# US 2015/0104654 A1 · Glass laminate, and method for using block copolymer hydrogenation product as binder for glass laminate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0104654 A1
- Document ID: US20150104654A1
- Status: Published application
- Kind: A1
- Application number: 14/403,901
- Filed: 2013-05-24
- Published: 2015-04-16
- Earliest claimed: 2012-05-25
- Applicants: Zeon Corporation
- Inventors: Teiji Kohara; Naoki Tanahashi
- Web page: https://patentgrep.com/patent/US20150104654A1

## CPC

- B32B 17/10798: {containing silicone}
- B32B 17/10587: {created by embossing}
- B32B 17/10678: {comprising UV absorbers or stabilizers, e.g. antioxidants}
- B32B 17/10697: {being cross-linked}
- C08F 8/42: Introducing metal atoms or metal-containing groups
- C08F 287/00: Macromolecular compounds obtained by polymerising monomers on to block polymers
- C08K 5/005: {Stabilisers against oxidation, heat, light, ozone}
- C09J 5/00: Adhesive processes in general; Adhesive processes not provided for elsewhere, e.g. relating to primers
- C09J 153/025: {modified}
- B32B 2250/03: 3 layers
- B32B 2605/00: Vehicles
- C08K 5/3492: Triazines
- C08K 5/5425: containing at least one C=C bond
- Y10T 428/31612: As silicone, silane or siloxane
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A laminated glass may be obtained by integrally bonding glass sheets through an adhesive, the adhesive comprising a hydrogenated block copolymer obtained by introducing an alkoxysilyl group into a hydrogenated block copolymer that is obtained by hydrogenating unsaturated bonds of a block copolymer that comprises at least two polymer blocks and at least one polymer block, the polymer block comprising a repeating unit derived from an aromatic vinyl compound as a main component, the polymer block comprising a repeating unit derived from a linear conjugated diene compound as a main component, and a ratio (wA:wB) of a weight fraction wA of the polymer block in the block copolymer to a weight fraction wB of the polymer block in the block copolymer being 30:70 to 60:40. The laminated glass may employ a block copolymer hydrogenation product comprising an alkoxysilyl group and excellent light-fastness, heat resistance, moisture resistance and transparency.

## Claims

### Claim 1

Laminated glass obtained by integrally bonding glass sheets through an adhesive, the adhesive comprising a hydrogenated block copolymer obtained by introducing an alkoxysilyl group into a hydrogenated block copolymer that is obtained by hydrogenating 90% or more of unsaturated bonds of a block copolymer that comprises at least two polymer blocks and at least one polymer block, the polymer block comprising a repeating unit derived from an aromatic vinyl compound as a main component, the polymer block comprising a repeating unit derived from a linear conjugated diene compound as a main component, and a ratio (wA:wB) of a weight fraction wA of the polymer block in the block copolymer to a weight fraction wB of the polymer block in the block copolymer being 30:70 to 60:40.

### Claim 2 (depends on 1)

The laminated glass according to claim 1, wherein the adhesive further comprises a hindered amine-based light stabilizer in an amount of 0.02 to 2.5 parts by weight based on 100 parts by weight of the hydrogenated block copolymer.

### Claim 3 (depends on 1)

The laminated glass according to claim 1, wherein the adhesive further comprises a UV absorber in an amount of 0.02 to 1 part by weight based on 100 parts by weight of the hydrogenated block copolymer.

### Claim 4

A method comprising using a hydrogenated block copolymer as an adhesive for laminated glass, the hydrogenated block copolymer being obtained by introducing an alkoxysilyl group into a hydrogenated block copolymer that is obtained by hydrogenating 90% or more of unsaturated bonds of a block copolymer that comprises at least two polymer blocks and at least one polymer block, the polymer block comprising a repeating unit derived from an aromatic vinyl compound as a main component, the polymer block comprising a repeating unit derived from a linear conjugated diene compound as a main component, and a ratio (wA:wB) of a weight fraction wA of the polymer block in the block copolymer to a weight fraction wB of the polymer block in the block copolymer being 30:70 to 60:40.