# US 2015/0104699 A1 · Nonaqueous electrolyte secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0104699 A1
- Document ID: US20150104699A1
- Status: Published application
- Kind: A1
- Application number: 14/509,553
- Filed: 2014-10-08
- Published: 2015-04-16
- Earliest claimed: 2013-10-11
- Assignees: Automotive Energy Supply Corporation
- Applicants: Automotive Energy Supply Corporation
- Inventors: Takashi NAKAGAWA
- Web page: https://patentgrep.com/patent/US20150104699A1

## CPC

- H01M 10/05: Accumulators with non-aqueous electrolyte (H01M10/39 takes precedence)
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 10/049: {Processes for forming or storing electrodes in the battery container}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0567: characterised by the additives
- H01M 10/4235: {Safety or regulating additives or arrangements in electrodes, separators or electrolyte (H01M10/4242 takes precedence)}
- H01M 50/147: Lids or covers
- H01M 10/446: {Initial charging measures}
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2010/4292: {Aspects relating to capacity ratio of electrodes/electrolyte or anode/cathode}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A battery subjected to a charging/discharging including at least initial charging is configured such that a power generating element constituting a laminated positive electrode and negative electrode separated by a separator is stored within a covering along with a nonaqueous electrolyte and an additive, the covering is sealed with a terminal leading out of the covering, and a relational expression RE<RC<RA is defined by using a total amount of presence WE of the additive component in the electrolyte, WC of the additive component in the positive electrode, and WA of the additive component in the negative electrode after charging/discharging as WT, and by using an abundance ratio of WE with respect to the total amount of WT, WC with respect to the total amount of WT, and WA with respect to the total amount of WT as RE, RC, and RA.

## Claims

### Claim 1

A nonaqueous electrolyte secondary battery subjected to a charging/discharging that at least includes an initial charging, comprising:
a power generating element including a positive electrode, a negative electrode, and a separator, the power generating element being configured to laminate the positive electrode and the negative electrode separated by the separator;
a nonaqueous electrolyte including an additive component; and
a covering storing the power generating element with the nonaqueous electrolyte,
the covering configured to form a seal with a terminal led outwardly, and
a relational expression RE<RC<RA defined by using a total amount of presence WE of the additive component in the electrolyte, an amount of presence WC of the additive component in the positive electrode, and an amount of presence WA of the additive component in the negative electrode after the charging/discharging as WT, and by using an abundance ratio of WE with respect to WT as RE, an abundance ratio of WC with respect to WT as RC, and an abundance ratio of WA with respect to WT as RA.

### Claim 2 (depends on 1)

The nonaqueous electrolyte secondary battery according to claim 1, wherein a ratio of a surface area of a positive electrode active material layer formed on the positive electrode with respect to a surface area of a negative electrode active material layer formed on the negative electrode is 1.8 or less.

### Claim 3 (depends on 1)

The nonaqueous electrolyte secondary battery according to claim 1, wherein an average specific surface area of the positive electrode active material layer is 0.60 m2/g or less.

### Claim 4 (depends on 1)

The nonaqueous electrolyte secondary battery according to claim 1, wherein a conducting agent contained in the positive electrode active material layer is 3 wt % or less.

### Claim 5 (depends on 1)

The nonaqueous electrolyte secondary battery according to claim 1, wherein a porosity of the positive electrode active material layer is less than a porosity of the negative electrode active material layer.

### Claim 6 (depends on 1)

The nonaqueous electrolyte secondary battery according to claim 1, wherein a conducting agent contained in the positive electrode active material layer is 3 wt % or less, and wherein a porosity of the positive electrode active material layer is less than a porosity of the negative electrode active material layer.

### Claim 7 (depends on 1)

The nonaqueous electrolyte secondary battery according to claim 1, wherein a ratio of a surface area of a positive electrode active material layer formed on the positive electrode with respect to a surface area of a negative electrode active material layer formed on the negative electrode is 1.8 or less, wherein a conducting agent contained in the positive electrode active material layer is 3 wt % or less, and wherein a porosity of the positive electrode active material layer is less than a porosity of the negative electrode active material layer.

### Claim 8 (depends on 1)

The nonaqueous electrolyte secondary battery according to claim 1, wherein an average specific surface area of the positive electrode active material layer is 0.60 m2/g or less, wherein a conducting agent contained in the positive electrode active material layer is 3 wt % or less, and wherein a porosity of the positive electrode active material layer is less than a porosity of the negative electrode active material layer.

### Claim 9 (depends on 2)

The nonaqueous electrolyte secondary battery according to claim 2, wherein a conducting agent contained in the positive electrode active material layer is 3 wt % or less.

### Claim 10 (depends on 3)

The nonaqueous electrolyte secondary battery according to claim 3, wherein a conducting agent contained in the positive electrode active material layer is 3 wt % or less.

### Claim 11 (depends on 2)

The nonaqueous electrolyte secondary battery according to claim 2, wherein a porosity of the positive electrode active material layer is less than a porosity of the negative electrode active material layer.

### Claim 12 (depends on 3)

The nonaqueous electrolyte secondary battery according to claim 3, wherein a porosity of the positive electrode active material layer is less than a porosity of the negative electrode active material layer.