# US 2015/0104610 A1 · Structure and paint for forming surface coat layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0104610 A1
- Document ID: US20150104610A1
- Status: Published application
- Kind: A1
- Application number: 14/511,179
- Filed: 2014-10-10
- Published: 2015-04-16
- Earliest claimed: 2013-10-10
- Assignees: Ibiden Co., Ltd.
- Applicants: Ibiden Co., Ltd.
- Inventors: Fumiyuki MUTSUDA; Yoshitaka FUJITA
- Web page: https://patentgrep.com/patent/US20150104610A1

## CPC

- C08K 3/22: of metals
- C03C 8/14: Glass frit mixtures having non-frit additions, e.g. opacifiers, colorants, mill-additions
- C03C 8/20: containing titanium compounds; containing zirconium compounds
- C08K 3/38: Boron-containing compounds
- C23D 5/00: Coating with enamels or vitreous layers
- C23D 5/005: {by a method specially adapted for coating special objects}
- F01N 13/08: Other arrangements or adaptations of exhaust conduits {(pipes, joints or supports therefor in general F16L; collecting or removing exhaust gases of vehicle engines in workshops B08B15/00, on highways E01C1/005)}
- F01N 13/14: having thermal insulation {(exhaust manifolds F01N13/102)}
- C08K 2003/2227: {of aluminium}
- F01N 2510/02: for thermal insulation
- Y10T 428/24372: Particulate matter
- Y10T 428/24612: Composite web or sheet
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C23D: ENAMELLING OF, OR APPLYING A VITREOUS LAYER TO, METALS
- F01N: GAS-FLOW SILENCERS OR EXHAUST APPARATUS FOR MACHINES OR ENGINES IN GENERAL; GAS-FLOW SILENCERS OR EXHAUST APPARATUS FOR INTERNAL-COMBUSTION ENGINES (arrangements in connection with gas exhaust of propulsion units in vehicles B60K13/00; combustion-air intake silencers specially adapted for, or arranged on, internal-combustion engines F02M35/00; protecting against, or damping, noise in general G10K11/16)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A structure includes a surface coat layer of which the thickness on a bump such as a weld bead and a weld spatter or an edge portion, possibly formed on the surface of a base, is not greatly different from the thickness on a flat portion. The structure therefore has excellent properties including heat insulation properties and electrical insulation properties. The structure includes a base that is made of a metal, and has a flat portion and at least one of a bump and an edge portion on a surface; and a surface coat layer that is formed from an amorphous inorganic material and particles of a crystalline inorganic material, and covers the surface of the base, the surface coat layer including a first coat portion covering the flat portion and a second coat portion covering the at least one of a bump and an edge portion.

## Claims

### Claim 1

A structure comprising:
a base that is made of a metal, and has a flat portion and at least one of a bump and an edge portion on a surface; and
a surface coat layer that is formed from an amorphous inorganic material and particles of a crystalline inorganic material, and covers the surface of the base,
the surface coat layer including a first coat portion covering the flat portion and a second coat portion covering the at least one of a bump and an edge portion,
the surface coat layer having a thickness ratio of the second coat portion to the first coat portion (second coat portion thickness/first coat portion thickness) of from 0.4 to less than 1.0,
the particles of the crystalline inorganic material constituting from 5 to 70% by weight of the whole of the surface coat layer.

### Claim 2 (depends on 1)

The structure according to claim 1,
wherein the particles of the crystalline inorganic material constitute from 20 to 70% by weight of the whole of the surface coat layer.

### Claim 3 (depends on 1)

The structure according to claim 1,
wherein the particles of the crystalline inorganic material have an average particle size of from 0.1 to 50 μm.

### Claim 4 (depends on 3)

The structure according to claim 3,
wherein the particles of the crystalline inorganic material have an average particle size of from 0.1 μm to less than 10 μm.

### Claim 5 (depends on 1)

The structure according to claim 1,
wherein the first coat portion has a thickness of from 50 to 1000 μm.

### Claim 6 (depends on 1)

The structure according to claim 1, further comprising an overcoat layer formed on the surface coat layer,
wherein the overcoat layer is free from the crystalline inorganic material or contains from 0.1 to 20% by weight of the crystalline inorganic material, and
in the case that the crystalline inorganic material is contained in the overcoat layer, the crystalline inorganic material has an average particle size of from 0.1 to 50 μm.

### Claim 7 (depends on 6)

The structure according to claim 6,
wherein the overcoat layer has a surface roughness RzJIS in accordance with JIS B 0601 (2001) of from 0.05 to 10 μm.

### Claim 8 (depends on 1)

The structure according to claim 1,
wherein the crystalline inorganic material contains at least one selected from the group consisting of calcia, magnesia, ceria, alumina, and an oxide of a transition metal.

### Claim 9 (depends on 1)

The structure according to claim 1,
wherein the crystalline inorganic material contains at least one selected from the group consisting of α-alumina and yttria-stabilized zirconia.

### Claim 10 (depends on 1)

The structure according to claim 1,
wherein the amorphous inorganic material contains low melting glass that has a softening point of from 300° C. to 1000° C.

### Claim 11 (depends on 10)

The structure according to claim 10,
wherein the low melting glass contains at least one of barium glass, boron glass, strontium glass, alumina-silica glass, soda zinc glass, and soda barium glass.

### Claim 12 (depends on 1)

The structure according to claim 1,
wherein the bump is formed by at least one of a weld bead and a weld spatter.

### Claim 13

A paint for forming a surface coat layer, the surface coat layer formed on a base that is made of a metal, and has a flat portion and at least one of a bump and an edge portion on a surface,
the paint comprising an amorphous inorganic material and particles of a crystalline inorganic material,
the crystalline inorganic material constituting from 5 to 70% by weight of a total amount of the amorphous inorganic material and the crystalline inorganic material.

### Claim 14 (depends on 13)

The paint according to claim 13,
wherein the particles of the crystalline inorganic material have an average particle size of from 0.1 to 50 μm.

### Claim 15 (depends on 13)

The paint according to claim 13,
wherein the particles of the crystalline inorganic material are particles of at least one selected from the group consisting of calcia, magnesia, ceria, alumina, and an oxide of a transition metal.

### Claim 16 (depends on 13)

The paint according to claim 13,
wherein the amorphous inorganic material contains low melting glass that has a softening point of 300 to 1000° C.

### Claim 17 (depends on 16)

The paint according to claim 16,
wherein the low melting glass contains at least one of barium glass, boron glass, strontium glass, alumina-silica glass, soda zinc glass, and soda barium glass.