# US 2015/0104713 A1 · Method for the production of electrodes for fully solid batteries

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0104713 A1
- Document ID: US20150104713A1
- Status: Published application
- Kind: A1
- Application number: 14/355,182
- Filed: 2012-10-30
- Published: 2015-04-16
- Earliest claimed: 2011-11-02
- Assignees: I-Ten
- Applicants: I-Ten
- Inventors: Fabien Gaben; Frédéric Bouyer; Bruno Vuillemin
- Web page: https://patentgrep.com/patent/US20150104713A1

## CPC

- H01M 4/0457: {from dispersions or suspensions; Electrophoresis}
- H01M 4/0402: {Methods of deposition of the material}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 4/043: {involving compressing or compaction}
- H01M 4/0435: {Rolling or calendering}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/58: of inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy; of polyanionic structures, e.g. phosphates, silicates or borates
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The invention relates to a process for fabrication of an electrode film in an all-solid-state battery comprising successive steps to: a) Procure a substrate, preferably a conducting substrate, b) Deposit an electrode film on said substrate by electrophoresis, from a suspension containing particles of electrode materials, c) Dry the film obtained in the previous step, d) Thermal consolidation of the electrode film obtained in the previous step by sintering, sintering being done at a temperature TR that preferably does not exceed 0.7 times the melting temperature (expressed in ° C.), even more preferably does not exceed 0.5 times the melting temperature (expressed in ° C.), and much more preferably does not exceed 0.3 times the melting temperature (expressed in ° C.) of the electrode material that melts at the lowest temperature.

## Claims

### Claim at position 1

1-17. (canceled)

### Claim 18

A process for fabrication of an electrode film in an all-solid-state battery, comprising:
providing a conducting substrate;
depositing, from a suspension containing particles of electrode materials having an average size of less than 1 μm, an electrode film on said conducting substrate by electrophoresis;
drying the electrode film; and
thermally consolidating the dried electrode film by sintering at a temperature that does not exceed 0.7 times a melting temperature of the electrode material that melts at a lowest temperature.

### Claim 19 (depends on 18)

The process of claim 18, wherein the temperature does not exceed 0.5 times the melting temperature of the electrode material that melts at the lowest temperature.

### Claim 20 (depends on 18)

The process of claim 18, wherein the temperature does not exceed 0.3 times the melting temperature of the electrode material that melts at the lowest temperature.

### Claim 21 (depends on 18)

The process of claim 18, wherein the average size of particles of electrode material is one of:
less than 100 nm; and
less than or equal to 30 nm.

### Claim 22 (depends on 18)

The process of claim 18, further comprising mechanically compacting the dried electrode film, one of before, during, or after thermally consolidating the dried electrode film.

### Claim 23 (depends on 22)

The process of claim 22, wherein mechanically compacting the dried electrode film is done by application of a compression pressure between one of:
20 and 100 MPa; and
40 and 60 MPa.

### Claim 24 (depends on 22)

The process of claim 22, wherein at least one of thermally consolidating the dried electrode film and mechanically compacting the dried electrode film is done under a vacuum or an inert atmosphere.

### Claim 25 (depends on 18)

The process of claim 18, wherein the conducting substrate comprises an aluminium film.

### Claim 26 (depends on 18)

The process of claim 18, wherein the electrophoretic deposition is made by anaphoresis.

### Claim 27 (depends on 18)

The process of claim 18, wherein the thickness of the deposited electrode film is one of:
less than 20 μm;
less than 10 μm; and
less than 5 μm.

### Claim 28 (depends on 18)

The process of claim 18, wherein nanoparticles used for making the electrode film are chosen from among at least one of:
LiMn2O4, LiCoO2, LiNiO2, LiMn1,5Ni0,5O4, LiMn1,5Ni0,5-xXxO4 oxides (where x is selected from among Al, Fe, Cr, Co, Rh, Nd, other rare earths and in which 0<x<0.1), LiFeO2, LiMn1/3Ni1/3Co1/3O4;
LiFePO4, LiMnPO4, LiCoPO4, LiNiPO4, Li3V2(PO4)3 phosphates; and
all lithium forms of the following chalcogenides: V2O5, V3O8, TiS2, TiOySz, WOySz, CuS, CuS2.

### Claim 29 (depends on 18)

The process of claim 18, wherein nanoparticles used for making the electrode film are chosen from among at least one of:
tin oxinitrides (SnOxNy);
mixed silicon and tin oxinitrides (typical formula SiaSnbOyNz where a>0, b>0, a+b≦2, 0<y≦4. 0<z≦3) (also called SiTON), and SiSn0,87O1,2N1,72; and oxinitrides in the form SiaSnbCcOyNz where a>0, b>0, a+b≦2, 0<c−10, 0<y<24. 0<z<17; SiaSnbCcOyNzXn and SiaSnbOyNzXn where Xn is at least one of the elements F, Cl, Br, I, S, Se, Te, P, As, Sb, Bi, Ge, Pb;
SixNy type nitrides, SnxNy, ZnxNy, Li3-xMxN (where M=Co, Ni, Cu); and
SnO2, Li4Ti5O12, SnB0,6P0,4O2,9 oxides.

### Claim 30 (depends on 18)

The process of claim 18, wherein nanoparticles used for making the electrode film are chosen from SixNy type nitrides (in which x=3 and y=4), SnxNy type nitrides (in which x=3 and y=4), ZnxNy type nitrides (in which x=3 and y=4), and Li3-xMxN type nitrides (where M=Co, Ni, Cu).

### Claim 31 (depends on 18)

The process of claim 18, wherein nanoparticles used for making the electrode film comprise SiSn0,87O1,2N1,72.

### Claim 32 (depends on 18)

The process of claim 18, wherein at least one of electron conducting nanoparticles and lithium ion conducting nanoparticles are deposited at the same time as electrode material nanoparticles.

### Claim 33 (depends on 32)

The process of claim 32, wherein the conducting nanoparticles are composed of at least one of ceramic and vitroceramic materials chosen from at least one of:
lithium compounds based on lithium and phosphorus oxinitride (LiPON) in the form LixPOyNz where x˜2.8 and 2y+3z˜7.8 and 0.16≦z≦0.4, all variants in the form LiwPOxNySz where 2x+3y+2z=5=w and 3.2≦x≦3.8, 0.13≦y≦0.4, 0≦z≦0.2, 2.9≦w≦3.3 or in the form LitPxAlyOuNvSw where 5x+3y=5, 2u+3v+2w=5+t, 2.9≦t≦3.3, 0.94≦x≦0.84, 0.094≦y≦0.26, 3.2≦u≦3.8, 0.13≦v≦0.46, 0≦w≦0.2;
lithium compounds based on lithium, phosphorus and silicon oxinitride (LiSiPON);
lithium oxinitrides of the LiBON, LiBSO, LiSiPON, LiSON, thio-LiSiCON, LiPONB types (where B, P and S represent boron, phosphorus and sulfur respectively);
La0,51Li0,34Ti2,94, Li3,4V0,4Ge0,6O4, Li2O—Nb2O5, LiAlGaSPO4 compounds; and
formulations based on Li4SiO4, Li3PO4, Li2CO3, B2O3, Li2O, Al(PO3)3LiF, P2S3, Li2S, Li3N, Li14Zn(GeO4)4, Li3,6Ge0,6V0,4O4, LiTi2(PO4)3, Li0,35La0,55TiO3, Li3,25Ge0,25P0,25S4, Li1,3Al0,3Ti1,7(PO4)3, Li1+xAlxM2-x(PO4)3 (where M=Ge, Ti, and/or Hf, and where 0<x<1), Li1+x+yAlxTi2-xSiyP3-yO12 (where 0≦x≦1 and 0≦y≦1), and Li1+x+zMx(Ge1-yTiy)2-xSizP3-zO12 (where 0≦x≦0.8; 0≦y≦1.0; 0≦z≦0.6).

### Claim 34 (depends on 18)

The process of claim 18, wherein the electrolyte material comprises Li2,9PO3,3N0,46.

### Claim 35 (depends on 18)

The process of claim 18, wherein the electrolyte material comprises Li1.9Si0.28P1.0O1.1N1.0.

### Claim 36 (depends on 18)

The process of claim 18, wherein the electrolyte material is chosen from formulations based on 4.9LiI-34,1Li2O-61B2O3, 0,30Li2S-0.26B2S3.0.44LiI, 60Li2S-40SiS2, 0.02Li3PO4-0.98(Li2S—SiS2), 2(Li1,4Ti2Si0,4P2,6O12)—AlPO4, and 0.7Li2S-0.3P2S5.

### Claim 37 (depends on 18)

The process of claim 18, wherein suspensions of electrode material particles have a dry extract between 2 and 20 g/L.

### Claim 38 (depends on 18)

The process of claim 18, wherein suspensions of electrode material particles do not contain any stabilizers.

### Claim 39 (depends on 18)

The process of claim 18, wherein said suspensions of electrode material particles comprise graphite nanoparticles and nanoparticles of at least one of electron conducting materials and lithium ion conducting materials,

### Claim 40 (depends on 39)

The process of claim 39, wherein said electron conducting materials and lithium ion conducting materials melt at a lower temperature than the electrode materials.

### Claim 41

An electrode film in an all-solid-state battery, comprising:
at least one phase composed of one of an anode active material or a cathode active material, and at least one lithium ion conducting phase and electron conducting phase, said conducting phases being crystallized with a size grain between 1 and 100 nm.