# US 2015/0104708 A1 · Oxide cathode material for lithium ion battery having high energy density and preparation process thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0104708 A1
- Document ID: US20150104708A1
- Status: Published application
- Kind: A1
- Application number: 14/579,824
- Filed: 2014-12-22
- Published: 2015-04-16
- Earliest claimed: 2012-06-21
- Assignees: Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences; Ningde Contemporary Amperex Technology Limited
- Applicants: Ningbo Institute of Materials Technology & Engineering, Chinese Academy of Sciences; Ningde Contemporary Amperex Technology Limited
- Inventors: Yujing BI; Deyu WANG; Jun LI
- Web page: https://patentgrep.com/patent/US20150104708A1

## CPC

- H01M 4/366: {as layered products}
- C01G 51/42: containing alkali metals, e.g. LiCoO2
- C01G 53/502: containing lithium and cobalt
- C01G 53/504: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.5, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.5
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Provided are a high energy density oxide anode material for lithium ion battery, preparation process and use thereof. Said anode material includes a main part of the anode material and a covering layer. Said main part includes a shell and a core inside the shell. The material of said core is Li1+x[Ni1−y−zCoyMnz]O2 wherein −0.1≦x≦0.2, 0≦y≦0.5, 0≦z≦0.5 and 0≦y+z≦0.7. The material of said shell is Li1+a[Co1−bXb]O2, wherein −0.1≦a≦0.2, 0≦b≦0.5, and X is selected from Al, Mg, Cu, Zr, Ti, Cr, V, Fe, Mn, Ni, or combination thereof. Otherwise, The material of said main part is a mixture of Li1+x[Ni1−y−zCoyMnz]O2 and LiCoO2, wherein −0.1≦x≦0.2, 0≦y≦0.5, 0<z≦0.5 and 0≦y+z≦0.7. The material of said covering layer is selected from Al2O3, ZrO2, MgO, SiO2, ZnO2, TiO2, Y2O3, LiAlO2, or combination thereof. Said anode material has the advantages of high capacity, good cycle performance, low surface activity, high voltage resistance and fine safety. The preparation process is simple, and is suitable for large-scale production.

## Claims

### Claim 1

A cathode material comprising of a cathode material body and a coating layer located on the surface of the cathode material body,
wherein, the material of the coating layer is Al2O3, ZrO2, MgO, SiO2, ZnO, TiO2, Y2O3, LiAlO2, or the combination thereof;
said cathode material body includes a shell and a core inside the shell, wherein the core material is Li1−x[Ni1−y−zCoyMnz]O2, wherein, −0.1≦x≦0.2, 0≦y≦0.5, 0≦z≦0.5 and 0≦y+z≦0.7; the shell material is Li1−a[Co1−bXb]O2, wherein −0.1≦a≦0.2, 0≦b≦0.5, and X is Al, Mg, Cu, Zr, Ti, Cr, V, Fe, Mn, Ni, or the combination thereof; or
alternatively said cathode material body is a mixture of Li1−x[Ni1−y−zCoyMnz]O2 and LiCoO2, wherein, −0.1≦x≦0.2, 0≦y≦0.5, 0≦z≦0.5 and 0≦y+z≦0.7.

### Claim 2 (depends on 1)

According to the cathode material of claim 1, wherein the lattice structures of the core material and the shell material are α-NaFeO2, and the space groups thereof are R-3m.

### Claim 3 (depends on 1)

According to the cathode material of claim 1, wherein the ratio of the thickness of the shell and the radius of the cathode material particular is about 0.005-0.5; and/or the thickness of the coating layer is 0.2-50 nm.

### Claim 4 (depends on 1)

According to the cathode material of claim 1, wherein the amount of Ni in the core material is more than that in the shell material, and the amount of Co in the core material is less than that in the shell material.

### Claim 5 (depends on 1)

According to the cathode material of claim 1, wherein the core is comprised of crystalline grain with 0.1-5 μm and the shell is comprised of crystalline grain with 0.1-5 μm.

### Claim 6 (depends on 1)

A method for the preparation of the cathode material of claim 1 comprising the steps:
(a) precipitating the hydroxide of cobalt or that of X and cobalt on the surface of Ni1−y−zCoyMnz(OH)2 to obtain a core-shell precursor P;
(b) mixing the core-shell precursor P with a lithium source at the mole ratio of Li/P=1-1.2 and then sintering the mixture;
(c) precipitating the hydroxide of metal M on the surface of the sintered material;
(d) sintering at 200-1000° C. for 0.5-24 h to obtain the cathode material,
wherein, 0≦y≦1.0, 0≦z≦1.0, 0≦y+z≦1, and 0≦b≦1 .0;
X and M independently selected from one of Al, Mg, Cu, Zr, Ti, Cr, V, Fe, Mn, Ni, Y, Zn or the combination thereof.

### Claim 8 (depends on 6)

According to the method of claim 6, wherein in step (c), the sintered sample is placed into a buffer solution, a salt solution of M metal is added and the pH value is adjusted to alkalinity, and the hydroxide of metal M is precipitated on the surface of the sintered sample.

### Claim 9 (depends on 8)

According to the method of claim 8, wherein the buffer solution is one of acetic acid-sodium acetate, acetic acid-potassium acetate, acetic acid-lithium acetate, ammonia-ammonium chloride, aqueous ammonia, ammonium acetate-sodium acetate, acetic acid, ammonia-sodium hydroxide, ammonia-potassium hydroxide, phosphate buffer solution, borate buffer solution or the combination thereof, and the pH of said buffer solution is 4.0-14.0.

### Claim 10 (depends on 1)

A preparation method of the cathode material of claim 1 comprising the steps:
(a) mixing Ni1−y−zCoyMn7(OH)2 with Co3O4 to obtain a core-shell precursor P;
(b) mixing the core-shell precursor P with a lithium source at the mole ratio of Li/P=1-1.2 and then sintering the mixture;
(c) precipitating the hydroxide of metal M on the surface of sintered material;
(d) sintering at 200-1000° C. for 0.5-24 h to obtain the cathode material,
wherein, 0≦y≦1.0, 0≦z≦1.0, 0≦y+z≦1, and 0≦b≦1.0;
X and M independently selected from one of Al, Mg, Cu, Zr, Ti, Cr, V, Fe, Mn, Ni, Y, Zn or the combination thereof.

### Claim 11 (depends on 10)

According to the method of claim 10, wherein in step (c), the sintered sample is placed into a buffer solution, a salt solution of M metal is added and the pH value is adjusted to alkalinity, and the hydroxide of metal M is precipitated on the surface of the sintered sample.

### Claim 12 (depends on 11)

According to the method of claim 11, wherein the buffer solution is one of acetic acid-sodium acetate, acetic acid-potassium acetate, acetic acid-lithium acetate, ammonia-ammonium chloride, aqueous ammonia, ammonium acetate-sodium acetate, acetic acid, ammonia-sodium hydroxide, ammonia-potassium hydroxide, phosphate buffer solution, borate buffer solution or the combination thereof, and the pH of said buffer solution is 4.0-14.0.

### Claim 13 (depends on 1)

A lithium ion battery comprising of the cathode material of claim 1.