# US 2015/0104663 A1 · Olefinically unsaturated radial styrenic block copolymer and an improved vulcanizer-free latex comprising water and said radial styrenic block copolymer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0104663 A1
- Document ID: US20150104663A1
- Status: Published application
- Kind: A1
- Application number: 14/510,202
- Filed: 2014-10-09
- Published: 2015-04-16
- Earliest claimed: 2013-10-11
- Assignees: Kraton Polymers U.S. LLC
- Applicants: Kraton Polymers U.S. LLC
- Inventors: Wouter DE JONG; Maarten TROMP
- Web page: https://patentgrep.com/patent/US20150104663A1

## CPC

- C08K 5/375: containing six-membered aromatic rings {(C08K5/3725 takes precedence)}
- C08F 297/046: {polymerising vinyl aromatic monomers and isoprene, optionally with other conjugated dienes}
- C08K 5/13: Phenols; Phenolates
- C08K 5/37: Thiols
- C08K 5/372: Sulfides {, e.g. R-(S)x-R'}
- C08K 5/378: containing heterocyclic rings
- C08K 5/524: Esters of phosphorous acids, e.g. of H3PO3
- A41D 19/01505: {resistant to mechanical aggressions, e.g. cutting. piercing}
- Y10T 428/31938: Polymer of monoethylenically unsaturated hydrocarbon
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- A41D: OUTERWEAR; PROTECTIVE GARMENTS; ACCESSORIES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The invention concerns an olefinically unsaturated radial styrenic block copolymer having the general formula A-B—Y—(B-A)n wherein each A is independently a polymer block composed of at least 90 mol. % of an alkenyl aromatic hydrocarbon, each B is independently a polymer block composed of at least 90 mol. % of one or more conjugated dienes, Y is the remnant of a coupling agent, and n is an integer from 2 to 5. The invention is also an improved vulcanizer-free latex comprising water and the olefinically unsaturated radial styrenic block copolymer. Moreover, the invention concerns a process for preparing articles by coagulation dipping from the improved latex and dipped goods made from such latex.

## Claims

### Claim 1

An olefinically unsaturated radial styrenic block copolymer of the general formula:
A-B—Y—(B-A)n
wherein
each A is independently a polymer block composed for at least 90 mol. % of an alkenyl aromatic hydrocarbon;
the content of A by weight of the total weight of the polymer (PSC) is in the range of 8-13%;
Y is the remnant of a coupling agent having a functionality greater than 2;
the degree of branching (DoB) is n+1, wherein n is an integer from 2 to 5, preferably 2 to 4;
each B is independently an olefinically unsaturated polymer block composed for at least 90 mol. % of one or more conjugated dienes;
the styrenic block copolymer has a coupling efficiency (CE) of at least 90%;
each A block independently has a weight average molecular weight (MW A) ranging from 9,000 to 15,000, and
each B Block independently has a weight average molecular weight (MW B) ranging from 75,000 to 150,000, wherein the molecular weights are determined pursuant to ASTM 3536 using mon-dispersed polystyrene standards.

### Claim 2 (depends on 1)

The radial styrenic block copolymer of claim 1, wherein each B is a polymer block composed for at least 90 mol. % of isoprene.

### Claim 3 (depends on 2)

The radial styrenic block copolymer of claim 2, wherein at least one B comprises at most 10 mol. % butadiene with at least 1 butadiene unit directly connected to the remnant of the coupling agent Y.

### Claim 4 (depends on 1)

The radial styrenic block copolymer of claim 1, wherein each A is a polymer block composed for at least 90 mol. % of styrene.

### Claim 5 (depends on 1)

The radial styrenic block copolymer of any one of claim 1, wherein Y is the remnant of gamma-glycidoxy-propyltrimethoxysilane.

### Claim 6 (depends on 1)

The radial styrenic block copolymer of any one of claim 1, wherein the styrenic block copolymer has a coupling efficiency in the range of 92 to about 100%.

### Claim 7 (depends on 1)

The radial styrenic block copolymer of any one of claim 1, wherein the total A is in the range of 9-12% by weight of the total weight of the polymer.

### Claim 8 (depends on 1)

The radial styrenic block copolymer of any one of claim 1, wherein each A block independently has a weight average molecular weight ranging from 10,000 to 12,000.

### Claim 9 (depends on 1)

The radial styrenic block copolymer of any one of claims 1, wherein each B block independently has a weight average molecular weight ranging from 80,000 to 120,000.

### Claim 10 (depends on 1)

A vulcanizer-free artificial latex comprising water and one or more styrenic block copolymers as defined in claims 1 dispersed in said water in an amount of 20 to 80% by weight of the combination of water and styrenic block copolymer.

### Claim 11 (depends on 10)

The artificial latex of claim 10, comprising said one or more styrenic block copolymers in an amount of 50 to 70, preferably of 55 to 65% by weight of the combination of water and styrenic block copolymer.

### Claim 12 (depends on 10)

The artificial latex of claim 10, comprising
(a) a thio-functionalized phenolic antioxidant, or
(b) an antioxidant package comprising a primary phenolic antioxidant and a thioester as secondary antioxidant; or
(c) a combination of (a) and (b).

### Claim 13 (depends on 10)

The artificial latex of claim 10 comprising a primary phenolic antioxidant selected from 2,6-di-t-butyl-4-methylphenol, 2,6,-di-t-butylphenol, 2,6-di-t-butyl-4-methylphenol, butyl hydroxyanisole, 2,6-di-t-butyl-α-dimethylamino-p-cresol, octadecyl-3-(3,5-di-t-butyl-4-hydroxyphenyl)propionate, styrenated phenol, 2,2′-methylenebis(6-α-methylbenzyl-p-cresol), 4,4′-methylenebis(2,6-di-t-butylphenol), 2,2′-methylenebis(4-methyl-6-t-butylphenol), pentaerythritol tetrakis(3-(3,5-di-t-butyl-4-hydroxyphenyl)propionate), 3,3′,3′,5,5′, 5′-hexa-tert-butyl-a,a′,a′-(mesitylene-2,4,6-triyl)tri-p-cresol, alkylated bisphenol, the butylation reaction product of p-cresol and dicyclopentadiene, or a mixture of two or more thereof, and comprising a thioester selected from dilauryl thiodipropionate and distearyl thiodipropionate.

### Claim 14 (depends on 10)

The rubber latex of claim 10 comprising a thio-functionalized phenolic antioxidant selected from thiobisphenolic antioxidants such as 2,2′-thiobis(4-methyl-6-t-butylphenol), 4,4′-thiobis(6-t-butyl-o-cresol), 4,6-bis(octylthiomethyl)-o-cresol, 4,6-bis(dodecylthiomethyl)-o-cresol, thiodiethylene bis[3-(3,5-di-t-butyl-4-hydroxy-phenyl)propionate], 2,6-di-t-butyl-4-(4,6-bis(octylthio)-1,3,5-triazin-2-ylamino)phenol, or a mixture of two or more thereof, preferably selected from 2,6-di-t-butyl-4-(4,6-bis(octylthio)-1,3,5-triazin-2-ylamino)phenol, thiodiethylene bis[3-(3,5-di-t-butyl-4-hydroxy-phenyl)propionate] and 4,6-bis(dodecylthiomethyl)-o-cresol, or a mixture of two or more thereof).

### Claim 15 (depends on 10)

The rubber latex of claim 10 comprising a thio-functionalized phenolic antioxidant, and/or a combination of a primary phenolic antioxidant and a thioester wherein the amount of the thio-functionalized phenolic antioxidant is within a range of from 0.1 to 3.0 parts by weight, preferably within a range of from 0.15 to 2.5 parts by weight, and more preferably within a range of from 0.2 to 2.0 parts by weight, per 100 parts by weight of the rubber constituting the rubber latex (phr), and/or wherein the amount of the primary antioxidant and the thioester are each independently within a range of from 0.1 to 3.0 parts by weight, preferably within a range of from 0.15 to 2.5 parts by weight, and more preferably within a range of from 0.2 to 2.0 parts by weight, per 100 parts by weight of the rubber constituting the rubber latex (phr).

### Claim 16 (depends on 10)

A process for preparing articles by coagulation dipping from the artificial latex according to any one of claim 10, wherein a film is made from the latex and said film is allowed to dry and wherein said film is annealed for at least 10 minutes at an annealing temperature within the range of 100-130° C.

### Claim 17 (depends on 16)

The process of claim 16, wherein said film is annealed at about 120° C.

### Claim 18 (depends on 1)

Dipped goods comprising a film composed of the olefinically unsaturated radial styrenic block copolymer of claim 1.