# US 2015/0104569 A1 · Barrier Layers for Silver Reflective Coatings and HPC Workflows for Rapid Screening of Materials for Such Barrier Layers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0104569 A1
- Document ID: US20150104569A1
- Status: Published application
- Kind: A1
- Application number: 14/574,755
- Filed: 2014-12-18
- Published: 2015-04-16
- Earliest claimed: 2013-03-13
- Assignees: Intermolecular, Inc.
- Applicants: Intermolecular Inc.
- Inventors: Guizhen Zhang; Jeremy Cheng; Guowen Ding; Minh Huu Le; Daniel Schweigert; Yu Wang
- Web page: https://patentgrep.com/patent/US20150104569A1

## CPC

- C23C 14/22: characterised by the process of coating
- C03C 17/36: at least one coating being a metal
- C03C 17/3605: {Coatings of the type glass/metal/inorganic compound}
- C03C 17/3618: {Coatings of type glass/inorganic compound/other inorganic layers, at least one layer being metallic}
- C03C 17/3644: {the metal being silver}
- C03C 17/3652: {the coating stack containing at least one sacrificial layer to protect the metal from oxidation}
- C03C 17/366: {Low-emissivity or solar control coatings}
- C03C 17/3681: {the multilayer coating being used in glazing, e.g. windows or windscreens}
- C23C 14/0036: {Reactive sputtering}
- C23C 14/042: {using masks}
- C23C 14/14: Metallic material, boron or silicon
- C23C 14/34: Sputtering
- G02B 1/12: by surface treatment, e.g. by irradiation
- G02B 1/14: Protective coatings, e.g. hard coatings
- Y10T 428/12542: More than one such component
- Y10T 428/12549: Adjacent to each other
- Y10T 428/12611: Oxide-containing component
- Y10T 428/12778: Alternative base metals from diverse categories
- Y10T 428/31678: Of metal
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Provided is High Productivity Combinatorial (HPC) testing methodology of semiconductor substrates, each including multiple site isolated regions. The site isolated regions are used for testing different compositions and/or structures of barrier layers disposed over silver reflectors. The tested barrier layers may include all or at least two of nickel, chromium, titanium, and aluminum. In some embodiments, the barrier layers include oxygen. This combination allows using relative thin barrier layers (e.g., 5-30 Angstroms thick) that have high transparency yet provide sufficient protection to the silver reflector. The amount of nickel in a barrier layer may be 5-10% by weight, chromium—25-30%, titanium and aluminum—30%-35% each. The barrier layer may be co-sputtered in a reactive or inert-environment using one or more targets that include all four metals. An article may include multiple silver reflectors, each having its own barrier layer.

## Claims

### Claim 1

A method for forming an article, the method comprising:
providing a substrate;
forming a reflective layer above the substrate; and
forming a barrier layer above the reflective layer, the barrier layer comprising nickel, chromium, titanium, and aluminum, wherein a concentration of nickel in the barrier layer is between 5% by weight and 10% by weight, a concentration of chromium in the barrier layer is between 25% by weight and 30% by weight, a concentration of titanium in the barrier layer is between 30% by weight and 35% by weight, and a concentration of aluminum in the barrier layer is between 30% by weight and 35% by weight.

### Claim 2 (depends on 1)

The method of claim 1, wherein the barrier layer further comprises oxygen.

### Claim 3 (depends on 1)

The method of claim 1, wherein nickel, chromium, titanium, and aluminum are uniformly distributed throughout the barrier layer.

### Claim 4 (depends on 1)

The method of claim 1, wherein the barrier layer consists essentially of nickel, chromium, titanium, and aluminum.

### Claim 5 (depends on 1)

The method of claim 1, wherein the barrier layer has a thickness of between 1 Angstroms and 100 Angstroms.

### Claim 6 (depends on 1)

The method of claim 1, wherein the barrier layer has a thickness of between 5 Angstroms and 30 Angstroms.

### Claim 7 (depends on 1)

The method of claim 1, wherein the barrier layer has a thickness of between 10 Angstroms and 20 Angstroms.

### Claim 8 (depends on 1)

The method of claim 1, wherein the barrier layer is deposited using physical vapor deposition.

### Claim 9 (depends on 1)

The method of claim 1, wherein the barrier layer is formed using co-sputtering of nickel, chromium, titanium, and aluminum.

### Claim 10 (depends on 1)

The method of claim 1, wherein the reflective layer comprises silver.

### Claim 11

A method for forming an article, the method comprising:
providing a substrate;
forming a reflective layer above the substrate, the reflective layer comprising silver; and
forming a barrier layer above the reflective layer, the barrier layer comprising nickel, chromium, titanium, and aluminum, wherein a concentration of nickel in the barrier layer is between 5% by weight and 10% by weight, a concentration of chromium in the barrier layer is between 25% by weight and 30% by weight, a concentration of titanium in the barrier layer is between 30% by weight and 35% by weight, and a concentration of aluminum in the barrier layer is between 30% by weight and 35% by weight, and wherein the barrier layer has a thickness of between 1 Angstroms and 100 Angstroms.

### Claim 12 (depends on 11)

The method of claim 11, further comprising forming a seed layer between the substrate and the reflective layer, the seed layer directly contacting the reflective layer and comprising at least one of ZnO, SnO2, Sc2O3, Y2O3, TiO2, ZrO2, HfO2, V2O5, Nb2O5, Ta2O5, CrO3, WO3, MoO3, or a combination thereof in a crystalline phase.

### Claim 13 (depends on 11)

The method of claim 11, further comprising forming a dielectric layer between the seed layer and the substrate or over the barrier layer, the dielectric layer comprising at least one of TiO2, SnO2, ZnSn, or a combination thereof.

### Claim 14 (depends on 13)

The method of claim 13, wherein the dielectric layer further comprises a dopant, the dopant comprising at least one of Al, Ga, In, Mg, Ca, Sr, Sb, Bi, Ti, V, Y, Zr, Nb, Hf, Ta, or a combination thereof.

### Claim 15 (depends on 11)

The method of claim 11, further comprising:
forming an additional reflective layer above the barrier layer, the additional reflective layer comprising silver; and
forming an additional barrier layer above the additional reflective layer, the additional barrier layer comprising nickel, chromium, titanium, and aluminum.

### Claim 16

A method for forming an article, the method comprising:
providing a substrate;
forming a bottom dielectric layer above the substrate, the bottom dielectric layer comprising at least one of TiO2, SnO2, ZnSn, or a combination thereof;
forming a seed layer above the bottom dielectric layer, the seed layer comprising at least one of ZnO, SnO2, Sc2O3, Y2O3, TiO2, ZrO2, HfO2, V2O5, Nb2O5, Ta2O5, CrO3, WO3, MoO3, or a combination thereof in a crystalline phase;
forming a reflective layer above the seed layer, wherein the reflective layer comprises silver; and
forming a barrier layer above the reflective layer, the barrier layer comprising nickel, chromium, titanium, and aluminum, wherein a concentration of nickel in the barrier layer is between 5% by weight and 10% by weight, a concentration of chromium in the barrier layer is between 25% by weight and 30% by weight, a concentration of titanium in the barrier layer is between 30% by weight and 35% by weight, and a concentration of aluminum in the barrier layer is between 30% by weight and 35% by weight; and
forming a top dielectric layer above the barrier layer, the bottom dielectric layer comprising at least one of TiO2, SnO2, ZnSn, or a combination thereof.

### Claim 17 (depends on 16)

The method of claim 16, wherein the barrier layer further comprises oxygen.

### Claim 18 (depends on 16)

The method of claim 16, wherein the barrier layer consists essentially of nickel, chromium, titanium, and aluminum.

### Claim 19 (depends on 16)

The method of claim 16, wherein the barrier layer has a thickness of between 1 Angstroms and 100 Angstroms.

### Claim 20 (depends on 16)

The method of claim 16, further comprising forming a diffusion barrier layer between the substrate and the bottom dielectric layer or above the top dielectric layer, the diffusion barrier layer comprising silicon nitride.