# US 2015/0104710 A1 · Cathode active material, cathode and nonaqueous secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0104710 A1
- Document ID: US20150104710A1
- Status: Published application
- Kind: A1
- Application number: 14/575,194
- Filed: 2014-12-18
- Published: 2015-04-16
- Earliest claimed: 2009-05-22
- Assignees: Sharp Kabushiki Kaisha
- Applicants: Sharp Kabushiki Kaisha
- Inventors: Koji OHIRA; Motoaki NISHIJIMA; Toshitsugu SUEKI; Shogo ESAKI; Isao TANAKA; Yukinori KOYAMA; Katsuhisa TANAKA; Koji FUJITA; Shunsuke MURAI
- Web page: https://patentgrep.com/patent/US20150104710A1

## CPC

- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/623: {fluorinated polymers}
- H01M 4/625: {Carbon or graphite}
- H01M 10/0481: {Compression means other than compression means for stacks of electrodes and separators}
- H01M 10/052: Li-accumulators
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 10/0587: of accumulators having only wound construction elements, i.e. wound positive electrodes, wound negative electrodes and wound separators
- C01B 33/20: Silicates (persilicates C01B15/14 {; containing aluminium C01B33/26})
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- Y02P 20/133: Renewable energy sources, e.g. sunlight
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- Y10T 29/4911: including sealing
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A cathode active material of the present invention is a cathode active material having a composition represented by General Formula (1) below, LiFe1−xMxP1-ySiyO4 (1), where: an average valence of Fe is +2 or more; M is an element having a valence of +2 or more and is at least one type of element selected from the group consisting of Zr, Sn, Y, and Al; the valence of M is different from the average valence of Fe; 0<x≦0.5; and y=x×({valence of M}−2)+(1−x)×({average valence of Fe}−2). This provides a cathode active material that not only excels in terms of safety and cost but also can provide a long-life battery.

## Claims

### Claim 1

A nonaqueous secondary battery, comprising:
a cathode including a cathode active material;
an anode;
an electrolyte; and
a separator,
the cathode active material having a composition represented by General Formula (1) below,
LiFe1−xMxP1-ySiyO4 (1)
where:
an average valence of Fe is +2 or more;
M is an element having a valence of +2 or more and is at least one type of element selected from the group consisting of Zr, Sn, Y, and Al;
the valence of M is different from the average valence of Fe;
0<x≦0.5; and
0<y≦1.0,
the cathode active material having, in a case where the nonaqueous secondary battery has a voltage of 3.9 V or higher, a composition represented by General Formula (2) below,
LixFe1−xMxP1-ySiyO4 (2).

### Claim 2 (depends on 1)

The nonaqueous secondary battery according to claim 1,
wherein:
the electrolyte is an electrolyte selected from the group consisting of an organic electrolyte, a gel electrolyte, a polymer solid electrolyte, an inorganic solid electrolyte, and a molten salt.

### Claim 3 (depends on 1)

The nonaqueous secondary battery according to claim 1,
wherein:
the cathode active material is provided with a carbon film.

### Claim 4 (depends on 1)

The nonaqueous secondary battery according to claim 1, further comprising:
a battery armor made of a metal.

### Claim 5 (depends on 1)

The nonaqueous secondary battery according to claim 1,
wherein:
the nonaqueous secondary battery is a layered cuboidal battery.

### Claim 6

A method for producing a nonaqueous secondary battery,
the nonaqueous secondary battery including:
a cathode including a cathode active material;
an anode;
an electrolyte; and
a separator,
the cathode active material having a composition represented by General Formula (1) below,
LiFe1−xMxP1-ySiyO4 (1)
where:
an average valence of Fe is +2 or more;
M is an element having a valence of +2 or more and is at least one type of element selected from the group consisting of Zr, Sn, Y, and Al;
the valence of M is different from the average valence of Fe;
0<x≦0.5; and
0<y≦1.0,
the method comprising the steps of:
forming a layered product or wound product including the cathode, the anode, and the separator; and
heating the layered product or wound product in a decompressed chamber.

### Claim 7 (depends on 6)

The method according to claim 6, further comprising the steps of:
inserting the layered product or wound product into a battery container; and
sealing the nonaqueous secondary battery by fitting a lid in an opening of the battery container and laser-welding the lid to the opening.

### Claim 8 (depends on 6)

The method according to claim 6, further comprising the steps of:
forming an electrode by applying, to a current collector, a slurry obtained by mixing the cathode active material, a conductive material, a binder, and an organic solvent; and
pressing the electrode by passing the electrode through a space between two metal rollers for the electrode to have an intended thickness,
the space between the two metal rollers having been adjusted to a size 0.858 to 0.867 time as large as the intended thickness.