrane over the mask;
after forming the first passivation membrane, performing a first repair process on the mask, wherein the first defective region is repaired to form a first repaired defective region;
performing a second PRPT to form a second passivation membrane over the mask, including the first repaired defective region; and
after forming the second passivation membrane, performing a second repair process on the mask, wherein the second defective region is repaired to form a second repaired defective region.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first and second passivation membranes are formed by performing an oxygen plasma treatment on the mask.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first and second passivation membranes are formed by performing a hot air flow treatment on the mask.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first and second passivation membranes are formed by performing a hot nitrogen flow treatment on the mask.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first and second passivation membranes are formed by performing a nitric acid wet treatment on the mask.

### Claim 6 (depends on 1)

The method of claim 1, wherein the defective regions are repaired by a gas-assisted focused-electron-beam-induced etching process.

### Claim 7 (depends on 1)

The method of claim 1, wherein the second passivation membrane is formed over a sidewall and a bottom of the first repaired defective region.

### Claim 8 (depends on 1)

The method of claim 1, further comprising:
determining a location and size of the first and second defective regions before performing the first PRPT; and
grouping the defective regions into the first defective region and the second defective region.

### Claim 9 (depends on 1)

The method of claim 1, wherein the mask has a plurality of defects, and wherein the second defective region includes a defect between two defects in the first defective region.

### Claim 10 (depends on 9)

The method of claim 9, wherein the first defective region includes a defect between two defects in the second defective region.

### Claim 11

A method for repairing an extreme ultraviolet (EUV) mask, comprising:
receiving an EUV mask having multiple defective regions;
determining a location and a size of each of the defective regions;
grouping defective regions into different groups;
performing a first pre-repair-passivation-treatment (PRPT) to form a first passivation membrane over the EUV mask;
after forming the first passivation membrane, repairing a first group of defective regions by a gas-assisted focused-electron-beam technique to form a first repaired defective region;
performing a second PRPT to form a second passivation membrane over the EUV mask, including the first repaired defective region; and
after forming the second passivation membrane, repairing a second group of defective regions by a gas-assisted focused-electron-beam technique to form a second repaired defective region.

### Claim 12 (depends on 11)

The method of claim 11, wherein the first and second passivation membranes are formed by performing an oxygen plasma treatment on the EUV mask.

### Claim 13 (depends on 11)

The method of claim 11, wherein the first and second passivation membranes are formed by performing a hot air flow treatment on the EUV mask.

### Claim 14 (depends on 11)

The method of claim 11, wherein the first and second passivation membranes are formed by performing a hot nitrogen flow treatment on the EUV mask.

### Claim 15 (depends on 11)

The method of claim 11, wherein the first and second passivation membranes are formed by performing a nitric acid wet treatment on the EUV mask.

### Claim 16 (depends on 11)

The method of claim 11, wherein the second passivation membrane is formed over a sidewall and bottom of the first repaired defective region.

### Claim 17 (depends on 11)

The method of claim 11, wherein a defective region in the first group of repaired defective regions is between two defective regions in the second group of repaired defective regions.

### Claim 18 (depends on 17)

The method of claim 17, wherein a defective region in the second group of repaired defective regions is between two defective regions in the first group of repaired defective regions.

### Claim 19

A method for repairing an extreme ultraviolet (EUV) mask, comprising:
receiving an EUV mask having at least one defective region, which is to be repaired;
determining a location and a size of the defect;
performing a pre-repair-passivation-treatment (PRPT) to form a passivation membrane over the EUV mask;
after forming the passivation membrane, repairing defective region by a gas-assisted focused-electron-beam technique.

### Claim 20 (depends on 19)

The method of claim 19, wherein the passivation membranes are formed by performing an oxygen plasma treatment on the EUV mask.